Correlation between toughness and metal volume fraction in carbon-glass fiber laminates tested under tensile loading
Source abstract
Abstract
The conducted work investigates the correlation between toughness characteristics and metal volume fraction in Fiber Metal Laminates (FMLs) subjected to tensile loads. Aerospace grade Al 7075-T6 was utilized as the varying metal alloy in the study. The metal alloy was combined with glass and carbon fiber layers to create different configurations of FMLs with varying stacking sequences. For better adhesion between metal and composite parts, aluminum layers were etched with sodium hydroxide and chromic-sulfuric acid solutions. The laminate sheets were prepared using the hand layup method which was followed by a vacuum bagging process. Specimens were cut and tested as per ASTM standard. Results of the experimentation showed that the aluminum volume fraction is directly related to the failure strain and modulus of toughness, however, inversely proportional to the stiffness characteristics of the laminates. The highest improvement of 111% in toughness parameter in comparison to pure composite laminate was reported. Finally, a comprehensive analysis on the type of fracture behavior in comparison to classical laminate theory was critically discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Fiber-reinforced polymer composites · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical and Aerospace Engineering, Air University, Islamabad, Pakistan
Computational Mechanics Group, Department of Mechanical Engineering, School of Mechanical and Manufacturing Engineering, National University of Sciences and Technology (NUST), Islamabad, Pakistan
Laboratory for Advanced Materials Processing (LAMP), National Center for Physics (NCP), Islamabad, Pakistan
References (32)
Show source-provided references
1. 10.1590/S1516-1439200600030000210.1590/S1516-14392006000300002 ↗
2. 10.1016/j.polymertesting.2019.02.00210.1016/j.polymertesting.2019.02.002 ↗
3. 10.1016/S0924-0136(96)02652-010.1016/S0924-0136(96)02652-0 ↗
4. 10.1177/152808372094710610.1177/1528083720947106 ↗
5. Chen Y · Adv Polym Technol · 2020 · 2020 · 1
6. 10.1177/073168441663260610.1177/0731684416632606 ↗
7. 10.1016/j.polymertesting.2018.07.00510.1016/j.polymertesting.2018.07.005 ↗
8. 10.1007/s40870-016-0057-310.1007/s40870-016-0057-3 ↗
9. 10.1016/j.mtcomm.2019.10083010.1016/j.mtcomm.2019.100830 ↗
10. 10.1016/j.matdes.2011.03.01110.1016/j.matdes.2011.03.011 ↗
11. 10.1016/j.compstruct.2017.02.10010.1016/j.compstruct.2017.02.100 ↗
12. 10.1016/j.compositesb.2019.10727710.1016/j.compositesb.2019.107277 ↗
13. 10.1007/s12221-021-0192-x10.1007/s12221-021-0192-x ↗
14. 10.1002/pc.2569910.1002/pc.25699 ↗
15. 10.1007/s12221-021-0656-z10.1007/s12221-021-0656-z ↗
16. 10.1007/s11661-008-9679-y10.1007/s11661-008-9679-y ↗
17. 10.1016/j.engfracmech.2017.01.00410.1016/j.engfracmech.2017.01.004 ↗
18. 10.1177/095440622091432510.1177/0954406220914325 ↗
19. 10.1177/105678952199873110.1177/1056789521998731 ↗
20. Sharma AP · Compos · 2017 · 125 · 259
21. 10.1016/j.mspro.2014.07.24210.1016/j.mspro.2014.07.242 ↗
22. Centers SM. “7075-T6 aluminium alloy.” https://www.smithmetal.com/7075.htm (accessed 06/23/2022, 2022).
23. 10.1016/j.jmrt.2017.10.01210.1016/j.jmrt.2017.10.012 ↗
24. Araldite L · Tech Data Sheet, Huntsman · 2010
25. 10.1080/0021846920802654310.1080/00218469208026543 ↗
26. 10.1109/IBCAST54850.2022.999010710.1109/IBCAST54850.2022.9990107 ↗
27. 10.1016/j.tafmec.2022.10341210.1016/j.tafmec.2022.103412 ↗
28. 10.1080/01932691.2022.214336910.1080/01932691.2022.2143369 ↗
29. 10.1016/j.finmec.2022.10014410.1016/j.finmec.2022.100144 ↗
30. 10.1109/IBCAST54850.2022.999053610.1109/IBCAST54850.2022.9990536 ↗
31. Kadhum AM · Al-Nahrain J Eng Sci · 2019 · 22 · 910.22401/ANJS.22.1.02 ↗
32. 10.1016/j.msea.2010.04.02810.1016/j.msea.2010.04.028 ↗