Novel hybrid material z-pins for balanced mode I to mode II delamination bridging
Source abstract
Abstract
Effective through-Thickness Reinforcement (TTR) for prepreg-based laminated composite structures can be achieved by use of Z-pins. Z-pins made from carbon-fibre reinforced rods provide a substantial enhancement of interlaminar fracture toughness in Mode I regimes, whereby the TTR undergoes complete frictional pull-out. However, the performance of carbon-fibre Z-pins in mode II is severely limited by their tendency to experience brittle failure. On the other hand, metal (e.g. steel) z-pins strongly enhance the interlaminar fracture toughness in Mode II-dominated regimes, as they can resist large sliding displacements because of their ductile response. Nevertheless, untreated metal TTR usually experiences low friction during pull-out, hence providing a limited toughening effect for mode I delamination. This paper presents a novel TTR architecture achieved by hybrid z-pins, which consist of a ductile core embedded into a carbon-fibre composite sheath. The key objective is to achieve a “balanced” toughening performance across the full mode-mixity range, combining the benefits provided by monolithic carbon-fibre and ductile metal TTR. The delamination-bridging performance of the novel hybrid z-pins is characterised using an Arcan-type rig, for regimes spanning from pure Mode I to pure Mode II. It is demonstrated that the novel hybrid z-pins provide a substantial enhancement of the interlaminar fracture toughness across the full range of mode-mixity conditions, in contrast to monolithic pins made of single-material constituents.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Composite Structure Analysis and Optimization · Advanced Fiber Optic Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Z-pin insertion process for through-thickness reinforced thermoplastic composites10.1177/0021998318781233 ↗
2. Through-the-thickness reinforcement for composite structures: A review
3. Z-Pin composites: aerospace structural design considerations10.1061/(ASCE)AS.1943-5525.0000078 ↗
4. Laminates · 2009
5. Influence of stitching on the out-of-plane behavior of composite materials – A mechanistic review10.1177/00219983211009290 ↗
6. A.P. Mouritz, Review of z-pinned composite laminates, Compos.: Part A, 38, 2007, Doi: 10.1016/j.compositesa.2007.08.016.10.1016/j.compositesa.2007.08.016 ↗
7. S.L. Huang, R.J. Richey, E.W. Deska, Cross reinforcement in a GR/EP laminate. Winter Annu. San Fr. Calif: Am. Soc. Mech. Eng., 1978.
8. Automated method of transverse reinforcement of composites by short fibers10.1007/BF00811696 ↗
9. Transversal reinforcement of composite materials using ultrasonic vibrations10.1007/BF00616801 ↗
10. Mechanisms of crack bridging by composite and metallic rods10.1016/j.compositesa.2004.03.006 ↗
11. Delamination of Z-pinned carbon fibre reinforced laminates10.1016/j.compscitech.2004.12.018 ↗
12. Delamination resistant laminates by Z-Fiber® pinning: Part I manufacture and fracture performance10.1016/S1359-835X(04)00180-0 ↗
13. Experimental characterisation of mixed mode traction–displacement relationships for a single carbon composite Z-pin10.1016/j.compscitech.2014.02.001 ↗
14. Improving the delamination bridging performance of Z-pins through the use of a ductile matrix10.1016/j.compositesa.2022.107241 ↗
15. B. M'membe, M. Yasaee, S.R. Hallett, I.K. Partridge, Effective use of metallic z-pins for composites' through thickness reinforcement, Compos. Sci. Technol. 175, 2019, Doi: 10.1016/j.compscitech.2019.02.024.10.1016/j.compscitech.2019.02.024 ↗
16. Snubbing effects in the pullout of a fibrous rod from a laminate10.1080/15376490490493899 ↗
17. Comparative study of metal and composite z-pins for delamination fracture and fatigue strengthening of composites10.1016/j.engfracmech.2016.01.003 ↗
18. B. M'membe, Novel Through Thickness Reinforcement Development for Composite Materials, PhD, Department of Aerospace Engineering, University of Bristol, 2016.
19. Improving the delamination bridiging performance of fibrous composite Z-pins
20. Pseudo-ductile behavior of fibrous composite Z-pins10.1016/j.compositesa.2024.108009 ↗
21. Hexcel, “HexPly 8552,” in Product Data Sheet, ed, 2020.
22. B. M'membe, J.K. Lander, R.C. Backhouse, S. . Hallett, M. Yasaee, I.K. Partridge, “US2017057201A1 Composite Component,” 2017.
23. Thyssenkrupp materials (UK). “Stainless steel 316L data sheet”. 2017. Available at: https://www.thyssenkrupp-materials.co.uk/stainless-steel-316l-14404.html.
24. Ulbrich. “Nitinol (Nickel-Titanium) Alloy Datasheet”. 2015.
25. Toyobo Corporation. “PBO Fibre Zylon Technical Information”. 2005.
26. Shimadzu Scientific Instruments. “AGS-X Series Universal Electromechanical Test Frames.” https://www.ssi.shimadzu.com/products/universal-tensile-testing/ags-x.html.
27. A novel model of delamination bridging via Z-pins in composite laminates10.1016/j.ijsolstr.2014.05.017 ↗
28. Cartié · 2000