Double cantilever beam testing of multidirectional laminates
Source abstract
Abstract
Abstract Several difficulties in the double cantilever beam (DCB) tests of multidirectional laminates often prevent valid measurements of the mode I critical strain energy release rate G Ic . In this paper, several DCB specimens were analysed with 3D finite element models. The results showed that the undesired effects of residual stresses and of mode-mixity can be minimised. An interlaminar stress based fracture criterion predicts that the G Ic of multidirectional specimens is typically 10–40% higher than the G Ic of unidirectional [0°] n laminates. This agrees with the few valid experimental data available.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical Behavior of Composites · Composite Structure Analysis and Optimization · Structural Analysis and Optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Standard test methods for delamination resistance of composite materials: current status10.1023/A:1008869811626 ↗
2. Fibre-reinforced plastic composites—determination of mode I interlaminar fracture toughness, GIc, for unidirectionally reinforced materials. ISO; 2001. p. 15024.
3. Factors affecting the interlaminar fracture energy of graphite/epoxy laminates
4. Determination of GIc in angle ply composites using a cantilever beam test method10.1177/073168448300200101 ↗
5. The characterization of mode I delamination failure in non-woven multidirectional laminates10.1016/0010-4361(84)90708-0 ↗
6. Delamination analysis of composites with distributed damage using a J integral
7. Mode I interlaminar fracture of symmetrical cross-ply laminates10.1016/0266-3538(91)90025-K ↗
8. A modified DCB specimen for mode I testing of multidirectional laminates10.1177/002199839202601101 ↗
9. Delamination fracture of multidirectional carbon-fibre/epoxy composites under mode I, mode II and mixed-mode I/II loading10.1177/002199839903300105 ↗
10. Initiation and bifurcation mechanisms of cracks in multidirectional laminates10.1016/S0266-3538(99)00179-7 ↗
11. Mode I fracture resistance characteristics of graphite/epoxy laminated composites10.1002/pc.10173 ↗
12. Mode I interlaminar fracture of carbon/epoxy cross-ply composites10.1016/S0266-3538(01)00223-8 ↗
13. An analytical investigation of delamination front curvature in double cantilever beam specimens10.1177/002199839002401101 ↗
14. Effect of stacking sequence on energy release rate distributions in multidirectional DCB and ENF specimens10.1016/S0013-7944(96)00037-9 ↗
15. Energy release rate analysis for adhesive and laminate double cantilever beam specimens emphasizing the effect of residual stresses10.1016/S0143-7496(99)00016-0 ↗
16. Kaninnen · 1985
17. Convergence of strain energy release rate components for edge-delaminated composite laminates10.1016/0013-7944(88)90196-8 ↗
18. Calculation of stress intensity factors for interlaminar cracks in composite laminates10.1016/S0266-3538(97)00006-7 ↗
19. Designation of mode mix in orthotropic composite delamination problems10.1023/A:1007466905925 ↗
20. Stress intensity factors as the fracture parameters for delamination crack growth in composite laminates10.1016/S1359-8368(96)00056-X ↗
21. Finite element modelling of delamination growth in the DCB and edge delaminated DCB specimens10.1016/0263-8223(95)00047-X ↗