journal article·2022-10-08Open access

Influence of Pre-Tinning Process on Coating Morphology and Interface Structure of Low Carbon Steel Dipped in Molten 6061 Al Alloy

Naglaa Fathy, Khaled Saad Abdel Halim, K. M. Hafez, Mohamed Ramadan, Badreddine Ayadi, Abdulaziz S. Alghamdi, Khaled M. Ibrahim

Coatings· Volume 12· Issue 10

Abstract

Pre-treated low carbon steel specimens with flux or flux + tin mixture were coated by hot-dip aluminizing process. Al alloy (6061) was melted and hold at 750 °C. Fluxed and pre-tinned low carbon steel samples were dipped in a molten bath for time intervals of 0.5, 1, 2.5 and 3.5 min. Applying double coating processes via tinning-aluminizing techniques facilitated the formation of Fe-Al intermetallic interface and increasing the thickness of homogenous coating layer over the substrate material. The presence of Sn facilitates to great extent the formation of a better interlayer-free bond of residual flux and/or oxides. The fluxed–dipped steel substrates have inhomogeneous distribution of Al alloy coating as well as an interface with residual flux and oxides for dipping time up to 2.5 min. A homogenous distribution with good thickness morphology of the Al alloy coating and homogeneous thin intermetallic interface was achieved for tinned steel substrate at all applied dipping times. The comparison between the pre-tinning and pre-fluxing processes on steel substrates showed a significant effect of tinning over fluxing treatment acting on the thickness layer of Al-coating and interface using a short time dipping. For dipping time up to 2.5 min, the hardness of pre-tinning substrates is greater than that of fluxed ones due to the presence of residual flux and void interface in fluxed steel.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Physics, College of Science, University of Hail, Hail P.O. Box 2440, Saudi Arabia

College of Engineering, University of Hail, Hail P.O. Box 2440, Saudi Arabia

Central Metallurgical Research and Development Institute (CMRDI), Helwan 11421, Egypt

Laboratory of Applied Fluid Mechanics, Environment and Process Engineering ”LR11ES57”, National School of Engineers of Sfax (ENIS), University of Sfax, Route Soukra Km 3.5, Sfax 3038, Tunisia

Funding

Scientific Research Deanship at University of Ha’il—Saudi Arabia

References (23)

Show source-provided references
1. Studies on the characterization and morphological features of the coating on interstitial free steel dipped in molten Al-Si-Mg alloy at 800 °C10.1016/j.jmrt.2020.02.104 ↗
2. Observation of high-temperature phase transformation in the Si-modified aluminide coating on mild steel using EBSD10.1016/j.matchar.2010.02.001 ↗
3. Microstructural evolution of intermetallic layer in hot-dipped aluminide mild steel with silicon addition10.1016/j.surfcoat.2011.04.061 ↗
4. Rock. Microstructure studies of an aluminide coating on 9Cr-1Mo steel during high temperature oxidation10.1016/j.surfcoat.2005.11.038 ↗
5. The high-temperature oxidation behavior of hot-dipping Al–Si coating on low carbon steel10.1016/j.surfcoat.2005.11.031 ↗
6. Metallurgy of continuous hot dip aluminizing10.1179/imr.1994.39.5.191 ↗
7. Khaliq, A., Alghamdi, A.S., Ramadan, M., Subhani, T., Rajhi, W., Haider, W., and Hasan, M.M. (2022). Intermetallic compounds formation during 316L stainless steel reaction with Al–Zn–Si coating alloy. Crystals, 12.10.3390/cryst12050735 ↗
8. Investigation of phase evolution of Al–Si–Mg coating on hot dipped interstitial-free steel10.1016/j.rinma.2020.100078 ↗
9. Aluminium diffusion coating on medium carbon steel10.2320/matertrans1989.36.1170 ↗
10. EBSD study of crystallographic identification on Fe-Al-Si intermetallic phases in aluminide coatings on mild steels10.4028/www.scientific.net/AMR.79-82.907 ↗
11. Ramadan, M., Alghamdi, A., Hafez, K., Subhani, T., and Halim, K.A. (2020). Development and optimization of tin/flux mixture for direct tinning and interfacial bonding in aluminum/steel bimetallic compound casting. Materials, 13.10.3390/ma13245642 ↗
12. Ramadan, M., Alghamdi, A.S., Subhani, T., and Halim, K.S.A. (2020). Fabrication and characterization of Sn-based babbitt alloy nanocomposite reinforced with Al2O3 nanoparticles/carbon steel bimetallic material. Materials, 13.10.3390/ma13122759 ↗
13. Correction to: Novel approach for using ductile iron as substrate in bimetallic materials for higher interfacial bonding bearings
14. Alghamdi, A.S., Halim, K.S.A., Amin, M.A., Alshammari, A.S., Fathy, N., and Ramadan, M. (2021). Interfacial microstructure and corrosion behaviour of mild steel coated with alumina nanoparticles doped tin composite via direct tinning route. Coatings, 11.10.3390/coatings11111318 ↗
15. Halim, K.S.A., Ramadan, M., Sherif, E.-S.M., Hafez, K.M., Subhani, T., Fathy, N., Alghamdi, A.S., and Khedr, M.H. (2022). Enhancement of surface and interface properties of low carbon steel by hybrid ZnO and NiO nanoparticles reinforced tin coating. Crystals, 12.10.3390/cryst12030332 ↗
16. A novel electrodeposition route for fabrication of the superhydrophobic surface with unique self-cleaning, mechanical abrasion and corrosion resistance properties10.1016/j.cej.2016.05.133 ↗
17. Cardanol-based polybenzoxazine superhydrophobic coating with improved corrosion resistance on mild steel10.1016/j.porgcoat.2019.06.037 ↗
18. Formation of an Fe–Sn intermetallic layer during the reflow, process after tin plating
19. Thermodynamic evaluation of Fe–Sn phase diagram10.1016/S0364-5916(96)00021-1 ↗
20. Ramadan, M., Khaliq, A., Hafez, K.M., Alghamdi, A.S., Fathy, N., Harraz, F.A., Ayadi, B., and Halim, K.S.A. (2022). Super bonding strength of Al2O3 nanoparticles reinforced Sn interlayer steel/aluminum bimetal casting. Crystals, 12.10.3390/cryst12030324 ↗
21. Formation of Al–Zn–Si coatings on low carbon steel substrates
22. Al–Fe–Si (aluminum–iron–silicon)
23. Intermetallic phases formed during tin implantation into iron and steels10.1063/1.333022 ↗