Effect of TiC Content and TaC Addition in Substrates on Properties and Wear Behavior of TiAlN-Coated Tools
Source abstract
Abstract
The present paper reports a new way to improve the wear resistance of coated carbide tools by increases in TiC content and the addition of TaC in substrates. The results suggest that the average grain size of the substrate increased with the increases in TiC (0–14 wt.%) content, and the hardness of the TiAlN coating deposited on the substrate exhibits a similar trend. In addition, the adhesion strength of the TiAlN-coated carbide increases with increasing TiC content, which can be attributed the formation of the (Ti,W)C phase and the similar hardness of the substrate and coating. The addition of TaC into the substrates inhibits the grain growth and thereby causes the hardness and adhesion strength of the TiAlN coatings to improve from 24.6 GPa and 16.7 N to 30.1 GPa and 17.3 N, respectively. In turning tests, the TiAlN coating deposited on the substrates with the TaC addition achieved the best wear resistance in turning stainless steel because it possessed the highest substrate and coating hardness and sufficient adhesion strength. However, the TiAlN coating deposited on the substrates with a higher TiC content shows the better wear resistance in turning titanium (TC4), which can be attributed to it having the highest adhesion strength.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Physical and Mechanical Engineering, Jishou University, Jishou 416000, China
Zhuzhou Cemented Carbide Cutting Tools Co., Ltd., Zhuzhou 412000, China
Funding
Research foundation of the Education Bureau of Hunan province, China · PhD research startup foundation of Jishou University
References (37)
Show source-provided references
1. Single layer and multilayer wear resistant coatings of (Ti,Al)N: A review10.1016/S0921-5093(02)00259-9 ↗
2. Problems and solutions in machining of titanium alloys10.1007/s00170-013-5326-x ↗
3. Multilayer-growth of TiAlN/WS self-lubricating composite coatings with high adhesion and their cutting performance on titanium alloy10.1016/j.compositesb.2021.108620 ↗
4. Mechanical, oxidation, and cutting properties of AlCrN/AlTiSiN nano-multilayer10.1016/j.surfcoat.2022.128094 ↗
5. Improved properties of TiAlN coating by combined Si-addition and multilayer architecture10.1016/j.jallcom.2019.03.248 ↗
6. Improved properties of Ti-Al-N coating by multilayer structure10.1016/j.ijrmhm.2011.05.001 ↗
7. Grain size effect of pre- and post-coating treated cementedcarbides on PVD films’ adhesion and mechanical properties
8. Effect of high hardness and adhesion of gradient TiAlSiN coating on cutting performance of titanium alloy10.1016/j.jallcom.2019.153137 ↗
9. Influence of substrate pre-treatments on residual stresses and tribo-mechanical properties of TiAlN-based PVD coatings10.1016/j.surfcoat.2014.08.075 ↗
10. Study on the growth and wear behavior of the TiAlN-based composite coating deposited on TiCN-based cermets with different binder phase10.1016/j.wear.2020.203460 ↗
11. Effect of TiC addition and Co binder content in cemented carbide substrates on the microstructure and mechanical properties of the TiAlN-based composite films10.1016/j.vacuum.2020.109787 ↗
12. Bhushan, B. (2000). Mechanical and tribological requirements and evaluation of coating composites. Modern Tribology Handbook, CRC Press.10.1201/9780849377877-36 ↗
13. Evaluation of the adhesion and failure mechanism of the hard CrN coatings on different substrates10.1016/j.surfcoat.2019.01.059 ↗
14. Scratch adhesion characteristics of PVD TiAlN deposited on high speed steel, cemented carbide and PCBN substrates10.1016/j.wear.2013.08.025 ↗
15. Influence of Si content on mechanical and tribological properties of TiAlSiN PVD coatings at elevated temperatures10.1016/j.surfcoat.2017.05.014 ↗
16. Machining performance of Ti-Al-Si-N coated inserts10.1016/j.surfcoat.2010.07.043 ↗
17. High temperature oxidation and cutting performance of AlCrN, TiVN and multilayered AlCrN/TiVN hard coatings10.1016/j.surfcoat.2017.06.080 ↗
18. Investigation on microstructure and mechanical properties of reactively synthesized TiAlN/AlON nanomultilayers10.1016/j.vacuum.2011.11.019 ↗
19. Effect of micro/nano-scale textures on anti-adhesive wear properties of WC/Co-based TiAlN coated tools in AISI 316 austenitic stainless steel cutting10.1016/j.apsusc.2015.07.132 ↗
20. High temperature fracture mechanism of ultrafine WC-Co cemented carbides containing (Ti,W)C10.1016/j.ijrmhm.2020.105428 ↗
21. Effects of TaC on microstructure and mechanical properties of coarse grained WC-9Co cemented carbides10.1016/S1003-6326(15)63715-3 ↗
22. Effect of TaC and TiC on the friction and dry sliding wear of WC-6 wt.%Co cemented carbides against steel counterfaces10.1016/j.ijrmhm.2013.02.009 ↗
23. Effects of Ni content on microstructure, mechanical properties and Inconel 718 cutting performance of AlTiN-Ni nanocomposite coatings10.1016/j.ceramint.2018.09.192 ↗
24. Wear mechanisms of WC-Co cutting tools from high-speed tribological tests10.1016/j.wear.2008.12.035 ↗
25. Contact temperatures and their influence on wear during pin-on-disk tribotesting10.1016/j.triboint.2013.10.022 ↗
26. Effect of Co content on microstructure and mechanical properties of ultrafine grained WC-Co cemented carbide sintered by spark plasma sintering10.1016/j.ceramint.2018.07.100 ↗
27. A comparative research on magnetron sputtering and arc evaporation deposition of Ti-Al-N coatings10.1016/j.tsf.2011.01.358 ↗
28. Influence of TiC additions on the corrosion behaviour of WC-Co hardmetals in alkaline solution10.1016/j.ijrmhm.2014.05.009 ↗
29. Microstructure, mechanical properties, and milling performance of arc-PVD AlTiN–Cu and AlTiN/AlTiN–Cu coatings10.1007/s11771-018-3755-2 ↗
30. Microstructures and properties of PVD TiAlN coating deposited on cermets with different Ti(C,N) grain size10.1007/s11771-020-4326-x ↗
31. Effect of adhesion and tribological properties of modified composite nano-structured multi-layer nitride coatings on WC-Co tools life10.1016/j.triboint.2018.07.039 ↗
32. Phase interfaces between AlTiN and WC/Mo2C in WC-Mo2C substrate and the related characteristics10.1016/j.ijrmhm.2018.01.005 ↗
33. The effect of deep cryogenic treatment on microstructure and wear behavior of H11 tool steel10.1134/S0031918X19090035 ↗
34. Structure and properties of PVD TiAlN and TiAlN/CrAlN coated Ti(C,N)-based cermets10.1016/j.ceramint.2016.10.151 ↗
35. Analysis for Wear Behaviors of Oxidative Wear10.1007/s11249-010-9741-y ↗
36. Relationship of microstructure, mechanical properties and titanium cutting performance of TiAlN/TiAlSiN composite coated tool10.1016/j.ceramint.2016.01.159 ↗
37. Low adhesion effect of TaO functional composite coating on the titanium cutting performance of coated cemented carbide insert10.1016/j.matdes.2016.07.125 ↗