journal article·2025-07-17Open access

Surface Treatments on Cobalt–Chromium Alloys for Layering Ceramic Paint Coatings in Dental Prosthetics

Willi-Andrei Uriciuc, Maria Suciu, Lucian Barbu-Tudoran, Adrian-Ioan Botean, Horea Florin Chicinaș, Miruna-Andreea Anghel, Cătălin Ovidiu Popa, Aranka Ilea

Coatings· Volume 15· Issue 7

Abstract

Ceramic dental prosthetics with internal metal structures are made from a cobalt–chromium alloy that is coated with ceramic. This study aims to validate surface treatments for the metal that enhance the adhesion of the ceramic coating under masticatory forces. Surface conditioning is performed using mechanical methods, like sandblasting (SB), and thermal methods, such as oxidation (O). The ceramic coating is applied to the metal component following the conditioning process, which can be conducted using either a single method or a combination of methods. Each conditioned sample undergoes characterization through various techniques, including drop shape analysis (DSA), scanning electron microscopy (SEM), X-ray diffraction (EDX), and atomic force microscopy (AFM). After the ceramic coating is applied and subjected to thermal sintering, the metal–ceramic samples are mechanically tested to assess the adhesion of the ceramic layer. The research findings, illustrated by scanning electron microscopy (SEM) images of the metal structures’ surfaces, indicate that alloy powder particles ranging from 10 to 50 µm were either adhered to the surfaces or present as discrete dots. Particles that exceed the initial design specifications of the structure can be smoothed out using sandblasting or mechanical finishing techniques. The energy-dispersive spectroscopy (EDS) results show that, after sandblasting, fragments of aluminum oxide remain trapped on the surface of the metal structures. These remnants are considered impurities, which can negatively impact the adhesion of the ceramic to the metal substrate. The analysis focuses on the exfoliation of the ceramic material from the deformed metal surfaces. The results emphasize the significant role of the sandblasting method and the micro-topography it creates, as well as the importance of the oxidation temperature in the treatment process. Drawing on 25 years of experience in dental prosthetics and the findings from this study, this publication aims to serve as a guide for applying the ceramic bonding layer to metal surfaces and for conditioning methods. These practices are essential for enhancing the adhesion of ceramic materials to metal substrates.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty Nursing and Science for Health, “Iuliu Hațieganu” University of Medicine and Pharmacy, 400012 Cluj-Napoca, Romania

Integrated Laboratory for Electronic Microscopy-Center for Alternative Energy (LIME-CETATEA), National Institute for R&D of Isotopic and Molecular Technologies (INCEDETIM), 400293 Cluj-Napoca, Romania

Electron Microscopy Center, Biology and Geology Faculty, Babes-Bolyai University, Clinicilor 5-7, 400007 Cluj-Napoca, Romania

Department of Mechanical Engineering, Technical University of Cluj-Napoca, 103-105 Muncii Blvd., 400641 Cluj-Napoca, Romania

SC Guhring SRL, 32 Constructorilor Street, 407035 Apahida, Romania

Department of Dental Prosthesis Technology, Faculty of DentalMedicine, University of Medicine and Pharmacy of Craiova, Petru Rares 2-4 Street, 200349 Craiova, Romania

Faculty of Materials and Environmental Engineering, Technical University of Cluj-Napoca, 400641 Cluj-Napoca, Romania

Faculty Dental Medicine, “Iuliu Hațieganu” University of Medicine and Pharmacy, 400012 Cluj-Napoca, Romania

Funding

Iuliu Hatieganu University of Medicine and Pharmacy, Cluj-Napoca, Romania

References (42)

Show source-provided references
1. Physico-mechanical properties and prosthodontic applications of Co-Cr dental alloys: A review of the literature10.4047/jap.2014.6.2.138 ↗
2. O’Brien, W.J. (2002). Dental Materials and Their Selection, Quintessence Publishing Co., Inc.. [3rd ed.].
3. Antoniac, I.V. (2016). Handbook of Bioceramics and Biocomposites, Springer Nature.10.1007/978-3-319-12460-5 ↗
4. (2012). General Classes of Biomaterials. Craig’s Restorative Dental Materials, Elsevier.
5. Influence of framework design on the cervical color of metal ceramic crowns10.1016/S0022-3913(11)60136-4 ↗
6. Schwendicke, F. (2020). Digital Dentistry: Advances and Challenges. J. Clin. Med., 9.10.3390/jcm9124005 ↗
7. Viderščak, D., Schauperl, Z., Šolić, S., Ćatić, A., Godec, M., Kocijan, A., Paulin, I., and Donik, Č. (2021). Additively Manufactured Commercial Co-Cr Dental Alloys: Comparison of Microstructure and Mechanical Properties. Materials, 14.10.3390/ma14237350 ↗
8. Savencu, C.E., Șerban, C., and Porojan, L. (2020). Adaptability Evaluation of Metal-Ceramic Crowns Obtained by Additive and Subtractive Technologies. Appl. Sci., 10.10.3390/app10165563 ↗
9. Additive Manufacturing Technologies Used for 3D Metal Printing in Dentistry10.1007/s40496-017-0152-0 ↗
10. Yu, J.-M., Kang, S.-Y., Lee, J.-S., Jeong, H.-S., and Lee, S.-Y. (2021). Mechanical Properties of Dental Alloys According to Manufacturing Process. Materials, 14.10.3390/ma14123367 ↗
11. Liu, Y., and Shen, J.Z. (2014). Clinical Failures of Ceramic Dental Prostheses. Advanced Ceramics for Dentistry, Elsevier.10.1016/B978-0-12-394619-5.00005-5 ↗
12. Messer, R., and Wataha, J. (2002). Dental Materials: Biocompatibility. Encyclopedia of Materials: Science and Technology, Elsevier.10.1016/B0-08-043152-6/01843-X ↗
13. Dawod, N., Miculescu, M., Antoniac, I.V., Miculescu, F., and Agop-Forna, D. (2023). Metal–Ceramic Compatibility in Dental Restorations According to the Metallic Component Manufacturing Procedure. Materials, 16.10.3390/ma16165556 ↗
14. Chirca, O., Biclesanu, C., Florescu, A., Stoia, D.I., Pangica, A.M., Burcea, A., Vasilescu, M., and Antoniac, I.V. (2021). Adhesive-Ceramic Interface Behavior in Dental Restorations. FEM Study and SEM Investigation. Materials, 14.10.3390/ma14175048 ↗
15. Cobalt-Chrome Medyloy–Sco, Technical Dates-Instruction for Use. Available online: https://www.bego.com/fileadmin/user_downloads/Mediathek/Medical/Leistungskatalog/EN/me_800160_0015_br_en.pdf.
16. Adhesion to Dental Ceramics10.1007/s40496-014-0030-y ↗
17. Ko, K.-H., Kang, H.-G., Huh, Y.-H., Park, C.-J., and Cho, L.-R. (2022). Effects of heat treatment on the microstructure, residual stress, and mechanical properties of Co-Cr alloy fabricated by selective laser melting. J. Mech. Behav. Biomed. Mater., 126.10.1016/j.jmbbm.2021.105051 ↗
18. Ceramic versus metal-ceramic implant-supported prostheses: A systematic review and meta-analysis10.1016/j.prosdent.2018.09.016 ↗
19. Worpenberg, C., Stiesch, M., Eisenburger, M., Breidenstein, B., Busemann, S., and Greuling, A. (2023). The effect of surface treatments on the adhesive bond in all-ceramic dental crowns using four-point bending and dynamic loading tests. J. Mech. Behav. Biomed. Mater., 139.10.1016/j.jmbbm.2023.105686 ↗
20. Cobalt-chromium alloys fabricated with four different techniques: Ion release, toxicity of released elements and surface roughness10.1016/j.dental.2020.08.012 ↗
21. Evaluation of the effect of different surface treatments on the bond strength of non-precious alloy–ceramic interface: An SEM study10.15171/joddd.2019.031 ↗
22. Yoo, S.Y., Kim, S.K., Heo, S.J., Koak, J.Y., and Kim, J.G. (2020). Effects of Bonding Agents on Metal-Ceramic Bond Strength of Co-Cr Alloys Fabricated by Selective Laser Melting. Materials, 13.10.3390/ma13194322 ↗
23. Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting10.1016/j.jdent.2012.02.006 ↗
24. Effect of oxidation heat treatment on the bond strength between a ceramic and cast and milled cobalt-chromium alloys10.1111/eos.12199 ↗
25. Uriciuc, W.A., Boșca, A.B., Băbțan, A.M., Vermeșan, H., Cristea, C., Tertiș, M., Pășcuță, P., Borodi, G., Suciu, M., and Barbu-Tudoran, L. (2022). Study on the Surface of Cobalt-Chromium Dental Alloys and Their Behavior in Oral Cavity as Cast Materials. Materials, 15.10.3390/ma15093052 ↗
26. Contemporary Dental Ceramic Materials, A Review: Chemical Composition, Physical and Mechanical Properties, Indications for Use10.3889/oamjms.2018.378 ↗
27. Metal-ceramic bond mechanism of the Co-Cr alloy denture with original rough surface produced by selective laser melting10.3901/CJME.2014.01.069 ↗
28. Surface-wetting characterization using contact-angle measurements10.1038/s41596-018-0003-z ↗
29. Available online: https://www.3shape.com/en/news/2012/3shape-releases-3shape-cambridge-2012.
30. Available online: https://www.kruss-scientific.com/en/products-services/products/dsa100e.
31. Gere, J.M., and Goodno, B.J. (2013). Mechanics of Materials, Cengage Learning. [8th ed.]. SI.
32. Hibbeler, R.C. (2005). Mechanics of Materials, Pearson Education International. [6th ed.].
33. Botean, A.I. (2019). Rezistenţa Materialelor. Solicitări Simple, Ediţia a II–A Revizuită şi Adăugită, Editura UT Press.
34. Botean, A.I. (2023). The use of trigonometric series for the study of isotropic beam deflection. Mathematics, 11.10.3390/math11061426 ↗
35. Effects of heat treatment on metal-ceramic combination of selective-laser-melted cobalt-chromium alloy10.1016/j.prosdent.2018.05.012 ↗
36. Hong, J.K., Kim, S.K., Heo, S.J., and Koak, J.Y. (2020). Mechanical Properties and Metal-Ceramic Bond Strength of Co-Cr Alloy Manufactured by Selective Laser Melting. Materials, 13.10.3390/ma13245745 ↗
37. Effect of heat treatment on microstructure and mechanical properties of Ni-and C-free Co-Cr-Mo alloys for medical applications10.2320/matertrans.46.1790 ↗
38. The future of dental devices is digital10.1016/j.dental.2011.10.014 ↗
39. Nishigawa, G., Maruo, Y., Irie, M., Maeda, N., Yoshihara, K., Nagaoka, N., Matsumoto, T., and Minagi, S. (2016). Various Effects of Sandblasting of Dental Restorative Materials. PLoS ONE, 11.10.1371/journal.pone.0147077 ↗
40. Takaichi, A., Kajima, Y., Kittikundecha, N., Htat, H.L., Cho, H.H.W., Hanawa, T., Yoneyama, T., and Wakabayashi, N. (2020). Effect of heat treatment on the anisotropic microstructural and mechanical properties of Co-Cr-Mo alloys produced by selective laser melting. J. Mech. Behav. Biomed. Mater., 102.10.1016/j.jmbbm.2019.103496 ↗
41. Investigation of chemical bonding at metal-ceramic interfaces10.1088/1757-899X/38/1/012014 ↗
42. Wettability versus roughness of engineering surfaces10.1016/j.wear.2010.03.029 ↗