journal article·2013-11Open access

Effects of plasma modified carbon nanotube interlaminar coating on crack propagation in glass epoxy composites

John Williams, Neil Graddage, Sameer Rahatekar

Abstract

Fibre reinforced pre-preg systems have very good in plane properties, however they are weak in their through thickness (z) direction. This research aims to address this issue by adding plasma treated carbon nanotubes (CNTs) between the prepreg plies using a simple drawdown coating procedure. The significant test result shows by coating carbon nanotubes with a relatively low areal density (1.2 g/m2) the propagation mode I toughness can be improved by up to 46%. Crack deviation leading to increased glass fibre bridging was observed for lower CNT coating concentrations explaining the improved performance. However at the highest areal coating density (2.0 g/m2) fibre bridging disappeared and a stick–slip crack response was observed resulting in lower delamination resistance. This research demonstrates a simple method to incorporate a nanointerlayer that can manipulate crack propagation, leading to increased delamination resistance.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Mechanical Behavior of Composites · Carbon Nanotubes in Composites · Smart Materials for Construction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. The impact resistance of composite materials: a review10.1016/0010-4361(91)90549-V ↗
2. Review of z-pinned composite laminates10.1016/j.compositesa.2007.08.016 ↗
3. Coupon tests on z-pinned and unpinned composite samples for damage resistant applications10.1002/masy.200750126 ↗
4. Delamination resistant laminates by z-fiber pinning: Part I manufacture and fracture performance10.1016/j.compositesa.2004.06.029 ↗
5. Mode I DCB testing of composite laminates reinforced with z-direction pins: a simple model for the investigation of data reduction strategies10.1016/S0013-7944(03)00116-4 ↗
6. Improvement of low-velocity impact and compression-after-impact performance by z-fibre pinning10.1016/j.compscitech.2006.02.029 ↗
7. Mode I interlaminar fracture toughness properties of advanced textile fibreglass composites10.1016/S1359-835X(98)00197-3 ↗
8. Improving the delamination resistance of CFRP by stitching a review10.1016/0266-3538(94)90019-1 ↗
9. Improved impact and delamination resistance through interleaving10.4028/www.scientific.net/KEM.37.317 ↗
10. Mixed-mode fracture in an interleaved carbon-fibre/epoxy composite10.1016/0266-3538(95)00062-3 ↗
11. The effect of adhesive thickness on interlaminar fracture toughness of interleaved cfrp specimens10.1016/0010-4361(89)90341-8 ↗
12. Improvement of vibration damping capacity and fracture toughness in composite laminates by the use of polymeric interleaves10.1115/1.1370385 ↗
13. Mode I interlaminar fracture of interleaved graphite/epoxy10.1177/002199839202600306 ↗
14. Mode I interfacial toughening through discontinuous interleaves for damage suppression and control10.1016/j.compositesa.2011.10.009 ↗
15. Mode II interfacial toughening through discontinuous interleaves for damage suppression and control10.1016/j.compositesa.2011.09.026 ↗
16. Exceptionally high young’s modulus observed for individual carbon nanotubes10.1038/381678a0 ↗
17. Nanobeam mechanics: elasticity, strength, and toughness of nanorods and nanotubes10.1126/science.277.5334.1971 ↗
18. Mechanical properties of carbon nanotubes: a fiber digest for beginners10.1016/S0008-6223(02)00012-X ↗
19. Specific surface area of carbon nanotubes and bundles of carbon nanotubes10.1016/S0008-6223(00)00155-X ↗
20. Influence of different carbon nanotubes on the mechanical properties of epoxy matrix composites a comparative study10.1016/j.compscitech.2005.04.021 ↗
21. Improving the dispersion and integration of single-walled carbon nanotubes in epoxy composites through functionalization10.1021/nl0342489 ↗
22. A comparative study on properties of multi-walled carbon nanotubes (MWCNTs) modified with acids and oxyfluorination10.1016/j.jfluchem.2006.10.010 ↗
23. Dispersion and functionalization of carbon nanotubes for polymer-based nanocomposites: a review10.1016/j.compositesa.2010.07.003 ↗
24. Electrical conductivity of chemically modified multiwalled carbon nanotube/epoxy composites10.1016/j.carbon.2004.08.015 ↗
25. The use of surfactants for dispersing carbon nanotubes and graphene to make conductive nanocomposites10.1016/j.cocis.2012.03.001 ↗
26. Improvement of tensile properties of poly(methyl methacrylate) by dispersing multi-walled carbon nanotubes functionalized with poly(3-hexylthiophene)-graft-poly(methyl methacrylate)10.1016/j.compscitech.2008.03.008 ↗
27. Effect of block-copolymsser dispersants on properties of carbon nanotube/epoxy systems10.1016/j.compscitech.2011.11.034 ↗
28. Radio-frequency plasma functionalization of carbon nanotubes surface O2, NH3, and CF4 treatments10.1063/1.2071455 ↗
29. Functionalization of carbon nanotubes by atomic nitrogen formed in a microwave plasma Ar+N2 and subsequent poly([varepsilon]-caprolactone) grafting10.1039/B613581C ↗
30. Sidewall functionalization of single-walled carbon nanotubes through CF4 plasma treatment and subsequent reaction with aliphatic amines10.1016/j.cplett.2005.01.042 ↗
31. Plasma treatment as a method for functionalising and improving dispersion of carbon nanotubes in epoxy resins10.1007/s10853-012-6830-3 ↗
32. Effective amino-functionalization of carbon nanotubes for reinforcing epoxy polymer composites10.1088/0957-4484/17/6/003 ↗
33. Interlaminar and intralaminar reinforcement of composite laminates with aligned carbon nanotubes10.1016/j.compscitech.2009.09.001 ↗
34. An experimental study of interlaminar shear fracture toughness of a nanotube reinforced composite10.1016/j.compositesb.2010.06.001 ↗
35. Effects of carbon nanofiller functionalization and distribution on interlaminar fracture toughness of multi-scale reinforced polymer composites10.1016/j.carbon.2011.11.001 ↗
36. Enhancing interlaminar fracture characteristics of woven CFRP prepreg composites through CNT dispersion10.1177/0021998311410472 ↗
37. The effect of adding carbon nanotubes to glass/epoxy composites in the fibre sizing and/or the matrix10.1016/j.compositesa.2010.01.001 ↗
38. Rtm processing and electrical performance of carbon nanotube modified epoxy/fibre composites10.1016/j.compositesa.2011.12.019 ↗
39. Bayer Materials Science Baytubes C150P Data sheet. ; 2012.
40. Haydale Ltd., Clos Fferws, Parc Hendre, Carmarthenshire, SA18 3BL, UK. www.Haydale.com; 2013.
41. Walters I. Methods and apparatus for particle processing with plasma. Patent No. EP2440323 (A1). ; 2010.
42. Walters I, Williams M. Particulate materials, composites comprising them, preparation and uses thereof. Patent No. WO2012076853 (A1). ; 2012.
43. Hexcel, Hexcel 913 data sheet. ; 2012.
44. The cataphoresis of suspended particles. Part I. The equation of cataphoresis10.1098/rspa.1931.0133 ↗
45. Malvern Instruments Ltd., UK, Malvern Zetasizer Nanoseries, Software version 6.20, Manual: MAN0317-5.0 ; 2009.
46. Quantitative evaluation of surfactant-stabilized single-walled carbon nanotubes: dispersion quality and its correlation with zeta potential10.1021/jp8021634 ↗
47. Zeta-potential measurements of surfactant-wrapped individual single-walled carbon nanotubes10.1021/jp070853e ↗
48. 2011
49. ASTM-D5528-01. Mode I interlaminar fracture toughness of unidirectional fiber-reinforced polymer matrix composites, technical report, American Society for Testing and Materials International; 2007.
50. Influence of the zeta potential on the dispersability and purification of single-walled carbon nanotubes10.1021/jp050781w ↗
51. Stability of multi-walled carbon nanotubes dispersion with copolymer in ethanol10.1016/S0927-7757(03)00155-9 ↗
52. Electrostatic interactions between shortened multiwall carbon nanotubes and polyelectrolytes10.1021/la026746n ↗
53. Application of centrifugation to the large-scale purification of electric arc-produced single-walled carbon nanotubes10.1021/ja062041m ↗
54. Carbon nanotube-reinforced epoxy-composites: enhanced stiffness and fracture toughness at low nanotube content10.1016/j.compscitech.2004.04.002 ↗
55. Matrix deformation and fracture in graphite reinforced epoxies
56. Investigation of fiber bridging in double cantilever beam specimens10.1520/CTR10421J ↗
57. Fracture behaviour of a rapidly cured polyethersulfone toughened carbon fibre/epoxy composite10.1016/j.compstruct.2009.09.045 ↗