Thickness tapering of composite laminates is a common strategy for efficient and lightweight composite structures. The termination of specific plies necessary to achieve such tapering is well known to introduce sites for delamination initiation in laminates. This propensity for delamination is highly dependent on the thickness of the terminated ply, which presents a significant challenge in using thicker materials to improve the production rate of large-scale composite structures. In this work, the effectiveness of ply scarfing in improving the compressive failure stress of tapered laminates made using thick, unidirectional non-crimp fabrics (NCF) was experimentally investigated for the first time. Unidirectional tapered laminates were manufactured using two different NCFs with fibre areal weights of 620 and 1070 g/m2 via resin infusion. Specimens made of the 1070 g/m2 material which incorporated a ply terminated using the ply scarfing method were compared with those including plies terminated using the conventional ply-drop method. which incorporated a ply terminated using the ply scarfing method. The compression failure behaviour of the specimens was analysed using a high-speed camera. The results showed that ply scarfing suppressed delamination of the belt plies under compression and increased the failure stress by ∼60%. Furthermore, the tapered geometry of the terminated ply’s end was effective in preventing the void entrapment at the ply drop and significantly reducing the manufacturing variability.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Textile materials and evaluations · Structural Analysis of Composite Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. The study of tapered laminated composite structures: a review10.1016/S0266-3538(00)00138-X ↗
2. Effect of through-thickness tensile and compressive stresses on delamination propagation fracture energy10.1520/CTR10593J ↗
3. Delamination in asymmetrically tapered composites loaded in tension10.1016/0263-8223(96)00044-X ↗
4. Delamination of tapered composite structures10.1016/0013-7944(89)90241-5 ↗
5. Influence of internally dropped-off plies on the impact damage of asymmetrically tapered laminated CFRP10.1016/j.compositesa.2014.09.024 ↗
6. Influence of realistic ply-drop geometries on interlaminar stresses in tapered laminates10.1520/STP14030S ↗
7. Enhancement of tensile strength of tapered laminates by utilizing thin-ply composites10.1016/j.compositesb.2022.110372 ↗
8. Analysis of thickness-tapered unidirectional composite compression specimens10.1177/002199839703102204 ↗
9. Experimental study of thickness-tapered unidirectional composite compression specimens10.1007/BF02328577 ↗
10. Compressive failure of laminates containing an embedded wrinkle; experimental and numerical study10.1016/j.compositesa.2015.03.012 ↗
11. New model to predict static strength of tapered laminates10.1016/0010-4361(95)90414-U ↗
12. Failure mechanisms under compression loading in composites with designed out-of-plane fibre waviness10.1179/1743289812Y.0000000019 ↗
13. Compressive strength of composite laminates with terminated internal plies10.1016/j.compositesa.2004.10.024 ↗
14. Novel tape termination method for automated fibre placement : cutting characteristics and delamination suppression10.1016/j.compositesa.2020.106023 ↗
15. Gordon T, Xu X, Kawashita L, Wisnom MR, Hallett SR, Kim BC. Delamination suppression in tapered unidirectional laminates with multiple ply drops using a tape scarfing technique. Compos Part A Appl Sci Manuf 2021;150. https://doi.org/10.1016/j.compositesa.2021.106627.10.1016/j.compositesa.2021.106627 ↗
16. Suppression of delamination at ply drops in tapered composites by ply chamfering10.1177/0021998305053459 ↗
17. Vacuum assisted resin transfer molding (VARTM) in polymer matrix composites
18. D6641/D6641M-14. Standard test method for compressive properties of polymer matrix composite materials using a combined loading compression (CLC)
19. An improved technique for compression testing of unidirectional fibre-reinforced plastics; development and results10.1016/S0010-4361(94)80006-5 ↗
20. Temperature effects on mixed mode I/II delamination under quasi-static and fatigue loading of a carbon/epoxy composite10.1016/j.compositesa.2015.05.016 ↗
21. Asp LE, Edgren F, Anders S. Effects of stitch pattern on the mechanical properties of non-crimp fabric composites. European Conference on Composite Materials, ECCM11, Rhodes, Greece, Rhodes, Greece; 2004.
22. Compression failure mechanisms in unidirectional composites10.1177/002199839202601804 ↗
23. Compressive failure of fibre composites10.1016/0022-5096(93)90068-Q ↗
24. An experimental study of fibre waviness and its effects on compressive properties of unidirectional NCF composites10.1016/j.compositesa.2018.02.013 ↗
25. Comparison of analytical approaches predicting the compressive strength of fibre reinforced polymers