Impact of Fire-Retardant coating on the residual compressive strength of hybrid Fibre-Reinforced polymer tubes exposed to elevated temperature
Source abstract
Abstract
Enhancing the fire resistance of fibre‐reinforced polymer (FRP) composites is vital for ensuring structural safety in fire‐prone infrastructures. This study investigates the thermal degradation and residual compressive strength of filament-wound hybrid fibre-reinforced polymer (HFRP) tubes exposed to temperatures ranging from 25 °C to 350 °C. The tubes, composed of 50 % carbon fibre and 50 % E-glass fibre, with a 60:40 fibre–resin ratio, were subjected to thermal conditioning to simulate real-world fire exposure. For uncoated tubes, a balance between resin post-curing and pyrolytic degradation preserves compressive strength up to 200 °C, but strength sharply decreases beyond this threshold due to intensified pyrolysis, with virtually no residual strength at 350 °C. Fire-retardant coatings, Nullifire SC902, activate above 200 °C, providing limited protection, and the samples retain 20–21 % of their original compressive strength at 350 °C. As revealed by complementary Scanning Electron Microscopy (SEM), Thermogravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC), and Fourier Transform Infrared Spectroscopy (FTIR) analyses, key degradation mechanisms include matrix degradation and cracking and fibre exposure. Overall, the fire-retardant coating offers some benefits at higher temperatures, but its effectiveness is limited by activation thresholds and prolonged exposure. The findings show the need for further optimisation of fire-resistant systems for HFRP composites to improve their safety and durability in fire-prone applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fire effects on concrete materials · Structural Behavior of Reinforced Concrete · Flame retardant materials and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (84)
Show source-provided references
1. Hybrid fibre reinforced polymer and seawater sea sand concrete structures: A systematic review on short-term and long-term structural performance10.1016/j.conbuildmat.2021.124335 ↗
2. Harle · 2024
3. Durability of FRP-to-concrete bonded joints subjected to 110 months accelerated laboratory and field exposure10.1016/j.engstruct.2024.117681 ↗
4. Tensile properties of GFRP laminates after exposure to elevated temperatures: Effect of fiber configuration, sample thickness, and time of exposure10.1016/j.compstruct.2020.111971 ↗
5. Aerodynamic Performance of an Adaptive GFRP Wind Barrier Structure for Railway Bridges10.3390/ma13184214 ↗
6. Bond between sand-coated GFRP bars and normal-strength, self-compacting, and fiber-reinforced concrete under seawater and alkaline solution10.1061/JCCOF2.CCENG-3987 ↗
7. Bond durability between steel-FRP composite bars and concrete under seawater corrosion environments10.1016/j.conbuildmat.2024.135456 ↗
8. Carbon emissions of durable FRP composite structures in civil engineering10.1016/j.engstruct.2024.118482 ↗
9. Durability of glass FRP bar‐reinforced seawater–sea sand concrete beams under sustained loading in a subtropical coastal environment10.1002/pc.28717 ↗
10. Analysis-oriented stress–strain model of CRFP-confined circular concrete columns with applied preload10.1617/s11527-018-1169-0 ↗
11. Short-term durability of GFRP stirrups under wet-dry and freeze–thaw cycles10.1016/j.conbuildmat.2023.132533 ↗
12. Durability of FRP bars and FRP bar reinforced seawater sea sand concrete structures in marine environments10.1016/j.conbuildmat.2022.128898 ↗
13. Mechanical properties of FRP materials at elevated temperature–definition of a temperature conversion factor for design in service conditions10.1016/j.conbuildmat.2023.130298 ↗
14. Impact performance and damage assessment of GFRP-RC columns at high temperatures: a numerical insight
15. Effect of strain rate on compressive behaviour of high-strength concrete after exposure to elevated temperatures10.1016/j.firesaf.2016.04.006 ↗
16. Axial crush behavior and energy absorption capability of foam-filled GFRP tubes under elevated and high temperatures10.1016/j.compstruct.2016.04.028 ↗
17. An experimental study of the mechanical properties of fibre reinforced polymer (FRP) and steel reinforcing bars at elevated temperatures10.1016/j.compstruct.2006.04.069 ↗
18. Modeling of thermal responses for FRP composites under elevated and high temperatures10.1016/j.compscitech.2007.05.039 ↗
19. Fire resistance design of un-protected FRP-strengthened RC beams10.1617/s11527-016-0865-x ↗
20. Fire resistance performance of FRP rebar reinforced concrete columns10.4334/IJCSM.2009.3.2.111 ↗
21. Effects of UV radiation, moisture and elevated temperature on mechanical properties of GFRP pultruded profiles10.1016/j.conbuildmat.2019.117137 ↗
22. The performance of near-surface mounted CFRP strengthened RC beam in fire10.1016/j.firesaf.2017.04.031 ↗
23. Thermal behavior of fire-exposed concrete slabs reinforced with fiber-reinforced polymer bars
24. Mouritz · 2007
25. Mechanical properties and bond characteristics of different fiber reinforced polymer rebars at elevated temperatures10.1016/j.conbuildmat.2017.03.113 ↗
26. Hygrothermal resistance of pultruded carbon, glass and carbon/glass hybrid fiber reinforced epoxy composites10.1016/j.conbuildmat.2021.125710 ↗
27. Tests on seawater and sea sand concrete-filled CFRP, BFRP and stainless steel tubular stub columns10.1016/j.tws.2016.08.016 ↗
28. Behavior of recycled aggregate concrete-filled basalt and carbon FRP tubes10.1016/j.conbuildmat.2015.12.068 ↗
29. Bond performance between sand coated hybrid glass-carbon FRP tubes and seawater sea sand concrete after exposure to elevated temperatures10.1016/j.conbuildmat.2024.137984 ↗
30. Effect of fiber hybrid mode on the tension–tension fatigue performance for the pultruded carbon/glass fiber reinforced polymer composite rod10.1016/j.engfracmech.2021.108208 ↗
31. Combined effects of sustained bending loading, water immersion and fiber hybrid mode on the mechanical properties of carbon/glass fiber reinforced polymer composite10.1016/j.compstruct.2021.115060 ↗
32. Combined effects of cyclic/sustained bending loading and water immersion on the interface shear strength of carbon/glass fiber reinforced polymer hybrid rods for bridge cable10.1016/j.conbuildmat.2021.125587 ↗
33. Effects of rod size and fiber hybrid mode on the interface shear strength of carbon/glass fiber composite rods exposed to freezing-thawing and outdoor environments10.1016/j.jmrt.2021.08.088 ↗
34. Effect of fiber hybridization types on the mechanical properties of carbon/glass fiber reinforced polymer composite rod10.1080/15376494.2021.1974620 ↗
35. Design, preparation and mechanical properties of novel glass fiber reinforced polypropylene bending bars10.1016/j.conbuildmat.2024.136455 ↗
36. Hybrid effect on tensile properties of FRP rods with various material compositions10.1016/j.compstruct.2006.04.065 ↗
37. Fiber fracture in hybrid composite systems10.1016/0266-3538(94)90156-2 ↗
38. Demonstration of pseudo-ductility in high performance glass/epoxy composites by hybridisation with thin-ply carbon prepreg10.1016/j.compositesa.2013.04.006 ↗
39. Tree-based machine learning approach to modelling tensile strength retention of Fibre Reinforced Polymer composites exposed to elevated temperatures10.1016/j.compositesb.2023.111132 ↗
40. Mechanical property evolution and life prediction of carbon fiber and pultruded carbon fiber reinforced polymer plate exposed to elevated temperatures10.1002/pc.25782 ↗
41. Effect of temperature on material properties of carbon fiber reinforced polymer (CFRP) tendons: Experiments and model assessment10.3390/ma12071025 ↗
42. Thermal Expansion of Glass Fabric‐Epoxy Composites at Cryogenic Temperatures, AIP Conference Proceedings, American Institute of
43. Enhancing compressive behaviour of seawater sea sand concrete filled hybrid carbon-glass FRP tubes exposed to seawater: Effect of thickness10.1016/j.engstruct.2024.119052 ↗
44. Influence of immersion in water under hydraulic pressure on the interfacial shear strength of a unidirectional carbon/glass hybrid rod10.1016/j.polymertesting.2018.10.004 ↗
45. Filament-wound glass-fibre reinforced polymer composites: Potential applications for cross arm structure in transmission towers
46. Tensile strength retention of fibre-reinforced polymer composites exposed to elevated temperatures: A meta-analysis review10.1016/j.conbuildmat.2024.137150 ↗
47. Effects of various temperatures on the mechanical strength of GFRP box profiles10.1016/j.conbuildmat.2016.09.130 ↗
48. Experimental investigation and probabilistic models for residual mechanical properties of GFRP pultruded profiles exposed to elevated temperatures10.1016/j.compstruct.2018.12.032 ↗
49. Experimental and numerical investigations on the post-heating performance of concrete-filled pultruded GFRP tubes under concentric compression10.1016/j.compstruct.2024.117914 ↗
50. Modeling of strength degradation for fiber-reinforced polymer composites in fire10.1177/0021998309344642 ↗
51. Residual compressive section capacity of filament wound carbon, glass, and basalt fibre-reinforced polymer tubes: Influence of elevated temperatures
52. Residual compressive section capacity of filament wound carbon, glass, and basalt fibre-reinforced polymer tubes: Influence of elevated temperatures10.1016/j.compstruct.2022.116490 ↗
53. Fire structural modeling of polymer composites with passive thermal barrier10.1177/0734904109340878 ↗
54. Flame retardant polymer composites10.1007/s12221-015-0705-6 ↗
55. Effect of boron carbide nanoparticles on the fire reaction and fire resistance of carbon fiber/epoxy composites10.1016/j.polymer.2013.07.038 ↗
56. Evaluating the influence of varied fire-retardant surface coatings on post-heat flexural properties of glass/epoxy composites10.1016/j.firesaf.2013.01.009 ↗
57. A large-scale fire test of an immersed tunnel under the protection of fire resistive coating10.1016/j.tust.2021.103844 ↗
58. Mechanical strength of CFRP and GFRP composites filled with APP fire retardant powder exposed to elevated temperature10.1016/j.firesaf.2020.103178 ↗
59. Effect of intumescent paint coating on mechanical properties of FRP bars at elevated temperature10.1016/j.polymertesting.2018.08.020 ↗
60. Residual compressive strength of seawater sea sand concrete filled hybrid carbon-glass fibre reinforced polymer tubes under seawater: effects of fibre type and orientation10.1016/j.jobe.2023.106383 ↗
61. Residual compressive strength of filament wound hybrid glass/carbon fibre reinforced polymer tubes after exposure to elevated temperature10.1016/j.compstruct.2023.117050 ↗
62. ASTM, ASTM E 2550-17. Standard Test Method for Thermal Stability by Thermogravimetry, West Conshohocken, USA; (2017).
63. ASTM, ASTM D3822/D3822M-14. Standard Test Method for Tensile Properties of Single Textile Fibers, West Conshohocken, USA; (2020).
64. ASTM, ASTM D638-22. Standard Test Method for Tensile Properties of Plastics. , West Conshohocken, USA; 2022; (2022).
65. ASTM, ASTM D695-23. Standard Test Method for Compressive Properties of Rigid Plastics, West Conshohocken, USA; 2023; (2023).
66. ASTM, ASTM D2240-15. Standard Test Method for Rubber Property—Durometer Hardness, West Conshohocken, USA; 2021; (2021).
67. ASTM, ASTM D2196-20. Standard Test Methods for Rheological Properties of Non-Newtonian Materials by Rotational Viscometer, West Conshohocken, Philadelphia. 802 Pa 19103; (2020).
68. Performance of glass fiber reinforced polymer bars under elevated temperatures10.1016/j.compositesb.2012.01.034 ↗
69. Residual strength testing in pultruded FRP material under a variety of temperature cycles and values10.1016/j.compstruct.2015.07.034 ↗
70. Effect of post-cure on the glass transition temperature and mechanical properties of epoxy adhesives10.1080/01694243.2013.790294 ↗
71. J.-P. Pascault, H. Sautereau, J. Verdu, R.J. Williams, Thermosetting polymers, CRC press, (2002).10.1201/9780203908402 ↗
72. Epoxy network structure effect on physical aging behavior10.1002/app.1986.070320424 ↗
73. Effect of cure temperature on the glass transition temperature and mechanical properties of epoxy adhesives10.1080/00218464.2013.779559 ↗
74. Thermal stability and lifetime estimates of a high temperature epoxy by Tg reduction10.1016/j.polymdegradstab.2013.08.001 ↗
75. Isothermal degradation and thermooxidative degradation of an epoxy powder coating10.1007/s10973-005-0630-9 ↗
76. Effect of postcuring immersed in water under hydraulic pressure on fatigue performance of large‐diameter pultruded carbon/glass hybrid rod10.1111/ffe.12978 ↗
77. Effect of thickness and reinforcement configuration on flexural and impact behaviour of GFRP laminates after exposure to elevated temperatures10.1016/j.compositesb.2018.08.054 ↗
78. Temperature effect on the mechanical properties of carbon, glass and carbon–glass FRP laminates10.1016/j.conbuildmat.2014.11.020 ↗
79. Laminate theory analysis of composites under load in fire10.1177/0021998305055543 ↗
80. Models for predicting elastic modulus and tensile strength of carbon, basalt and hybrid carbon-basalt FRP laminates at elevated temperatures10.1016/j.conbuildmat.2016.03.175 ↗
81. Effect of temperature on strength and stiffness properties of near-surface mounted FRP reinforcement10.1016/j.compositesb.2013.10.055 ↗
82. Effect of fire on FRP reinforced concrete members10.1016/S0263-8223(02)00045-4 ↗
83. Mechanical properties of pultruded carbon fibre-reinforced polymer (CFRP) plates at elevated temperatures10.1016/j.engstruct.2011.03.006 ↗
84. Tensile strength modeling of glass fiber—polymer composites in fire10.1177/0021998307075461 ↗