Abstract
Abstract The tribological behaviors of polyurethane (PU) composite coatings filled with nano-SiO2 were investigated using a ring-on-block wear tester under different friction conditions, and the worn surfaces of nano-SiO2 filled PU coating and transfer films formed on the surface of the counterpart ring were investigated by scanning electron microscopy (SEM) and optical microscope (OM), respectively. The results show that the tribological behaviors of SiO2 filled PU coating are very sensitive to the formation of transferred films. The wear life of the SiO2 filled PU coating under water lubrication is the lowest and under liquid paraffin lubrication is the highest. The OM analyses indicated that a lubricating film can be more easily formed on the frictional surfaces under liquid paraffin lubrication; thus the lubrication condition at the rubbing surfaces can be greatly improved, leading to the decrease of the friction and wear of nano-SiO2 filled PU coating. However, water hinders the formation of transferred films and might penetrate and corrode the filler–matrix interface, which lead to the worst anti-wear property of nano-SiO2 filled PU coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Tribology and Wear Analysis · Lubricants and Their Additives · Polymer Nanocomposites and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Friction and wear properties of UHMWPE/Al2O3 ceramic under different lubricating conditions10.1016/S0043-1648(01)00647-0 ↗
2. Effects of various kinds of fillers on the tribological behavior of polytetrafluoroethylene composites under dry and oil-lubricated conditions10.1002/app.1286 ↗
3. The tribological properties of Kevlar pulp reinforced epoxy composites under dry sliding and water lubricated condition10.1016/j.wear.2006.03.014 ↗
4. Comparative investigation on the wear and transfer behaviors of carbon fiber reinforced polymer composites under dry sliding and water lubrication10.1016/j.compscitech.2004.11.009 ↗
5. Friction and wear of water lubricated PEEK and PPS sliding contacts10.1016/S0043-1648(02)00059-5 ↗
6. Tribological characteristics of nanometer Si3N4 filled poly(ether ether ketone) under distilled water lubrication10.1002/1097-4628(20010222)79:8<1394::AID-APP60>3.0.CO;2-D ↗
7. Tribological properties of epoxy nanocomposites: I. Enhancement of the wear resistance by nano-TiO2 particles10.1016/j.wear.2004.09.005 ↗
8. A study on the friction and wear behavior of PTFE filled with alumina nanoparticles10.1016/S0043-1648(03)00252-7 ↗
9. The friction and wear characteristics of nanometer ZnO filled polytetrafluoroethylene10.1016/S0043-1648(01)00816-X ↗
10. Effect of particle surface treatment on the tribological performance of epoxy based nanocomposites10.1016/S0043-1648(02)00252-1 ↗
11. Tribological behavior of PTFE film with nanodiamond10.1016/j.surfcoat.2004.07.102 ↗
12. On dry sliding friction and wear behaviour of PEEK and PEEK/SiC-composite coatings10.1016/j.wear.2005.03.017 ↗
13. Studies on the tribological behavior and transfer film–counterface bond strength for polyphenylene sulfide filled with nanoscale alumina particles10.1016/S0043-1648(99)00345-2 ↗
14. A study of the tribological behaviour of CrN, Graphit-iC and Dymon-iC coatings under oil lubrication10.1016/j.surfcoat.2004.07.078 ↗
15. Tribological behavior of the carbon fiber reinforced polyphenylene sulfide (PPS) composite coating under dry sliding and water lubrication10.1016/j.msea.2005.09.094 ↗
16. Antiwear and lubrication properties of polyurethane/polytetrafluoroethylene-bonded coating10.1002/app.11380 ↗
17. Sliding wear of polyetherimide matrix composites: I. Influence of short carbon fibre reinforcement10.1016/j.wear.2004.09.054 ↗