Abstract The fracture surface morphology of short fiber reinforced thermoplastics (SFRTs) has often been used to assess qualitatively the degree of fiber–matrix interfacial adhesion. Mechanical properties such as tensile strength, fracture toughness and failure strain, etc. are then correlated with the morphology. Fracture surfaces showing fibers surrounded by a large amount of matrix material is commonly regarded as indication of strong fiber–matrix interfacial adhesion while smooth fibers are characteristic of weak interfacial adhesion. Many experimental results of SFRTs have been so interpreted. However, it is shown in this paper that strictly speaking, such interpretations are generally incorrect. Moreover, the amount of matrix material does not provide a quantitative measure of the adhesion. Correct implication of the morphology of fracture surfaces is clarified. Short glass fiber reinforced polyamide 6,6/polypropylene (PA 6,6/PP) blends toughened by rubber are employed as examples for SFRTs since the PA 6,6/PP blend system by changing PA 6,6 concentration in the matrix blend represents a wide range of matrix materials. It is demonstrated that the fracture surface morphology of such composites is dependent on both fiber–matrix interfacial adhesion strength and matrix shear yield strength. Consequently, tensile failure strain is well correlated with the post-mortem fracture surface morphology of these SFRTs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical Behavior of Composites · Fiber-reinforced polymer composites · Composite Material Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Tensile and impact strengths of unidirectional, short fiber-reinforced thermoplastics10.1016/0010-4361(79)90012-0 ↗
2. Fracture resistance of unfilled and calcite-filled ABS composites reinforced by short glass fibers (SGF) under impact load10.1016/S1359-835X(97)00111-5 ↗
3. Characterization of tensile behavior of hybrid short glass fibre/calcite particle/ABS composites10.1016/S1359-835X(97)00117-6 ↗
4. Tensile properties of short-glass-fiber- and short-carbon-fiber-reinforced polypropylene composites10.1016/S1359-835X(00)00068-3 ↗
5. Microstructural efficiency and fracture toughness of short fiber/thermoplastic matrix composites10.1016/0266-3538(85)90090-9 ↗
6. Yielding and impact behavior of pp/sgf/epr ternary composites with controlled morphology10.1007/BF00352659 ↗
7. Alsewailem FD. Rubber toughening of glass-fiber-reinforced nylon 66. PhD thesis, Western Virginia University; 2002. p. 117–30.
8. Fracture resistance of polyblends and polyblend matrix composites. Part III. Role of rubber type and location in nylon 6,6/SAN composites10.1023/A:1013266204096 ↗
9. Mechanical properties of glass fiber/talc/polybutylene–terephthalate composites as processed by the radlite technique10.1016/0266-3538(93)90157-C ↗
10. Mechanical properties and morphology of polypropylene composites. III. Short glass fiber reinforced elastomer modified polypropylene
11. Glass fiber-reinforced polyamide composites toughened with ABS and EPR-g-MA10.1002/1097-4628(20010418)80:3<484::AID-APP1122>3.0.CO;2-5 ↗
12. Effect of rubber functionality on microstructures and fracture toughness of impact-modified nylon 6,6/polypropylene blends. Part I. Structure–property relationships10.1016/S0032-3861(98)00363-2 ↗
13. Effect of rubber functionality on microstructures and fracture toughness of impact-modified nylon 6,6/polypropylene blends. Part II—toughening mechanisms10.1016/S0032-3861(99)00750-8 ↗
14. Effects of fiber length and orientation distributions on the mechanical properties of short-fiber-reinforced polymers—a review
15. Effects of fiber length and fiber orientation distributions on the tensile strength of the tensile strength of short-fiber-reinforced polymers10.1016/S0266-3538(96)00072-3 ↗
16. Strength predictions of injection molding compounds10.1177/073168449000900301 ↗
17. The fiber pull-out energy of misaligned short fiber composites10.1023/A:1018593931951 ↗
18. The influence of fibre length and concentration on the properties of glass fibre reinforced polypropylene: 5. Injection moulded long and short fibre PP10.1016/S1359-835X(02)00179-3 ↗
19. Some further considerations of the theory of fibre debonding and pull-out from an elastic matrix, I. Constant interfacial frictional shear stress10.1016/0010-4361(93)90258-A ↗
20. Analyses of the micromechanics of the stress transfer in single- and multi-fiber pull-out tests10.1016/S0266-3538(99)00157-8 ↗