Processing Technologies and Properties of Cu-10Sn Formed by Selective Laser Melting Combined with Heat Treatment
Source abstract
Abstract
The selective laser melting (SLM) process of the Cu-10Sn alloy and effects of heat treatment were examined in this study. The Taguchi test and Box–Behnken design were performed to determine the laser power (LP), scanning speed (SS), and hatch space (HS). The best process parameters were selected using the highest density: the optimum HS was 160 μm; SS was 278 mm s −1 ; LP was 192 W; and density reached 98.76%. The tensile strength, elongation, Vickers hardness, and impact toughness of the Cu-10Sn alloy formed by SLM are 435 MPa, 13%, 122HV1, and 10 J·cm −2 , respectively. Heat treatment can significantly increase the ductility and impact toughness of the Cu-10Sn alloy, but at the same time, it can reduce its strength. The strength of parts obtained by all five heat treatment methods is much greater than that of castings. Parts that are annealed at 600°C for 4 h have the best mechanical properties, its tensile strength and elongation were 378 MPa and 15%, respectively.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Nanophotonic Functional Materials and Devices of Guangdong Province, South China Normal University, Guangzhou, China.
Guangdong Provincial Key Laboratory of Industrial Ultrashort Pulse Laser Technology, Shenzhen, China.
Han's Laser Technology Industry Group Co., Ltd., Shenzhen, China.
References (27)
Show source-provided references
1. 10.1016/j.matlet.2015.05.07610.1016/j.matlet.2015.05.076 ↗
2. 10.1016/j.matdes.2015.11.08310.1016/j.matdes.2015.11.083 ↗
3. 10.1016/j.matdes.2014.10.03410.1016/j.matdes.2014.10.034 ↗
4. 10.1016/j.matlet.2016.04.01010.1016/j.matlet.2016.04.010 ↗
5. 10.1557/jmr.2014.19410.1557/jmr.2014.194 ↗
6. 10.1016/j.jallcom.2006.05.04410.1016/j.jallcom.2006.05.044 ↗
7. 10.1016/j.jmatprotec.2006.09.02610.1016/j.jmatprotec.2006.09.026 ↗
8. 10.1016/j.matlet.2007.09.08710.1016/j.matlet.2007.09.087 ↗
9. 10.1016/j.jallcom.2008.05.06510.1016/j.jallcom.2008.05.065 ↗
10. 10.1108/1355254031050223910.1108/13552540310502239 ↗
11. 10.1016/S0924-0136(03)00755-610.1016/S0924-0136(03)00755-6 ↗
12. 10.1016/S0924-0136(03)00766-010.1016/S0924-0136(03)00766-0 ↗
13. 10.1063/1.493592610.1063/1.4935926 ↗
14. Mao Z. Forming processing and properties of copper-tin alloy in selective laser melting. Chongqing China: Chongqing University Ph.D. 2018. (In Chinese)
15. 10.1088/2053-1591/aaee5d10.1088/2053-1591/aaee5d ↗
16. 10.1016/j.jmbbm.2018.08.04710.1016/j.jmbbm.2018.08.047 ↗
17. 10.1088/1757-899X/140/1/01201910.1088/1757-899X/140/1/012019 ↗
18. 10.1016/j.biomaterials.2017.02.03010.1016/j.biomaterials.2017.02.030 ↗
19. 10.1016/j.actamat.2016.04.02910.1016/j.actamat.2016.04.029 ↗
20. Wu W, , Yang Y, , and Huang Y. Direct manufacturing of Cu-based alloy parts by selective laser melting. Chin Opt Lett, 2007; 5:37–40.
21. 10.1016/j.addma.2016.04.00310.1016/j.addma.2016.04.003 ↗
22. 10.1007/s11661-016-3779-x10.1007/s11661-016-3779-x ↗
23. 10.1016/j.matchar.2020.11019410.1016/j.matchar.2020.110194 ↗
24. 10.1016/j.ijrmhm.2019.10514410.1016/j.ijrmhm.2019.105144 ↗
25. 10.1016/j.msea.2018.02.05110.1016/j.msea.2018.02.051 ↗
26. Tan Z Zhang X Zhou Z et al. Thermal effect on the microstructure of the lattice structure Cu-10Sn alloy fabricated through selective laser melting J Alloys Compd 2019;787:903–908.10.1016/j.jallcom.2019.02.196 ↗
27. Barucca G Santecchia E Majni G et al. Structural characterization of biomedical Co–Cr–Mo components produced by direct metal laser sintering Mater Sci Eng C 2015;48:263–269.10.1016/j.msec.2014.12.009 ↗