article·2004-07-13

Fracture mechanisms and failure processes at stiffener run-outs in polymer matrix composite stiffened elements

Emile S. Greenhalgh, Manuel Huertas Garcia

Publisher page

Abstract

Abstract This paper describes the fractographic analyses of three stringer run-out designs which had been loaded to failure in tension. The main aims of the investigation were to deduce the failure processes in the elements, and to characterise the effect of local geometry of the stringer run-out on the failure process. The analysis showed that the critical failure mechanism in the elements was the development of +45° ply splitting at the skin surface, initially under mode I dominated intralaminar fracture. However, as these splits grew beneath the stringer foot, the mode II component increased. This led to mixed-mode delamination growth, extending parallel to the +45° ply, at the skin/adhesive interface. Subsequently, the delamination migrated through the skin via ply splits, ultimately reaching the interface between the second and third (−45°/0°) plies, in which it remained until catastrophic failure. Extending and tapering the stringer foot led to shifting of the site of the +45° ply splitting; this was attributed to in-plane tensile stresses in the skin being inhibited in the modified designs. The reduced out-of-plane support on the stiffener foot in the modified designs led to an increase in the mode I component at the delamination from the stringer tip. It also led to an increase in the degree of multi-plane delamination growth. Based on the fractographic observations, recommendations for modelling the elements were suggested.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · Material Properties and Processing · Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.