journal article·2025-11-22Open access

Study on Synergistic Enhancement of Surface Properties of Ti-6Al-4V Alloy for Dental Applications by Magnetic Abrasive Finishing

Lang Xiong, Hanqi Su, Junjiang Hao, Yucheng Su

Coatings· Volume 15· Issue 12

Abstract

Titanium alloys are widely used in dental implants due to their superior biocompatibility and mechanical strength. However, these alloys are prone to corrosion and wear in the oral environment, thereby shortening their clinical lifespan. This study investigates the enhancement of titanium alloy surface properties using magnetic abrasive finishing (MAF) and examines the influence of magnetic needle diameters (0.2–1.5 mm) on surface modification. Titanium alloy samples were processed by MAF and systematically evaluated for surface morphology, grain size, surface hardness, residual stress, electrochemical corrosion behavior, and tribological performance. Results demonstrated that MAF improves surface morphology, significantly refines grain size, and enhances surface hardness and compressive residual stress, thereby optimizing surface properties. The 1.0 mm magnetic needle group demonstrated the best performance, achieving a Vickers hardness of 376.71 ± 12.48 HV and a compressive residual stress of −579.1 ± 8.49 MPa. In addition, this group showed a higher self-corrosion potential (−0.5661 V), a lower corrosion current density (0.0114 μA·cm−2), and the lowest wear rate ((4.49 ± 0.42) × 10−4 mm3/N·m) in artificial saliva, demonstrating superior corrosion and wear resistance. Overall, MAF technology markedly enhances the surface integrity of titanium alloys in artificial saliva through the synergistic effects of grain refinement and stress modulation. These findings provide valuable experimental evidence supporting future efforts to optimize the surface properties of titanium alloy dental implants.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Advanced Surface Polishing Techniques · Erosion and Abrasive Machining

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Stomatology College of Jiamusi University, Jiamusi University, Jiamusi 154002, China

Beijing CRS Medical Device Co., Ltd., Beijing 102600, China

Beijing Citident Hospital of Stomatology, Beijing 100032, China

Beijing Implant Training College (BITC), Beijing 100032, China

Dental Implant Center, Peking Union Medical College Hospital, Chinese Academy of Medical Sciences, Beijing 100032, China

References (43)

Show source-provided references
1. Marin, E., and Lanzutti, A. (2023). Biomedical Applications of Titanium Alloys: A Comprehensive Review. Materials, 17.10.3390/ma17010114 ↗
2. Lin, C.P., Shyu, Y.T., Wu, Y.L., Tsai, M.H., Chen, H.S., and Wu, A.Y. (2022). Effects of Marginal Bone Loss Progression on Stress Distribution in Different Implant-Abutment Connections and Abutment Materials: A 3D Finite Element Analysis Study. Materials, 15.10.3390/ma15175866 ↗
3. Comparison of surface aspects of turned and anodized titanium dental implant, or abutment material for an optimal soft tissue integration10.1016/j.heliyon.2022.e10263 ↗
4. Synergistic interactions between corrosion and wear at titanium-based dental implant connections: A scoping review10.1111/jre.12469 ↗
5. Alhamad, M., Barao, V.A.R., Sukotjo, C., Cooper, L.F., and Mathew, M.T. (2021). Ti-Ions and/or Particles in Saliva Potentially Aggravate Dental Implant Corrosion. Materials, 14.10.3390/ma14195733 ↗
6. Barros, C.D.d.R., Rocha, J.C., Bastos, I.N., and Ponciano Gomes, J.A.d.C. (2021). Tribocorrosion Resistance of Dental Implant Alloys—Assessment of cp-Ti, Ti6Al4V, and NiCr in Neutral and Acidified Saliva. J. Bio- Tribo-Corros., 7.10.1007/s40735-021-00508-5 ↗
7. Microbiologically influenced corrosion can cause a dental implant rejection10.1016/j.electacta.2024.144087 ↗
8. Mellado-Valero, A., Munoz, A.I., Pina, V.G., and Sola-Ruiz, M.F. (2018). Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva. Materials, 11.10.3390/ma11010171 ↗
9. Yilmaz, E.Ç., and Sadeler, R. (2021). A Literature Review on Chewing Simulation and Wear Mechanisms of Dental Biomaterials. J. Bio- Tribo-Corros., 7.10.1007/s40735-021-00529-0 ↗
10. Effects of overloading in mastication on the mechanical behaviour of dental implants10.1016/j.matdes.2012.12.019 ↗
11. State-of-the-art review on laser cladding process as an in-situ repair technique10.1177/09544089211044558 ↗
12. Laser surface cladding of metal parts10.1016/j.rsurfi.2023.100142 ↗
13. Heimann, R.B. (2023). The nature of plasma spraying. Coatings, 13.10.3390/coatings13030622 ↗
14. Anodization of titanium alloys for orthopedic applications
15. Magnetic abrasive finishing: Innovations and possibilities10.1016/j.jmapro.2024.12.070 ↗
16. Houshi, M.N. (2016). A comprehensive review on magnetic abrasive finishing process. Advanced Engineering Forum, Trans Tech Publications.10.4028/www.scientific.net/AEF.18.1 ↗
17. Enhancing Surface Integrity of Selective Laser Melted Al-Si Alloys through Ultrasonic Assisted Magnetic Abrasive Finishing utilizing SiC Abrasives10.1007/s12633-023-02721-y ↗
18. Residual stress evolution and tailoring of cold pilgered Ti-3Al-2.5V tube10.1016/j.ijmecsci.2022.107366 ↗
19. Surface integrity of titanium part by ultrasonic magnetic abrasive finishing10.1007/s00170-015-7028-z ↗
20. Behavior characteristics of abrasives for improving surface integrity in magnetic pin polishing10.1007/s12206-020-2218-5 ↗
21. Noyan, I.C., and Cohen, J.B. (2013). Residual Stress: Measurement by Diffraction and Interpretation, Springer.
22. Influence of grain refinement on the corrosion behavior of metallic materials: A review10.1007/s12613-021-2308-0 ↗
23. Study of the structural, optical, electrical and electrochemical properties of copper oxide thin films synthesized by spray pyrolysis10.1007/s10854-024-12006-8 ↗
24. Golgovici, F., Tudose, A.-E., Mosinoiu, L.F., and Demetrescu, I. (2025). Characterization of NiCrAlY Layers Deposited on 310H Alloy Using the EB-PVD Method After Oxidation in Water at High Temperature and Pressure. Appl. Sci., 15.10.3390/app15052361 ↗
25. Regulation of trace aluminum addition on the corrosion resistance of Cu-12.5Ni-5Sn-xAl alloy10.1016/j.mtcomm.2025.111616 ↗
26. Improved surface integrity of Ti6Al4V fabricated by selective electron beam melting using ultrasonic surface rolling processing10.1016/j.jmatprotec.2021.117264 ↗
27. Effects of Ultrasonic Assisted Magnetic Abrasive Finishing on Surface Integrity of Titanium Alloy
28. Numerical calculation of wear in rolling contact based on the Archard equation: Effect of contact parameters and consideration of uncertainties10.1016/j.wear.2021.204188 ↗
29. Ultrasonic impact surface strengthening treatment and fatigue behaviors of titanium alloy thin-walled open hole components10.1016/j.engfracmech.2024.110292 ↗
30. Zha, X., Yuan, Z., Qin, H., Xi, L., Guo, Y., Xu, Z., Dai, X., and Jiang, F. (2024). Investigating the Dynamic Mechanical Properties and Strengthening Mechanisms of Ti-6Al-4V Alloy by Using the Ultrasonic Surface Rolling Process. Materials, 17.10.3390/ma17061382 ↗
31. Study on surface properties of Ti-6Al-4V titanium alloy by ultrasonic rolling10.1016/j.simpat.2022.102643 ↗
32. Synchronously tailoring of residual stress and surface quality of high-strength titanium alloy tube using magnetic field-assisted finishing10.1016/j.jmapro.2025.02.085 ↗
33. Corrosion-fatigue property of anodic oxidation coated 6082-T6 aluminium alloy: Effect of substrate residual stress and microstructure beneath coating-substrate interface10.1016/j.ijfatigue.2023.107803 ↗
34. Residual stress relaxation and duty cycle on high cycle fatigue life of micro-arc oxidation coated AA7075-T6 alloy10.1016/j.ijfatigue.2019.105283 ↗
35. An Overview of Near-Neutral pH Stress Corrosion Cracking in Pipelines and Mitigation Strategies for Its Initiation and Growth10.5006/1967 ↗
36. Effect of machining-induced surface residual stress on initiation of stress corrosion cracking in 316 austenitic stainless steel10.1016/j.corsci.2016.03.008 ↗
37. Effect of TiAlSiN coating residual stress on its sliding wear and cutting wear performance10.1007/s00170-022-10508-5 ↗
38. Effect of compressive residual stress on wear resistance of IGT25+ gas turbine compressor blades made of 1.4923 steel10.52547/mme.22.3.167 ↗
39. Fretting-corrosion at the Implant–Abutment Interface Simulating Clinically Relevant Conditions10.1016/j.dental.2024.08.007 ↗
40. Degradation mechanisms and future challenges of titanium and its alloys for dental implant applications in oral environment10.1016/j.msec.2017.02.159 ↗
41. Fretting-corrosion behavior on dental implant connection in human saliva10.1016/j.jmbbm.2019.02.025 ↗
42. A more defective substrate leads to a less defective passive layer: Enhancing the mechanical strength, corrosion resistance and anti-inflammatory response of the low-modulus Ti-45Nb alloy by grain refinement10.1016/j.actbio.2021.02.045 ↗
43. Wear behavior and microhardness studies of tantalum (Ta)-coated 316L stainless steel by DC magnetron sputtering for the orthopedic applications10.1007/s10853-022-07939-6 ↗