Wear Mechanism of an AlCrN-Coated Solid Carbide Endmill Cutter and Machined Surface Quality under Eco-Friendly Settings during Open Slot Milling of Tempered JIS SKD11 Steel
Source abstract
Abstract
In the die and mold industry, tempered JIS SKD11 steel is selected to manufacture cold-forming dies that require an optimum balance of toughness, strength, and wear resistance. Therefore, the machinability of tempered JIS SKD11 in the milling machining process is challenging. The use of eco-friendly machining settings is intended to diminish tool wear and enhance the quality of the machined surface as well as the accuracy of the machined components. Adapting to the aforementioned factors for cold-forming dies is a pivotal issue. In this study, the machinability of tempered JIS SKD11 steel was analyzed under dry, MQL, cryogenic cooling with liquid nitrogen (LN2), and liquid carbon dioxide (LCO2) machining settings during open slot milling operations with varying input parameters, including cutting speeds and cutting feeds. An in-depth evaluation of output responses, including tool wear, surface roughness, cutting temperature in the cutting zone, and microhardness of the machined surface, was also conducted. The findings unveiled that the flank wear of the cutters and surface roughness of the machined surfaces obtained minimum values of 0.22 mm and 0.197 µm, respectively, during open slot milling operations at a cutting speed of 100 m/min and a cutting feed of 204 mm/min under cryogenic cooling with liquid carbon dioxide (LCO2). The findings from this study suggest that employing cryogenic cooling with LCO2 could serve as a viable substitute for dry, MQL, and cryogenic cooling with LN2 methods to enhance the machinability of hardened JIS SKD11 steel.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced machining processes and optimization · Metal Alloys Wear and Properties · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Mechanical Engineering Laboratory, Faculty of Mechanical Engineering, Cao Thang Technical College (CTTC), 65 Huynh Thuc Khang, Ben Nghe Ward, District 1, Ho Chi Minh City 700000, Vietnam
Department of Machine Design, Faculty of Mechanical Engineering, Ho Chi Minh City University of Technology (HCMUT), 268 Ly Thuong Kiet Street, District 10, Ho Chi Minh City 700000, Vietnam
Vietnam National University Ho Chi Minh City, Linh Trung Ward, Thu Duc City, Ho Chi Minh City 700000, Vietnam
References (49)
Show source-provided references
1. Astakhov, V.P., and Davim, J.P. (2011). Machining of Hard Materials, Springer.
2. Machining Characteristics of Hard Materials10.1016/S0007-8506(07)61592-3 ↗
3. High speed end milling of hardened AISI D2 tool steel (~58 HRC)10.1016/S0924-0136(02)00155-3 ↗
4. Rapid machining of hardened AISI H13 and D2 moulds, dies and press tools10.1016/S0924-0136(02)00861-0 ↗
5. Comparative evaluation of conventional and wiper ceramic tools on cutting forces, surface roughness, and tool wear in hard turning AISI D2 steel10.1243/09544054JEM762 ↗
6. Cutting of Hardened Steel10.1016/S0007-8506(07)63455-6 ↗
7. Machinability investigations in hard turning of AISI D2 cold work tool steel with conventional and wiper ceramic inserts10.1016/j.ijrmhm.2008.12.007 ↗
8. Machinability Evaluation in Hard Milling of AISI D2 Steel10.1590/1980-5373-MR-2015-0263 ↗
9. Hard turning: AISI 4340 high strength low alloy steel and AISI D2 cold work tool steel10.1016/j.jmatprotec.2005.04.082 ↗
10. Effect of the minimum quantity lubrication in high-speed end-milling of AISI D2 cold-worked die steel (62 HRC) by coated carbide tools10.1016/j.surfcoat.2008.06.129 ↗
11. Determination of machinability metrics of AISI 5140 steel for gear manufacturing using different cooling/lubrication conditions10.1016/j.jmrt.2022.09.067 ↗
12. Fox-Rabinovich, G., Kovalev, A., Gershman, I., Wainstein, D., Aguirre, M.H., Covelli, D., Paiva, J., Yamamoto, K., and Vedhuis, S. (2018). Complex Behavior of Nano-Scale Tribo-Ceramic Films in Adaptive PVD Coatings under Extreme Tribological Conditions. Entropy, 20.10.3390/e20120989 ↗
13. High speed mchining of moulds and dies for net shape manufacture10.1016/S0261-3069(99)00092-8 ↗
14. Sebbe, N.P.V., Fernandes, F., Silva, F.J.G., Pedroso, A.F.V., Sales-Contini, R.C.M., Barbosa, M.L., Durao, L.M., and Magalhaes, L.L. (2024). Wear Behavior of TiAlVN-Coated Tools in Milling Operations of INCONEL® 718. Coatings, 14.10.3390/coatings14030311 ↗
15. Khetre, S., Bongale, A., Kumar, S., and Ramesh, B.T. (2024). Temperature Analysis in Cubic Boron Nitrate Cutting Tool during Minimum Quantity Lubrication Turning with a Coconut-Oil-Based Nano-Cutting Fluid Using Computational Fluid Dynamics. Coatings, 14.10.3390/coatings14030340 ↗
16. Chauhan, D., Makhesana, M.A., Rahman, R.R.A., Joshi, V., and Khanna, N. (2023). Comparison of Machining Performance of Ti-6Al-4V under Dry and Cryogenic Techniques Based on Tool Wear, Surface Roughness, and Power Consumption. Lubricants, 11.10.3390/lubricants11110493 ↗
17. Gong, L., Su, L., Liu, Y., Zhao, W., Khan, A.M., and Jamil, M. (2023). Investigation on Machinability Characteristics of Inconel 718 Alloy in Cryogenic Machining Processes. Lubricants, 11.10.3390/lubricants11020082 ↗
18. Şap, S., Usca, U.A., Uzun, M., Kuntoglu, M., Salur, E., and Pimenov, D.Y. (2022). Investigation of the Effects of Cooling and Lubricating Strategies on Tribological Characteristics in Machining of Hybrid Composites. Lubricants, 10.10.3390/lubricants10040063 ↗
19. Fernández, D., Sandá, A., and Bengoetxea, I. (2019). Cryogenic Milling: Study of the Effect of CO2 Cooling on Tool Wear When Machining Inconel 718, Grade EA1N Steel and Gamma TiAl. Lubricants, 7.10.3390/lubricants7010010 ↗
20. Kaynak, Y., and Gharibi, A. (2018). Progressive Tool Wear in Cryogenic Machining: The Effect of Liquid Nitrogen and Carbon Dioxide. J. Manuf. Mater. Process., 2.10.3390/jmmp2020031 ↗
21. Dai, X., Zhuang, K., Pu, D., Zhang, W., and Ding, H. (2020). An Investigation of the Work Hardening Behavior in Interrupted Cutting Inconel 718 under Cryogenic Conditions. Materials, 13.10.3390/ma13092202 ↗
22. Muhamad, S.S., Ghani, J.A., Haron, C.H.C., and Yazid, H. (2022). Wear Mechanism of Multilayer Coated Carbide Cutting Tool in the Milling Process of AISI 4340 under Cryogenic Environment. Materials, 15.10.3390/ma15020524 ↗
23. Wainstein, D., and Kovalev, A. (2018). Tribooxidation as a Way to Improve the Wear Resistance of Cutting Tools. Coatings, 8.10.3390/coatings8060223 ↗
24. Iqbal, A., Suhaimi, H., Zhao, W., Jamil, M., Nauman, M.M., He, N., and Zaini, J. (2020). Sustainable Milling of Ti-6Al-4V: Investigating the Effects of Milling Orientation, Cutter′s Helix Angle, and Type of Cryogenic Coolant. Metals, 10.10.3390/met10020258 ↗
25. Comprehensive machining analysis to establish cryogenic LN2 and LCO2 as sustainable cooling and lubrication techniques10.1016/j.triboint.2020.106314 ↗
26. Influence of hybrid Cryo-MQL lubri-cooling strategy on the machining and tribological characteristics of Inconel 71810.1016/j.triboint.2021.107178 ↗
27. Technological and tribological characteristics improvement of additively manufactured SS 316L components machined under sustainable cooling conditions10.1016/j.triboint.2023.108329 ↗
28. (1993). Tool-Life Testing with Single-Point Turning Tools (Standard No. ISO 3685:1993).
29. The effects of cryogenic cooling on surface integrity in hard machining: A comparison with dry machining10.1016/j.cirp.2012.03.052 ↗
30. Wear mechanisms of solid carbide cutting tools in dry and cryogenic machining of AISI H13 steel with varying cutting-edge radius10.1016/j.wear.2023.204758 ↗
31. Cryogenic and minimum quantity lubrication for an eco-efficiency turning of AISI 30410.1016/j.jclepro.2016.08.030 ↗
32. Comparison between sustainable cryogenic techniques and nano-MQL cooling mode in turning of nickel-based alloy10.1016/j.jclepro.2019.05.196 ↗
33. Simulation of the effects of cryogenic liquid nitrogen jets in Ti6Al4V milling10.1016/j.jmapro.2022.11.053 ↗
34. The effects of cryogenic cooling on tool wear and chip morphology in turning of tantalum-tungsten alloys Ta-2.5W10.1016/j.jmapro.2022.12.063 ↗
35. High-speed milling of hardened steel under minimal quantity lubrication with liquid nitrogen10.1016/j.jmapro.2023.04.013 ↗
36. Cryogenic CO2 assisted hard turning of AISI 52100 with robust CO2 delivery10.1016/j.jmapro.2023.05.036 ↗
37. Side-milling of Incoloy 825 under pulsed and continuous modes of cryogenic cooling10.1016/j.jmapro.2023.09.010 ↗
38. Wu, J., He, L., Wu, Y., Zhou, C., Zou, Z., Zhan, G., Zhou, T., Du, F., Tian, P., and Zou, Z. (2021). Enhancing Wear Resistance and Cutting Performance of a Long-Life Micro-Groove Tool in Turning AISI 201. Coatings, 11.10.3390/coatings11121515 ↗
39. Structure, properties and wear performance of nano-multilayered TiAlCrSiYN/TiAlCrN coatings during machining of Ni-based aerospace superalloys10.1016/j.surfcoat.2010.04.050 ↗
40. PVD-CrAlN and TiAlN coated Si3N4 ceramic cutting tools—1. Microstructure, turning performance and wear mechanism10.1016/j.ceramint.2017.04.041 ↗
41. Impact wear and abrasion resistance of CrN, AlCrN and AlTiN PVD coatings10.1016/j.surfcoat.2012.08.077 ↗
42. Evaluation of wear mechanisms of coated carbide tools when face milling titanium alloy10.1016/S0924-0136(99)00438-0 ↗
43. Liu, G., Huang, C., Wang, X., Zhao, B., and Ji, M. (2024). Friction and Wear of Cutting Tools and Cutting Tool Materials. Lubricants, 12.10.3390/lubricants12060192 ↗
44. Wang, X., Zhang, X., Pan, D., Niu, J., Fu, X., and Qiao, Y. (2023). Tool Wear and Surface Integrity of γ-TiAl Cryogenic Coolant Machining at Various Cutting Speed Levels. Lubricants, 11.10.3390/lubricants11060238 ↗
45. In pursuit of sustainable cutting fluid strategy for machining Ti-6Al-4V using life cycle analysis
46. Role of sustainable cooling/lubrication conditions in improving the tribological and machining characteristics of Monel-400 alloy10.1016/j.triboint.2022.107880 ↗
47. Review on design and development of cryogenic machining setups for heat resistant alloys and composites10.1016/j.jmapro.2021.05.053 ↗
48. (2018). Granulated Cork and Cork Powder—Classification, Properties and Packing (Standard No. ISO 1997:2018).
49. (1989). Tool Life Testing in Milling—Part 2: End Milling (Standard No. ISO 8688–2:1989).