Cracking Failure Analysis of Drill Pipe Joint with Hardbanding
Source abstract
Abstract
A batch of drill pipe joints in a well cracked and failed due to hardbanding. In this study, various experiments were conducted to analyze the reasons for cracking failure, including data verification, macroscopic morphology analysis, mechanical properties, microstructure analysis, and micro-Vickers hardness of cracked areas, as well as macroscopic, metallographic, and energy spectrum analysis of the fracture surface after opening the cracked area. The results indicated that (1) the chemical composition, tensile strength, Charpy impact test, and Brinell hardness results of the joint met the requirements of the order technical conditions. (2) The hardbanding in the cracked area had multiple pores and cracks on its outer surface and inside. The maximum diameter of the internal porosity was about 3.4 mm, and the length of the internal crack was about 1 mm. (3) The main reason for the cracking of a batch of drill pipe joints due to hardbanding is a quality problem of the secondary repair welding of the hardbanding. The cracks in the failed drill pipe originated from the porosity and cracks in the hardbanding of the drill pipe box joint. Under the influence of alternating stress and high-pressure mud erosion underground, the cracks rapidly extended to the inner wall, and the porosity in the hardbanding accelerated crack propagation, ultimately causing the drill pipe to crack and fail.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Erosion and Abrasive Machining · Drilling and Well Engineering · Structural Integrity and Reliability Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
CNPC Tubular Goods Research Institute, Xi’an 710077, China
Bohai Petroleum Equipment Fujian Steel Pipe Co., Ltd., Fuzhou 350500, China
References (27)
Show source-provided references
1. Effect of cuttings particle content on the tribological behavior of Fe/DLC at casing and drill pipe joints: A molecular dynamics study10.1016/j.molliq.2024.124006 ↗
2. The friction and wear of various hard-face claddings for deep-hole drilling10.1016/j.wear.2007.01.046 ↗
3. Role of binder phase on properties and holding ability of WC based diamond hardbanding matrix10.1016/j.ijrmhm.2025.107184 ↗
4. Effect of Ni content and maceration metal on the microstructure and properties of WC based diamond composites10.1016/j.ijrmhm.2020.105196 ↗
5. Material properties and tool performance of PCD reinforced WC matrix composites for hardbanding applications10.1016/j.ijrmhm.2015.03.011 ↗
6. Effect of Fe-based pre-alloyed powder on the microstructure and holding strength of impregnated diamond bit matrix10.1016/j.ijrmhm.2018.11.015 ↗
7. Manipulation of the thermal conductivity for two-phase WC-Ni composites through a microstructure-based model along with key experiments10.1016/j.jmrt.2022.11.136 ↗
8. Mechanical properties and microstructural characteristics of WC-bronze-based impregnated diamond composite reinforced by nano-NbC10.1016/j.triboint.2022.107777 ↗
9. Homogeneous and structured PCD/WC-Co materials for drilling10.1016/j.diamond.2004.06.013 ↗
10. Probing the tribological behaviors of diamond-like carbon film in water-based drilling fluid environment by varying normal loads10.1016/j.diamond.2022.109552 ↗
11. Effect of carbon diffusion on friction and wear properties of diamond-like carbon in boundary base oil lubrication10.1016/j.triboint.2016.10.047 ↗
12. Improving WC-Co coating adhesive strength on rough substrate: Finite element modeling and experiment10.1016/j.jmst.2019.07.033 ↗
13. Effect of actual WC content on the reciprocating wear of a laser cladding NiCrBSi alloy reinforced with WC
14. Tribological behavior of PDC-cutter including cemented carbide and polycrystalline diamond composites produced by HPHT for drilling applications10.1016/j.ijrmhm.2024.106756 ↗
15. Dependence of wear behaviors of hardmetal YG8B on coarse abrasive types and their slurry concentrations10.1016/j.wear.2011.05.027 ↗
16. Improving drill pipe durability by wear-resistant surfacing10.1016/j.matpr.2019.12.384 ↗
17. Experimental research on improving the wear resistance and anti-friction properties of drill pipe joints10.1108/ILT-06-2021-0232 ↗
18. Microstructure and wear resistance performance of Cu–Ni–Mn alloy based hardfacing coatings reinforced by WC particles10.1016/j.jallcom.2015.09.130 ↗
19. Hardbanding failure in a heavy weight drill pipe10.1016/j.engfailanal.2011.03.014 ↗
20. (2021). Standard Test Methods and Practices for Chemical Analysis of Steel Products (Standard No. ASTM A751-21).
21. (2024). Standard Test Methods and Definitions for Mechanical Testing of Steel Products (Standard No. ASTM A370-24).
22. (2018). Standard Test Method for Brinell Hardness of Metallic Materials (Standard No. ASTM E10-18).
23. (2022). Standard Test Methods for Rockwell Hardness of Metallic Materials (Standard No. ASTM E18-22).
24. (2017). Standard Guide for Preparation of Metallographic Specimens (Standard No. ASTM E3-11 (2017)).
25. (2018). Standard Test Methods for Determining the Inclusion Content of Steel (Standard No. ASTM E45-18a).
26. (2024). Standard Test Methods for Determining Average Grain Size (Standard No. ASTM E112-24).
27. (2017). Determination of Banded Structure of Steel-Part 1: Micrographic Method Using Standards Diagrams (Standard No. GB/T 34474.1-2017).