Abstract

To simulate the erosion damage behavior of thermal barrier coatings (TBCs) under actual service conditions in an aircraft engine environment, this study developed a multi-factor coupled test setup capable of simulating combined loading under high-temperature (1150 °C), high-speed (0.4 Mach), and solid-particle erosion conditions. Yttria-stabilized zirconia (YSZ) TBCs were prepared using electron beam physical vapor deposition (EB-PVD). For different erosion durations (2 h, 5 h, 8 h, 12 h), the evolution of macroscopic and microscopic morphologies as well as the development of residual stresses in the thermally grown oxide (TGO) layer were systematically investigated. The results indicate that the erosion process of the YSZ coating can be divided into three stages. During the initial high-erosion-rate stage (8.17 g/kg), erosion damage was confined to the grain tips of the columnar crystals, primarily caused by brittle fracture at the grain tips, and the TGO stress was relatively low (−0.6 GPa). During the intermediate stage, the erosion rate was lower (2.74 g/kg). Impact stresses induced microcracks within the columnar grains, which gradually connected to form intergranular fractures. This led to the expansion of localized spalling pits. The interface began to wrinkle, and the stress rose to −2.2 GPa. In the final accelerated failure stage (5.88 g/kg), horizontal cracks fully propagated, leading to large-scale peeling of the coating. The stress was released to −0.9 GPa. The coating failure mechanism evolves from surface damage to interfacial peeling, which is closely related to the coating structure, stress evolution, and interfacial state.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Erosion and Abrasive Machining · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Surface Engineering Institution, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China

AECC Key Laboratory of Advanced Corrosion and Protection on Aviation Materials, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China

Fundamental Science Laboratory on Aerospace Protective Coatings, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China

School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China

Funding

Beijing Institute of Aeronautical Materials

References (48)

Show source-provided references
1. Recent advances in the development of aerospace materials10.1016/j.paerosci.2018.01.001 ↗
2. Progress and strategies in advanced aerospace materials for extreme environments: A review10.1016/j.actaastro.2025.08.011 ↗
3. Progress update on failure mechanisms of advanced thermal barrier coatings: A review10.1016/j.porgcoat.2015.09.019 ↗
4. Microstructure evolution, thermal cycling life and failure behavior analysis of YSZ thermal barrier coatings prepared by EB-PVD with different electron beam currents
5. Effect of grit-blasting on the recrystallization behavior of DD6 single-crystal superalloy coated with NiCoCrAlYHf10.1016/j.jallcom.2024.173861 ↗
6. Preparation and failure mechanism of LaZrCeO thermal barrier coatings by EB-PVD
7. Long lifespan thermal barrier coatings overview: Materials, manufacturing, failure mechanisms, and multiscale structural design10.1016/j.ceramint.2022.10.222 ↗
8. Bogdan, M., and Peter, I. (2024). A Comprehensive Understanding of Thermal Barrier Coatings (TBCs): Applications, Materials, Coating Design and Failure Mechanisms. Metals, 14.10.3390/met14050575 ↗
9. Hu, X., Xie, Y., Li, F., and Yin, F. (2024). Research progress on environmental corrosion resistance of thermal barrier coatings: A review. Coatings, 14.10.3390/coatings14101341 ↗
10. A review on the performance and lifetime improvement of thermal barrier coatings10.1016/j.jeurceramsoc.2025.117274 ↗
11. YGYSZ/YSZ double ceramic layer thermal barrier coatings: Coating design and failure mechanism during thermal shock test10.1016/j.surfcoat.2025.132650 ↗
12. Microstructural evolution and failure mechanisms of thermal barrier coatings under extreme environmental conditions10.1016/j.jeurceramsoc.2024.117089 ↗
13. Failure analysis and life prediction of thermal barrier coatings on turbine blades under localized cyclic thermal loading10.1016/j.jmrt.2025.11.142 ↗
14. Simulation of foreign particle erosion-induced failure in thermal barrier coatings: A novel coupling plastic damage model of dual-horizon peridynamics and FEM10.1016/j.ijimpeng.2025.105255 ↗
15. Performance and failure modes of thermal barrier coatings deposited by EB-PVD on blades under real service conditions in gas turbine10.1016/j.jallcom.2024.176889 ↗
16. Solid particle erosion of thermal spray and physical vapour deposition thermal barrier coatings10.1016/j.wear.2011.06.013 ↗
17. Friction delamination mechanism of EB-PVD thermal barrier coatings in high-temperature and high-speed rotating service environment10.1016/j.jeurceramsoc.2023.01.014 ↗
18. Scaling laws governing the erosion and impact resistance of thermal barrier coatings10.1016/j.wear.2005.05.005 ↗
19. Effect of bond coating surface roughness on high-temperature performance of EB-PVD thermal barrier coatings10.1016/j.ceramint.2025.01.267 ↗
20. Microstructural characterization and room-temperature erosion behavior of as-deposited SPS, EB-PVD and APS YSZ-based TBCs10.1007/s11666-018-0763-6 ↗
21. Development and optimization of tailored composite TBC design architectures for improved erosion durability10.1007/s11666-017-0561-6 ↗
22. Erosion of gadolinia-doped EB-PVD TBCs10.1016/j.surfcoat.2006.03.022 ↗
23. Erosion behavior of EB-PVD 7YSZ coatings under corrosion/erosion regime: Effect of TBC microstructure and CMAS chemistry10.1016/j.jeurceramsoc.2018.06.039 ↗
24. Al modification for PS-PVD 7YSZ TBCs to improve particle erosion and thermal cycle performance10.1007/s40145-022-0596-0 ↗
25. Zhao, X., Liu, W., Li, C., Yan, G., Wang, Q., Yang, L., and Zhou, Y. (2022). Solid particle erosion behavior of La2Ce2O7/YSZ double ceramic layer and traditional YSZ thermal barrier coatings at high temperature. Coatings, 12.10.3390/coatings12111638 ↗
26. Nano and microhardness testing of aged EB-PVD TBCs10.1016/j.surfcoat.2004.08.018 ↗
27. A review of the erosion of thermal barrier coatings10.1088/0022-3727/40/16/R01 ↗
28. The effect of TBC morphology on the erosion rate of EB-PVD TBCs10.1016/j.wear.2004.04.011 ↗
29. Nano and micro-indentation studies of bulk zirconia and EB-PVD TBCs10.1016/S0257-8972(03)00737-0 ↗
30. The effect of TBC morphology and aging on the erosion rate of EB-PVD TBCs10.1016/j.triboint.2005.02.008 ↗
31. A Monte Carlo model for predicting the erosion rate of EB-PVD TBCs10.1016/j.wear.2003.09.001 ↗
32. On the effect of ageing on the erosion of EB-PVD TBCs10.1016/j.surfcoat.2003.06.019 ↗
33. Failure behaviour of EB-PVD YSZ thermal barrier coatings under simulated aero-engine operating conditions10.1016/j.surfcoat.2023.130027 ↗
34. Fatigue cracks in a thermal barrier coating system on a superalloy in multiaxial thermomechanical testing10.1016/j.ijfatigue.2007.01.037 ↗
35. Advanced thermal gradient mechanical fatigue testing of CMSX-4 with an oxidation protection coating10.1016/j.ijfatigue.2007.01.034 ↗
36. Damage mechanisms in solid particle impact and erosion testing of thermal barrier coatings10.1016/j.surfcoat.2025.132844 ↗
37. Erosion behavior of YSZ, LZC, and LZC/YSZ double ceramic layer thermal barrier coatings by EB-PVD under high-temperature gas streams with entrained solid particles10.1016/j.surfin.2026.109073 ↗
38. Wang, L., He, L., Zhang, R., Xu, Z., and Mu, R. Particle erosion behavior of La2(ZrxCe1−x)2O7/YSZ double ceramic layer TBCs deposited by electron beam physical vapor deposition. Wear, 2025, 566–567, 205763.10.1016/j.wear.2025.205763 ↗
39. Effect of microstructure and temperature on the erosion rates and mechanisms of modified EB-PVD TBCs10.1016/j.wear.2009.04.002 ↗
40. Erosion behavior of PS-PVD thermal barrier coatings and the effect of composite coating thickness10.4028/www.scientific.net/MSF.993.1095 ↗
41. The mechanical response of three EB-PVD thermal barrier coating microstructures10.1016/S0921-5093(99)00773-X ↗
42. LZC/YSZ DCL TBCs by EB-PVD: Microstructure, low thermal conductivity and high thermal cycling life10.1016/j.jeurceramsoc.2018.12.031 ↗
43. Stress analysis and failure mechanisms of plasma-sprayed thermal barrier coatings10.1007/s11666-017-0544-7 ↗
44. Nondestructive evaluation of oxidation stress in thermal barrier coatings using Cr3+ piezospectroscopy10.1063/1.117182 ↗
45. Measurement of residual stress in air plasma-sprayed Y2O3–ZrO2 thermal barrier coating system using micro-Raman spectroscopy10.1016/j.msea.2005.12.034 ↗
46. Effect of substrate curvature on residual stresses and failure modes of an air plasma-sprayed thermal coating system10.1016/j.jeurceramsoc.2013.05.018 ↗
47. Influence of cracks in APS TBCs on stress around TGO during thermal cycling: A numerical simulation study10.1016/j.surfcoat.2015.11.036 ↗
48. Wang, L., Yu, J., Zhang, T., Wang, Z., and Ding, K. (2023). Effect of interface curvature on local growth behavior and stress of thermal barrier coatings. Coatings, 13.10.3390/coatings13091618 ↗