Abstract

Abstract Failure of composite laminates is often the result of “secondary” transverse stresses causing delamination. One well known approach to prevent such failure is to incorporate a distinct interleaf material into the interlaminar region in order to increase its fracture toughness and, consequently, its resistance to delamination. In the recent years various carbon nanotube (CNT) interleaves gained much attention. This work presents experimental study of the Mode I progressive fracture of carbon/epoxy composite laminates modified with high volume fraction, aligned, non-functionalized and functionalized CNT interleaves. The interleaves used here are thin solid sheets produced from vertically grown multiwalled CNT arrays by shear pressing method. A dry or resin infused sheet is integrated between prepreg plies prior to the laminate cure. The obtained results show that both dry and pre-infused CNT interleaves significantly, up to two times, increase the critical strain energy release rate of the baseline non-interleaved laminate. Two methods of functionalizing CNTs within the preform are explored: O2/CF4 plasma and H2SO4/KnO4 wet chemical treatments. Both methods maintain the high alignment and aspect ratio of the CNTs. Although, functionalization results in no additional GIC toughening compared to the non-functionalized interleaves, the characteristics of the fracture surfaces are dramatically different.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Carbon Nanotubes in Composites · Mechanical Behavior of Composites · Smart Materials for Construction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Interlaminar fracture toughness and toughening of laminated composite materials: a review10.1016/0010-4361(89)90211-5 ↗
2. Inhomogeneous toughening of carbon fiber/epoxy composite using electrospun polysulfone nanofibrous membranes by in situ phase separation10.1016/j.compscitech.2007.07.010 ↗
3. Electrospun nanofibre toughened carbon/epoxy composites: effects of polyetherketone cardo (PEK-C) nanofibre diameter and interlayer thickness10.1016/j.compscitech.2010.06.019 ↗
4. Influence of electrospun Nylon 6,6 nanofibrous mats on the interlaminar properties of Gr–epoxy composite laminates10.1016/j.compstruct.2011.08.019 ↗
5. Electrospun nanofibers for enhancing structural performance of composite materials10.1002/pat.1837 ↗
6. Mode I and Mode II fracture energy of MWCNT reinforced nanofibrilmats interleaved carbon/epoxy laminates10.1016/j.compscitech.2013.10.013 ↗
7. Mode I and mode II interlaminar fracture toughness of CFRP laminates toughened by carbon nanofiber interlayer10.1016/j.compscitech.2007.06.007 ↗
8. Interlaminar toughness of interleaved CFRP using non-woven veils: Part 1. Mode-I testing10.1016/j.compositesa.2011.07.016 ↗
9. Interlaminar fracture toughness of composite laminates with CNT-enhanced nonwoven carbon tissue interleave10.1016/j.compscitech.2012.09.011 ↗
10. Effects of plasma modified carbon nanotube interlaminar coating on crack propagation in glass epoxy composites10.1016/j.compositesa.2013.07.018 ↗
11. Analysis of interlaminar fracture toughness and damage mechanisms in composite laminates reinforced with sprayed multi-walled carbon nanotubes10.1016/j.matdes.2013.07.081 ↗
12. Joining prepreg composite interfaces with aligned carbon nanotubes10.1016/j.compositesa.2008.03.011 ↗
13. Interlaminar and intralaminar reinforcement of composite laminates with aligned carbon nanotubes10.1016/j.compscitech.2009.09.001 ↗
14. An investigation of Mode I and Mode II fracture toughness enhancement using aligned carbon nanotubes forests at the crack interface10.1016/j.compstruct.2013.05.051 ↗
15. Multi-scale interlaminar fracture mechanisms in woven composite laminates reinforced with aligned carbon nanotubes10.1016/j.compscitech.2014.06.003 ↗
16. Chemistry of carbon nanotubes10.1021/cr050569o ↗
17. A novel approach to fabricate high volume fraction nanocomposites with long aligned carbon nanotubes10.1016/j.compscitech.2010.07.020 ↗
18. Conformal atomic layer deposition of alumina on millimeter tall, vertically-aligned carbon nanotube arrays10.1021/am505107s ↗
19. Surface and structural characterization of multi-walled carbon nanotubes following different oxidative treatments10.1016/j.carbon.2010.08.034 ↗
20. Standard test method for Mode I interlaminar fracture toughness of unidirectional fiber-reinforced polymer matrix composites
21. On crack-initiation conditions for mode I and mode II delamination testing of composite materials10.1016/S0266-3538(00)00080-4 ↗
22. Determination of fracture surface energies by the cleavage technique10.1063/1.1729091 ↗
23. Overview on the experimental investigation of the fracture toughness in composite materials
24. A status report on delamination resistance testing of polymer–matrix composites10.1016/j.engfracmech.2007.03.012 ↗
25. Hu X, Mai Y. Mode I delamination of fibre bridging in carbon fiber epoxy composites with and without PVAL coating 1993;46:147–156.10.1016/0266-3538(93)90170-L ↗