Metal reinforcements in polymer matrix composites (PMC) provide enhanced architectural freedom and functional capabilities at low cost, but a weak interfacial bonding limits their applications. We utilised Plasma Electrolytic Oxidation (PEO) to deliver 2D Al2O3/Al woven cores used as PMC reinforcements. Alumina coatings reduced fibre tensile strength and modulus but significantly enhanced the epoxy-fibre interfacial strength from ∼ 12 MPa to ∼ 33 MPa, changing the failure mode of the composite from interfacial debonding to rupture due to the enhanced resistance of the epoxy-Al2O3 interface. The optimised bonding of hybrid Al2O3/Al fibre reinforcements s increased composites’ specific flexural modulus (Ef /ρ) by ∼ 58%. The study demonstrated the utility of PEO-based approach in the preparation of hybrid reinforcements to polymer matrix composites with enhanced mechanical behaviour.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Mechanical Behavior of Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Callister · 2011
2. Clyne · 2019
3. Current status of carbon fibre and carbon fibre composites recycling10.1016/j.compositesb.2020.108053 ↗
4. Joining of carbon fibre reinforced polymer (CFRP) composites and aluminium alloys-A review10.1016/j.compositesa.2017.06.007 ↗
5. Fabrication and structural performance of periodic cellular metal sandwich structures10.1016/S0266-3538(03)00266-5 ↗
6. Mechanical and conductive properties of metal fibre-filled polymer composites10.1016/0010-4361(79)90010-7 ↗
7. Mechanisms of interfacial adhesion in metal-polymer composites-Effect of chemical treatment10.1016/j.compositesa.2011.03.019 ↗
8. Processing of ceramic-metal composites10.1179/1743676111Y.0000000073 ↗
9. Reactive Synthesis of Ceramic-Metal Composites10.1002/adem.201800324 ↗
10. Use of LCA to evaluate the environmental benefits of substituting chromic acid anodizing (CAA)10.1016/j.jclepro.2007.06.010 ↗
11. Plasma electrolysis for surface engineering10.1016/S0257-8972(99)00441-7 ↗
12. Review of the soft sparking issues in plasma electrolytic oxidation10.3390/met8020105 ↗
13. Introduction to plasma electrolytic oxidation—An overview of the process and applications10.3390/coatings10070628 ↗
14. The influences of duty cycle on the bonding strength of AZ31B magnesium alloy by microarc oxidation treatment10.1016/j.surfcoat.2010.05.016 ↗
15. Adhesive bond strength of PEO coated AA6060-T610.1016/j.surfcoat.2021.127898 ↗
16. Oxide ceramic coatings on aluminium alloys produced by a pulsed bipolar plasma electrolytic oxidation process10.1016/j.surfcoat.2004.10.147 ↗
17. An investigation into the mechanical and tribological properties of plasma electrolytic oxidation and hard-anodized coatings on 6082 aluminum alloy10.1016/j.msea.2011.06.032 ↗
18. Microstructure and multi-scale mechanical behavior of hard anodized and plasma electrolytic oxidation (PEO) coatings on aluminum alloy 505210.1016/j.surfcoat.2012.07.056 ↗
19. Enhancement in specific strength of open cell aluminium foams through plasma electrolytic oxidation treatment10.1016/j.scriptamat.2013.11.012 ↗
20. Effect of Plasma Electrolytic Oxidation coating on the specific strength of open-cell aluminium foams10.1016/j.matdes.2011.03.053 ↗
21. Porosity in plasma electrolytic oxide coatings10.1016/j.actamat.2005.12.029 ↗
22. Tailored aluminium oxide layers by bipolar current adjustment in the Plasma Electrolytic Oxidation (PEO) process10.1016/j.surfcoat.2006.09.005 ↗
23. Plasma electrolytic oxidation of pre-anodized aluminium10.1016/j.corsci.2009.08.004 ↗
24. Influence of the cathodic pulse on the formation and morphology of oxide coatings on aluminium produced by plasma electrolytic oxidation10.2478/v10172-012-0180-7 ↗
25. Delay in micro-discharges appearance during PEO of Al: Evidence of a mechanism of charge accumulation at the electrolyte/oxide interface10.1016/j.apsusc.2017.03.088 ↗
26. The role of cathodic current in PEO of aluminum: Influence of cationic electrolyte composition on the transient current-voltage curves and the discharges optical emission spectra10.1016/j.apsusc.2016.10.115 ↗
27. The role of cathodic current in plasma electrolytic oxidation of aluminum: Phenomenological concepts of the “soft sparking” mode10.1021/acs.langmuir.7b02284 ↗
28. Role of cathodic current in plasma electrolytic oxidation of Al: A quantitative approach to in-situ evaluation of cathodically induced effects10.1016/j.electacta.2019.05.161 ↗
29. Changes induced by process parameters in oxide layers grown by the PEO process on Al alloys10.1016/j.surfcoat.2011.01.046 ↗
30. Effects of electrical parameters on plasma electrolytic oxidation of aluminium10.1016/j.surfcoat.2013.01.029 ↗
31. The influence of pulse timing and current mode on the microstructure and corrosion behaviour of a plasma electrolytic oxidation (PEO) coated AM60B magnesium alloy10.1016/j.jallcom.2012.07.003 ↗
32. High growth rate, wear resistant coatings on an Al-Cu-Li alloy by plasma electrolytic oxidation in concentrated aluminate electrolytes10.1016/j.surfcoat.2014.12.078 ↗
33. D7264, d7264m-21. · 2015
34. A microbond method for determination of the shear strength of a fiber/resin interface10.1016/0266-3538(87)90059-5 ↗
35. Characterization of fiber/matrix interface strength: applicability of different tests, approaches and parameters10.1016/j.compscitech.2004.07.003 ↗
36. Measurement of the ultimate shear strength of a metal-ceramic interface10.1016/0001-6160(89)90120-X ↗
37. Suggested mechanism for the MAO ceramic coating on aluminium substrates using bipolar current mode in the alkaline silicate electrolytes10.1016/j.apsusc.2014.04.120 ↗
38. Relaxation kinetics of plasma electrolytic oxidation coated Al electrode: Insight into the role of negative current10.1021/acs.jpcc.0c07714 ↗
39. In-situ SEM analysis of brittle plasma electrolytic oxidation coating bonded to plastic aluminum substrate: microstructure and fracture behaviors10.1016/j.matchar.2019.109851 ↗
40. Cracking and decohesion of a thin Al2O3 film on a ductile Al-5% Mg substrate10.1016/j.actamat.2004.10.005 ↗
41. Asquith D, Tai Y, Wong C, Yates J, Matthews A, Yerokhin A. Measurement of the interfacial shear strength of a PEO coated aluminium alloy. in Proceedings of the 17th European Conference on Fracture (J. Pokluda, P. Sandera, P. Lukas, I. Dlouhy - editors), Brno, Czech Republic; 2008, Curran Associates, Inc. (2011). Vol. 1, pp. 2105-2111. (ISBN: 978-1-61782-319-0).
42. Nano-structured interpenetrating composites with enhanced Young’s modulus and desired Poisson’s ratio10.1016/j.compositesa.2016.10.006 ↗
43. Cyclic compression behavior and energy dissipation of aluminum foam-polyurethane interpenetrating phase composites10.1016/j.compositesa.2015.07.016 ↗
44. Interpenetrating phase composites10.1111/j.1151-2916.1992.tb04138.x ↗
45. Influence of coating morphology on adhesive bonding of titanium pre-treated by plasma electrolytic oxidation10.1016/j.surfcoat.2016.01.042 ↗
46. How can adhesion be determined from micromechanical tests?10.1016/S1359-835X(00)00055-5 ↗