The properties of glass fibres after conditioning at composite recycling temperatures
Source abstract
Abstract
Results are presented on E-glass fibre properties after thermal conditioning up to 600°C. Thermal conditioning led to up to 70% strength degradation. Tensile strength and failure strain of silane-coated fibres were relatively stable up to 250°C but exhibited a precipitous drop at higher conditioning temperatures. Unsized fibres exhibited a linear decrease in strength with increasing conditioning temperature. Little significant strength regeneration was obtained from a range of acid and silane post-treatments of heat conditioned fibres. A simple analysis of the cumulative fibre strength probability resulted in more useful understanding than the Weibull method. The modulus of both fibre types increased linearly with conditioning temperature. Evidence was found of a slow time-dependent reduction of glass fibre modulus during storage in an uncontrolled environment. The results are discussed in terms of the changes in surface coating and bulk glass structure during heat conditioning and the role of the glass fibre water content.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fiber-reinforced polymer composites · Mechanical Behavior of Composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Recycling glass fibre reinforced composites – history and progress10.1016/S0034-3617(13)70151-6 ↗
2. Technology Needs To Support Advanced Composites in the UK. Written by The InterAgency Composites Group. Department for Business, Innovation & Skills. November 2009. .
3. Red C. Wind turbine blades: big and getting bigger. Composites World June 2008. .
4. Recycling wind10.1016/S0034-3617(09)70043-8 ↗
5. Recovery of value-added products from the pyrolytic recycling of glass-fibre composite waste10.1179/174602205X40504 ↗
6. Chemical recycling of glass fibre reinforced composites using subcritical water10.1016/j.compositesa.2012.06.008 ↗
7. Recycling technologies for thermoset composite materials-current status10.1016/j.compositesa.2005.05.030 ↗
8. An investigation of the factors likely to affect the strength and properties of glass fibres
9. Strength degradation of glass fibers at high temperatures10.1007/s10853-008-3140-x ↗
10. Mechanical properties of thermally-treated and recycled glass fibres10.1016/j.compositesb.2010.12.020 ↗
11. Strength of high performance glass reinforcement fiber10.1111/j.2041-1294.2012.00089.x ↗
12. The strength of glass fibre reinforcement after exposure to elevated composite processing temperatures10.1007/s10853-013-7689-7 ↗
13. The weakening of silica fibres by heat treatment
14. Influence of thermal treatment on tensile failure of basalt fibers10.1016/S0013-7944(01)00119-9 ↗
15. The influence of fibre properties of the performance of glass-fibre-reinforced polyamide 6,610.1016/S0266-3538(99)00083-4 ↗
16. Effect of silane coupling agent on mechanical performance of glass fibre10.1007/s10853-012-6960-7 ↗
17. On the application of weibull analysis to experimentally determined single fibre strength distributions10.1016/j.compscitech.2013.01.009 ↗
18. Jenkins PG, Yang L, Liggat JJ, Thomason JL. Investigation of the strength loss of E-glass fibres after thermal conditioning. J Mater Sci [submitted for publication].
19. The thermal behaviour of glass fibre investigated by thermomechanical analysis10.1007/s10853-013-7369-7 ↗
20. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
21. Mechanical characterisation of glass fibres as an indirect analysis of the effect of surface treatment10.1023/A:1004572112470 ↗
22. Tensile strength and fracture surface characterisation of sized and unsized glass fibers10.1007/s10853-005-0661-4 ↗
23. The surface chemistry of amorphous silica10.1016/S0927-7757(00)00556-2 ↗
24. Microstructural and wettability study of surface pretreated glass fibres10.1016/S0924-0136(99)00212-5 ↗
25. The structure of γ-glycidoxypropyltrimethoxysilane on glass fiber surfaces: characterization by FTIR, SEM, and contact angle measurements10.1002/pc.20585 ↗
26. Characterisation and reuse of glass fibres recycled from scrap composites by a fluidised bed process10.1016/S1359-835X(98)00008-6 ↗
27. Compaction effects in glass fibers10.1111/j.1151-2916.1961.tb15352.x ↗
28. The influence of water on the glass properties10.1023/B:GPAC.0000045916.75073.1f ↗
29. Strength increase of silica glass fibers by surface stress relaxation10.1016/j.jnoncrysol.2013.07.033 ↗
30. Dynamic fatigue of sodium-silicate glasses with high water content
31. Effect of dissolved water on the internal friction of glass10.1016/0022-3093(74)90027-1 ↗
32. Water diffusion and surface structural relaxation of silica glasses10.1016/S0022-3093(01)00648-2 ↗