journal article·2012-02

Observation of transcrystalline growth of PLA crystals on sisal fibre bundles and the effect of crystal structure on interfacial shear strength

Marek Prajer, Martin P. Ansell

Composite Interfaces· Volume 19· Issue 1
Publisher page

Abstract

Hot-stage microscopy was used to characterise crystal growth at the interface between sisal fibre bundles and a polylactic acid (PLA) matrix in order to better understand the mechanical properties of sisal fibre–PLA composites. Cooling rates and crystallisation temperatures and times were varied to influence crystalline morphology at the interface. Single sisal fibre bundles were evaluated in their as received state or treated with 6 wt.% caustic soda solution for 48 h at room temperature. A microbond shear test was used to characterise the shear strength of the interface as a function of fibre surface treatment. These tests were performed on sisal fibre bundles carefully embedded in flat films of PLA supported on card mounts. Fibre bundles in a PLA matrix were cooled from 180 °C at rates from 2 to 9 °C/min and then crystallised isothermally. For as received fibre bundles uneven growth of PLA spherulites occurred at all cooling rates and crystallisation temperatures. For caustic soda treated fibres, uneven spherulitic growth was observed at crystallisation temperatures at and above 125 °C. In contrast, transcrystalline growth was observed for samples cooled to 120 °C at cooling rates from 2 to 6 °C/min and then allowed to crystallise. The microbond shear strengths of untreated and caustic soda treated fibre bundles were evaluated using Weibull statistics and the caustic soda treated fibres exhibited higher interfacial shear strengths in comparison to untreated fibres, reflecting the development of a transcrystalline layer at the fibre to matrix interface.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: biodegradable polymer synthesis and properties · Natural Fiber Reinforced Composites · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. 10.1533/9781845697310.1.6210.1533/9781845697310.1.62 ↗
2. 10.1016/S0032-3861(97)10203-810.1016/S0032-3861(97)10203-8 ↗
3. 10.1016/S0079-6700(02)00012-610.1016/S0079-6700(02)00012-6 ↗
4. 10.1002/app.1046010.1002/app.10460 ↗
5. 10.1007/s10853-006-5075-410.1007/s10853-006-5075-4 ↗
6. 10.1016/S1359-835X(00)00058-010.1016/S1359-835X(00)00058-0 ↗
7. 10.1007/BF0065927810.1007/BF00659278 ↗
8. 10.1021/ma00012a01710.1021/ma00012a017 ↗
9. 10.1002/pol.1984.17022116810.1002/pol.1984.170221168 ↗
10. 10.1016/j.compositesa.2005.12.03010.1016/j.compositesa.2005.12.030 ↗
11. Katayama T · WIT Transactions on the Built Environment · 2006 · 85 · 15910.2495/HPSM06017 ↗
12. 10.1023/B:JOOE.0000038544.75554.0e10.1023/B:JOOE.0000038544.75554.0e ↗
13. 10.1016/S0266-3538(03)00099-X10.1016/S0266-3538(03)00099-X ↗
14. Prajer M
15. Nairn JA. Fracture mechanics of the microbond and pull-out tests. In: Nairn JA. Moore DR, editors. The application of fracture mechanics to polymers, adhesives and 20 composites. Amsterdam: Elsevier; 2004. 213–8.
16. 10.1017/CBO978051152520910.1017/CBO9780511525209 ↗
17. Warwicker JO · Journal of Polymer Science. Part A · 1967 · 5 · 2579