Glass fibers with clay nanocomposite coating: Improved barrier resistance in alkaline environment
Source abstract
Abstract
Coatings made from neat vinyl ester and nanoclay reinforced vinyl ester composites are applied onto individual glass fibers as well as rovings to evaluate their barrier resistance against alkali and moisture attack. The fibers coated with clay nanocomposites present a significantly less damage caused by the diffusing alkali ions, giving rise to a much higher residual tensile strength after aging than the fibers without coating or those with a neat polymer coating. The static fatigue test performed on individual fibers verifies the advantage of using nanoclay composite to retard the corrosion process under the combined stress and alkaline environment. Similar beneficial effects of incorporating nanoclay on residual strength are identified for impregnated fiber bundles. The above observations confirm the excellent barrier characteristics of intercalated/exfoliated nanoclay in polymer that are applied in composite structures on both the microscopic and macroscopic scales.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Polymer Nanocomposites and Properties · Tribology and Wear Analysis · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Fiber reinforced cement-based (FRC) composites after over 40years of development in building and civil engineering10.1016/j.compstruct.2008.03.006 ↗
2. Durability of GFRP bars: a critical review of the literature10.1002/pse.205 ↗
3. Long-term bond performance of GFRP bars in concrete under temperature ranging from 20°C to 80°C10.1016/j.conbuildmat.2009.12.040 ↗
4. Durability prediction for GFRP reinforcing bars using short-term data of accelerated aging tests10.1061/(ASCE)1090-0268(2006)10:4(279) ↗
5. Experimental and analytical investigation of reinforced high strength concrete continuous beams strengthened with fiber reinforced polymer10.1016/j.matdes.2009.09.041 ↗
6. Glass fiber reinforced plastic (GFRP) rebars for concrete structures10.1016/0950-0618(95)00048-8 ↗
7. Specifications of Portland cement, ASTM C150 Standard, Annual book of ASTM standards, ASTM, West Conshohocken, Pa. vol. l04.01.
8. Durability of glass fiber-reinforced polymer reinforcing bars in concrete environment10.1061/(ASCE)1090-0268(2002)6:3(143) ↗
9. Durability of E-glass/vinylester reinforcement in alkaline solution
10. Durability of glass polymer composites subject to stress corrosion10.1061/(ASCE)1090-0268(2003)7:2(109) ↗
11. Synthesis and properties of polyimide-clay hybrid10.1002/pola.1993.080311009 ↗
12. Moisture diffusion through vinyl ester nanocomposites made with montmorillonite clay10.1002/pen.11078 ↗
13. Moisture barrier characteristics of organoclay–epoxy nanocomposites10.1016/j.compscitech.2004.10.014 ↗
14. Environmental degradation of epoxy–organoclay nanocomposites due to UV exposure: Part I Photodegradation10.1016/j.compscitech.2007.03.004 ↗
15. Environmental degradation of epoxy–organoclay nanocomposites due to UV exposure: Part II Residual mechanical properties10.1016/j.compscitech.2008.03.020 ↗
16. Barrier performance of silane–clay nanocomposite coatings on concrete structure10.1016/j.compscitech.2007.10.028 ↗
17. Use of polymer/layered-silicate nanocomposite coating as water/ion barrier for concrete10.1061/(ASCE)0899-1561(2008)20:7(484) ↗
18. Nanostructured coatings of glass fibers: improvement of alkali resistance and mechanical properties10.1016/j.actamat.2006.09.020 ↗
19. Nanocomposite coatings for healing surface defects of glass fibers and improving interfacial adhesion10.1016/j.compscitech.2007.10.009 ↗
20. Sizings on alkali-resistant glass fibers: environmental effects on mechanical properties10.1021/la020778t ↗
21. Coatings for glass fibers in a cementitious matrix10.1016/j.actamat.2004.06.028 ↗
22. Aging of alkali-resistant glass and basalt fibers in alkaline solutions: evaluation of the failure stress by Weibull distribution function10.1016/j.jnoncrysol.2009.09.018 ↗
23. Mode I interlaminar fracture behavior and mechanical properties of CFRPs with nanoclay-filled epoxy matrix10.1016/j.compositesa.2006.03.001 ↗
24. Impact damage resistance of CFRP with nanoclay-filled epoxy matrix10.1016/j.compscitech.2009.04.016 ↗
25. Fatigue damage behaviors of carbon fiber-reinforced epoxy composites containing nanoclay10.1016/j.compscitech.2010.08.004 ↗
26. Quasi-static and impact fracture behaviours of CFRPs with nanoclay-filled epoxy matrix10.1016/j.compositesa.2010.11.011 ↗
27. Tensile strength of glass fibers with carbon nanotube–epoxy nanocomposite coating10.1016/j.compositesa.2009.07.005 ↗
28. Tensile strength of glass fibers with carbon nanotube–epoxy nanocomposite coating: effects of CNT morphology and dispersion state10.1016/j.compositesa.2009.12.011 ↗
29. Vijay PV, Ganga R, Kalluri R. Hygrothermal response of GFRP bars under different conditioning schemes. In: Proceedings of 1st international conference on durability of composites for construction, Sherbrooke, Quebec, Canada; August 1998. p. 243.
30. Chin JW, Haight MR. Environmental effects on composite matrix resins used in construction. In: Proceedings of 1st international conference on durability of composites for construction, Sherbrooke, Quebec, Canada; August 1998. p. 229.
31. Corrosion of E-glass fibers in acidic environments10.1016/S0266-3538(96)00158-3 ↗
32. A multifunctional nanoporous layer created on glass through a simple alkali corrosion process10.1039/c0jm01695k ↗
33. Interaction between static fatigue and zero-stress aging in E-glass fiber composites10.1061/(ASCE)1090-0268(2003)7:1(3) ↗