journal article·2026-02

Interfacial optimization strategy of local point relax facilitates synergistic enhancement of strength and toughness in 2.5D SiCf/SiC composites

Zhaoliang Guo, Hongyun Luo, Qian Chen, Jie Cui, Jiaping Zhang, Jing Chen, Fule Qin, Chaoli Ma

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Fiber-reinforced polymer composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (68)

Show source-provided references
1. Flexural failure mechanism of 2.5D woven SiCf/SiC composites: combination of acoustic emission, digital image correlation and X-ray tomography10.1016/j.coco.2021.100921 ↗
2. Properties evolution and damage mechanism of SiC/SiC composites after thermal shock at 1300°C10.1016/j.ceramint.2024.06.263 ↗
3. Ultra-high temperature ablation behaviour of 2.5D SiC/SiC under an oxy-acetylene torch10.1016/j.corsci.2022.110263 ↗
4. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
5. Properties of multilayered interphases in SiC/SiC chemical‐vapor‐infiltrated composites with “Weak” and “strong” interfaces10.1111/j.1151-2916.1998.tb02627.x ↗
6. An overview of tensile and shear failure mechanisms of silicon carbide-based ceramic matrix composites10.1016/j.jmrt.2024.09.254 ↗
7. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre–matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
8. A novel strategy to prepare BN interface and its effects on microstructure and properties of SiCw/BN/SiC composites10.1016/j.jallcom.2020.158218 ↗
9. Mechanical properties of SiCf/SiC composites with PyC and the BN interface10.1016/j.ceramint.2015.02.041 ↗
10. Effect of BN/SiC interfacial coatings on the tensile properties of SiC/SiC minicomposites fabricated by PIP10.1016/j.ceramint.2020.06.292 ↗
11. Stress engineering of SiCf/SiC composites: Interfacial stress adjustment and its effects on tensile behaviors of UD SiCf/SiC composites fabricated by hybrid CVI and PIP methods10.1016/j.compositesb.2024.111711 ↗
12. Effect of a boron nitride interphase that debonds between the interphase and the matrix in SiC/SiC composites10.1111/j.1551-2916.2004.00104.x ↗
13. The improvement on mechanical and thermal properties of SiC/SiC composites via introducing CNTs into PyC interface10.1016/j.msea.2015.04.006 ↗
14. Influence of boron nitride nanotubes on the damage evolution of SiCf/SiC composites10.1016/j.jeurceramsoc.2018.06.030 ↗
15. Understanding interfacial bonding properties and mechanical properties of in situ synthesis of Cf/ZrB2–ZrC–SiC composite
16. Preparation of SiC fiber-reinforced SiC composites10.1016/j.jmatprotec.2003.10.028 ↗
17. Influence of interface characteristics on the mechanical properties of Hi-Nicalon type-S or Tyranno-SA3 fiber-reinforced SiC/SiC minicomposites10.1111/j.1744-7402.2010.02485.x ↗
18. Influence of texture and thickness of pyrocarbon coatings as interphase on the mechanical behavior of specific 2.5D SiC/SiC composites reinforced with Hi-Nicalon S fibers10.3390/coatings12050573 ↗
19. Carbon nanotube-based hierarchical composites: a review10.1039/c000041h ↗
20. Disclosing residual thermal stresses in UHT fibre-reinforced ceramic composites and their effect on mechanical behaviour and damage evolution10.1016/j.compositesb.2022.110369 ↗
21. Residual stress measurements in melt infiltrated SiC/SiC ceramic matrix composites using Raman spectroscopy10.1016/j.jeurceramsoc.2018.02.013 ↗
22. Damage behavior and toughening mechanism of SiCf/SiC-Ti3SiC2 composites: a combination of digital image correlation and acoustic emission10.1016/j.jeurceramsoc.2024.116998 ↗
23. Damage behavior and toughening mechanism of SiCf/SiC-Ti3SiC2 composites: a combination of digital image correlation and acoustic emission10.1016/j.jeurceramsoc.2024.116998 ↗
24. Influence of the thickness of pyrolytic carbon interphase on the mechanical behavior of SiC/(BN/PyC)/SiC composites10.1016/j.ceramint.2024.03.322 ↗
25. Effect of a BN interphase that debonds between the interphase and the matrix in SiC/SiC composites10.1111/j.1551-2916.2004.00104.x ↗
26. Flexural fatigue behavior and residual strength evolution of SiCnws-C/C composites10.1016/j.ceramint.2018.09.004 ↗
27. Effects of thermal shock on the microstructure, mechanical and thermophysical properties of ZrC-C composites10.1016/j.compositesa.2021.106642 ↗
28. Effect of heat treatment on the mechanical properties of SiCf/BN/SiC fabricated by CVI10.1016/j.ceramint.2015.11.030 ↗
29. Damage identification and fracture behavior of 2.5D SiCf/SiC composites under coupled stress states10.1016/j.matdes.2024.112964 ↗
30. Proportional limit stress and residual thermal stress of 3D SiC/SiC composite10.1016/j.jmst.2014.08.004 ↗
31. Relationships between hysteresis measurements and the constituent properties of ceramic matrix composites: II, experimental studies on unidirectional materials10.1111/j.1151-2916.1995.tb08047.x ↗
32. Heat treatment effects on microstructure and mechanical properties of CVI SiCf/PyC/SiC composites with Cansas-Ⅲ SiC fibers10.1016/j.jeurceramsoc.2023.06.034 ↗
33. Mandal A. Standard test method for apparent porosity, water absorption, apparent specific gravity and bulk density of burned refractory brick and shapes by boiling water, ASTM C 20–92. 2010;Vol. 15.01.
34. Comparison of the mechanical hysteresis of carbon/ceramic-matrix composites with different fiber preforms10.1016/j.carbon.2008.12.025 ↗
35. Residual stresses in fiber‐reinforced ceramics due to thermal expansion mismatch10.1111/j.1151-2916.1993.tb03988.x ↗
36. On the interfacial behaviour of a glass/epoxy composite during a micro-indentation test: assessment of interfacial shear strength using reduced indentation curves10.1016/S1359-835X(96)00092-9 ↗
37. Cox HL. The elasticity and strength of paper and other fibrous materials. Br J Appl Phys 1952;3(3):72. https://iopscience.iop.org/article/10.1088/0508-3443/3/3/302.10.1088/0508-3443/3/3/302 ↗
38. Davidge RW. Chapter 13 - The mechanical properties and fracture behaviour of ceramic-matrix composites (CMC) reinforced with continuous fibres. Compos Mater Ser 1989;6 547-569. Doi: 10.1016/B978-0-444-87286-9.50017-6.10.1016/B978-0-444-87286-9.50017-6 ↗
39. Standard B. Standard guide for determining the reproducibility of acoustic emission sensor response, ASTM E976-15 (2021).202.11.12.
40. Analysis of residual stress in 6H-SiC particles within Al2O3/SiC composites through Raman spectroscopy10.1111/j.1151-2916.1992.tb07207.x ↗
41. Effects of wet oxidation on residual stress variation of SiCf/SiC composites10.1016/j.ceramint.2022.01.028 ↗
42. Life assessment of thermomechanical fatigue in a woven SiC/SiC ceramic matrix composite with an environmental barrier coating at elevated temperature10.1016/j.ijfatigue.2023.107584 ↗
43. Further understanding of the improved mechanical properties for SiCf/BN/SiC composites prepared by CVI+PIP hybrid technique: Application of micro-mechanical methods10.1016/j.compositesb.2024.111633 ↗
44. Tension–tension fatigue behavior and residual strength evolution of SiC/(PyC/SiC)2/SiC minicomposites prepared by CVI+MI and CVI+PIP processes10.1016/j.ceramint.2021.06.209 ↗
45. FEM analysis of the stress response and failure mechanism of SiC-coated Cf/SiC composites during thermal shock10.1016/j.ceramint.2021.04.218 ↗
46. Effect of Co on thermal and mechanical properties of Si3N4 based ceramic tool material10.1016/j.ceramint.2019.06.198 ↗
47. The effect of neutron irradiation on the fiber/matrix interphase of silicon carbide composites10.1016/j.jnucmat.2008.11.015 ↗
48. Theory of mechanical properties of ceramic-matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
49. Mechanical Behavior of SiC(f)/SiC composites and correlation to in situ fiber strength at room and elevated temperatures10.1111/j.1151-2916.1996.tb07915.x ↗
50. Temperature dependence of tensile strength for a woven Boron‐Nitride‐Coated Hi‐Nicalon™ SiC fiber‐reinforced silicon‐carbide‐matrix composite10.1111/j.1151-2916.2001.tb00961.x ↗
51. Borosilicate glass-induced fiber degradation of SiC/BN/SiC composites exposed in combustion environments10.1111/ijac.12499 ↗
52. Degradation of continuous fiber ceramic matrix composites under constant-load conditions
53. Fiber strength measurement for KD-I(f)/SiC composites and correlation to tensile mechanical behavior at room and elevated temperatures10.1016/j.ceramint.2014.08.072 ↗
54. High-temperature tensile behavior of 3D SiC/SiC composites10.1088/1742-6596/1605/1/012126 ↗
55. The Concept of a strong Interface Applied to SiC/SiC Composites with a BN Interphase10.1016/S1359-6454(00)00247-0 ↗
56. Effects of temperature and atmosphere on microstructural evolution and mechanical properties of KD-II SiC fibers10.1016/j.ceramint.2020.06.225 ↗
57. High-temperature oxidation behavior and mechanism of the Si-based thermal protective coating for SiCf/SiC composites under static oxidation and H2O/O2/Na2SO4 corrosion oxidation10.1016/j.compositesb.2022.109906 ↗
58. Internal friction vs. thermal shock in C/C composites10.1016/j.compositesb.2016.06.078 ↗
59. Xue L-z, Luo W-f. Internal friction behavior of unidirectional carbon/carbon composites after different fatigue cycles10.1016/j.msea.2014.02.020 ↗
60. Temperature dependence of internal friction and elastic modulus of SiC/SiC composites10.1016/S0925-8388(03)00252-4 ↗
61. Effect of fiber directionality on the static and dynamic mechanical properties of 3D SiCf/SiC composites10.1016/j.msea.2016.02.006 ↗
62. Analysis of the fracture behavior and mechanism of PIP-C/SiC composites at high temperatures10.1016/j.compstruct.2024.118491 ↗
63. Identifying damage mechanisms of composites by acoustic emission and supervised machine learning10.1016/j.matdes.2023.111745 ↗
64. Muir C, Swaminathan B, Fields K, Almansour AS, Sevener K, Smith C, et al. A machine learning framework for damage mechanism identification from acoustic emissions in unidirectional SiC/SiC composites npj Comput Mater 2021;7(1):146. Doi: 10.1038/s41524-021-00620-7.10.1038/s41524-021-00620-7 ↗
65. Do high frequency acoustic emission events always represent fibre failure in CFRP laminates?10.1016/j.compositesa.2017.10.013 ↗
66. Investigation of the damage mechanisms for mode I delamination growth in foam core sandwich composites using acoustic emission10.1177/1475921714568403 ↗
67. Characterization and modeling damage and fracture of prepreg-MI SiC/SiC composites under tensile loading at room temperature10.1007/s10443-022-10015-6 ↗
68. Acoustic emission characterization of fracture toughness for fiber reinforced ceramic matrix composites10.1016/j.msea.2012.09.081 ↗