Failure behaviour of self-reinforced polypropylene at and below room temperature
Source abstract
Abstract
Abstract Self-reinforced polypropylene is a very tough material. It is even thought that its impact resistance increases with decreasing temperature. This was investigated by examining the constituent tapes and matrix. Tensile tests on both drawn polypropylene tapes and self-reinforced polypropylene were similar: the stiffness increased and the failure strain slightly decreased at low temperatures. The matrix, however, embrittled below room temperature due to the glass transition. In contrast with literature data on Izod impact resistance, the penetration impact resistance did not increase at low temperatures. At lower temperatures, the damaged area after non-penetration impact was significantly reduced. This was caused by a change in the damage mode from tape–matrix debonding to matrix cracking, as the matrix went through its glass transition. These conclusions provide the first understanding of the failure behaviour of self-reinforced polypropylene below room temperature, and can be exploited to further optimise the excellent impact resistance of self-reinforced polymers.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Polymer crystallization and properties · Mechanical Behavior of Composites · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. The science and technology of hot compaction10.1016/j.polymer.2003.11.050 ↗
2. Development of self-reinforced polymer composites10.1016/j.progpolymsci.2011.09.005 ↗
3. Single-polymer composites (SPCs): status and future trends10.1016/j.compscitech.2013.12.006 ↗
4. On the overdrawing of melt-spun isotactic polypropylene tapes10.1002/app.25128 ↗
5. Influence of postdrawing temperature on mechanical properties of melt-spun isotactic polypropylene10.1021/ma034949s ↗
6. The hot compaction of woven polypropylene tapes10.1023/A:1017540530295 ↗
7. The mechanical properties of woven tape all-polypropylene composites10.1016/j.compositesa.2006.01.003 ↗
8. The influence of weave architecture on the mechanical properties of self-reinforced polypropylene10.1016/j.compositesa.2013.06.015 ↗
9. Development and characterization of self-reinforced poly(propylene) composites: carded mat reinforcement10.1002/pat.813 ↗
10. Manufacturing and mechanical characterization of unidirectional polyethylene-fiber polyethylene-matrix composites10.1016/0266-3538(92)90086-I ↗
11. Processing of all-polypropylene composites for ultimate recyclability
12. Low velocity impact performance of recyclable all-polypropylene composites10.1016/j.compscitech.2005.11.010 ↗
13. The hot compaction behaviour of woven oriented polypropylene fibres and tapes. I. Mechanical properties10.1016/S0032-3861(02)00809-1 ↗
14. The hot compaction behaviour of woven oriented polypropylene fibres and tapes. II. Morphology of cloths before and after compaction10.1016/S0032-3861(02)00810-8 ↗
15. Tensile behaviour of intralayer hybrid composites of carbon fibre and self-reinforced polypropylene10.1016/j.compositesa.2014.01.001 ↗
16. Advanced materials enabling high-volume road transport applications of lightweight structural composite parts
17. Hybrid carbon fibre/nylon 12 single polymer composites10.1016/j.compositesa.2014.05.020 ↗
18. The hot compaction of high modulus melt-spun polyethylene fibers10.1007/BF00357801 ↗
19. Schimanski · 2002
20. The effect of processing conditions on the mechanical properties and thermal stability of highly oriented PP tapes10.1016/j.eurpolymj.2009.06.025 ↗
21. Jones RS, Riley DE. A new self-reinforced polypropylene composite. In: Proceedings of the 2nd annual conference of society of plastics engineers, automotive and composites division. Michigan, USA; 2002.
22. Effect of postdrawing temperature on structure, morphology, and mechanical properties of melt-spun isotactic polypropylene tapes10.1021/ma051223i ↗
23. The morphology of woven polypropylene tapes compacted at temperatures above and below optimum10.1023/A:1004555608836 ↗
24. On morphologies developed during two-dimensional compaction of woven polypropylene tapes10.1002/1097-4628(20001024)78:4<787::AID-APP110>3.0.CO;2-A ↗
25. The use of an interleaved film for optimising the properties of hot compacted polyethylene single polymer composites10.1016/j.polymer.2011.04.026 ↗
26. The use of interleaved films for optimising the production and properties of hot compacted, self reinforced polymer composites10.1016/j.compscitech.2007.11.003 ↗
27. The influence of process parameters on the properties of hot compacted self-reinforced polypropylene composites10.1016/j.compositesa.2014.05.022 ↗
28. Critical review of the molecular topology of semicrystalline polymers: the origin and assessment of intercrystalline tie molecules and chain entanglements10.1002/polb.20414 ↗
29. Ward · 2004
30. Molecular model of drawing polyethylene and polypropylene10.1007/BF00550305 ↗