journal article·2023-12

Formability, densification behavior and hierarchical grain structure of laser-directed energy deposition of TiB reinforced titanium matrix composites

Huaqiang Liu, Junzhu Han, Yuanfei Han, Minhan Fang, Xiaoyan Wang, Guangfa Huang, Weijie Lu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Sandwich structures with repairable cores based on truncated cube cells10.1016/j.compositesb.2022.110124 ↗
2. Additive manufacturing of fine-grained high-strength titanium alloy via multi-eutectoid elements alloying10.1016/j.compositesb.2022.110399 ↗
3. Machine learning–aided real-time detection of keyhole pore generation in laser powder bed fusion10.1126/science.add4667 ↗
4. In situ reactions during direct laser deposition of Ti-B4C composites10.1016/j.scriptamat.2020.03.021 ↗
5. In situ alloying based laser powder bed fusion processing of β Ti–Mo alloy to fabricate functionally graded composites10.1016/j.compositesb.2021.109059 ↗
6. Strategic dual laser 3D printing of structural metal-plastic hybrid materials10.1016/j.compositesb.2023.110794 ↗
7. Heat treatment effects on the hydrogen embrittlement of Ti6Al4V fabricated by laser beam powder bed fusion
8. Experimental realisation of build orientation effects on the mechanical properties of truly as-built Ti-6Al-4V SLM parts10.1016/j.jmapro.2021.01.027 ↗
9. Continuous and pulsed selective laser melting of Ti6Al4V lattice structures: effect of post-processing on microstructural anisotropy and fatigue behavior
10. TiB reinforced Ti-6Al-4V matrix composites with improved short-term creep performance fabricated by laser powder bed fusion10.1016/j.jmapro.2021.08.063 ↗
11. Microstructure and tensile properties of TiCp/Ti6Al4V titanium matrix composites manufactured by laser melting deposition10.1016/j.jmatprotec.2017.10.005 ↗
12. Microstructure evolution mechanisms and strength improvement of (6.5 vol% TiC+3.3vol%Ti5Si3)/Ti6Al4V composites via heat treatments10.1016/j.msea.2020.140581 ↗
13. A TiB whisker-reinforced titanium matrix composite with controllable orientation: a novel method and superior strengthening effect10.1016/j.msea.2021.142309 ↗
14. TiB whisker induced variant selection in titanium matrix composites10.1016/j.scriptamat.2022.114772 ↗
15. High-temperature deformation behavior and microstructure evolution of TiBw/Ti6Al4V composites during hot shear-compression deformation10.1016/j.jmrt.2021.08.089 ↗
16. Nano-TiB whiskers reinforced Ti–6Al–4V matrix composite fabricated by direct laser deposition: microstructure and mechanical properties
17. In situ reactions during direct laser deposition of Ti-B4C composites10.1016/j.scriptamat.2020.03.021 ↗
18. Columnar to equiaxed grain transition of laser deposited Ti6Al4V using nano-sized B4C particles10.1016/j.compositesb.2021.108667 ↗
19. Refined microstructure and ultrahigh mechanical strength of (TiN+TiB)/Ti composites in situ synthesized via laser powder bed fusion
20. Microstructural characterization and mechanical properties of nano-scale/sub-micron TiB-reinforced titanium matrix composites fabricated by laser powder bed fusion10.1016/j.jallcom.2021.163054 ↗
21. In-situ grain structure control in directed energy deposition of Ti6Al4V
22. Process induced multi-layered titanium-boron carbide composites via additive manufacturing
23. Nanocrystalline TiC reinforced Ti matrix bulk-form nanocomposites by Selective Laser Melting (SLM): densification, growth mechanism and wear behavior10.1016/j.compscitech.2011.07.010 ↗
24. Laser metal deposition of functionally graded Ti6Al4V/TiC10.1016/j.matdes.2015.06.135 ↗
25. Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite10.1016/j.matdes.2013.03.049 ↗
26. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
27. Microstructural evolution, mechanical and tribological properties of TiC/Ti6Al4V composites with unique microstructure prepared by SLM10.1016/j.msea.2021.141187 ↗
28. Selective laser melting of TiC reinforced 316L stainless steel matrix nanocomposites: influence of starting TiC particle size and volume content10.1016/j.matdes.2016.05.018 ↗
29. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
30. Effects of process parameters on the microstructure and mechanical properties of a laser micro-alloying TiB/Ti–6Al–4V titanium matrix composite10.1016/j.msea.2023.144988 ↗
31. New insights into the evolution of TiB whisker and TiC particle during selective laser melting of titanium matrix composites10.1016/j.msea.2023.145200 ↗
32. Effect of self-accommodation on α/α boundary populations in pure titanium10.1016/S1359-6454(03)00035-1 ↗
33. Phase transformation pathways in Ti-6Al-4V manufactured via electron beam powder bed fusion10.1016/j.actamat.2021.117131 ↗
34. High-mass-proportion TiCp/Ti6Al4V titanium matrix composites prepared by directed energy deposition
35. Influence of trace boron addition on microstructure, tensile properties and their anisotropy of Ti6Al4V fabricated by laser directed energy deposition10.1016/j.matdes.2019.107943 ↗
36. Effects of boron addition on microstructures and mechanical properties of Ti-6Al-4V manufactured by direct laser deposition10.1016/j.matdes.2019.108191 ↗
37. Selective laser melting of nanocomposite Ti-6Al-4V and TiC powder10.4028/www.scientific.net/KEM.822.575 ↗
38. Manufacturing of a nanosized TiB strengthened Ti-based alloy via electron beam powder bed fusion
39. In situ (TiBw+TiCp)/Ti6Al4V composites with a network reinforcement distribution10.1016/j.msea.2010.07.025 ↗
40. Reprint: boron modified titanium alloys10.1016/j.pmatsci.2021.100815 ↗
41. Microstructural effects on the mechanical behavior of B-modified Ti–6Al–4V alloys10.1016/j.actamat.2007.05.009 ↗
42. Microstructure and mechanical properties of investment casted titanium matrix composites with B4C additions10.1016/j.msea.2015.01.067 ↗
43. Reinforcements stimulated dynamic recrystallization behavior and tensile properties of extruded (TiB + TiC + La2O3)/Ti6Al4V composites10.1016/j.jallcom.2016.12.418 ↗
44. Effect of extrusion dies angle on the microstructure and properties of (TiB + TiC)/Ti6Al4V in situ titanium matrix composite10.1016/j.msea.2016.05.021 ↗
45. Microstructure characteristics and enhanced properties of network-structured TiB/(TA15-Si) composites via rolling deformation at different temperatures
46. Laser additive manufacturing of carbon nanotubes (CNTs) reinforced aluminum matrix nanocomposites: processing optimization, microstructure evolution and mechanical properties
47. Microstructure evolution and mechanical properties of in-situ Ti6Al4V–TiB composites manufactured by selective laser melting10.1016/j.compositesb.2020.108567 ↗
48. Pore formation model for direct laser deposition of Al2O3–ZrO2 ceramic10.1016/j.jeurceramsoc.2021.09.042 ↗
49. Laser additive manufacturing of nano-TiC reinforced Ni-based nanocomposites with tailored microstructure and performance10.1016/j.compositesb.2018.12.146 ↗
50. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB + TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
51. Growth mechanism of the tubular TiB crystals in situ formed in the coatings laser-borided on Ti–6Al–4V alloy10.1016/j.matlet.2010.08.014 ↗
52. Ye · 2002
53. Microstructural evolution and characteristics of bonding zone in multilayer laser cladding of Fe-based coating10.1016/j.jmatprotec.2018.08.005 ↗
54. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
55. Quantitative measurement of displacement and strain fields from HREM micrographs10.1016/S0304-3991(98)00035-7 ↗
56. Selective laser melted high Ni content TiNi alloy with superior superelasticity and hardwearing10.1016/j.jmst.2021.09.067 ↗
57. Microstructural effects on the mechanical behavior of B-modified Ti–6Al–4V alloys10.1016/j.actamat.2007.05.009 ↗
58. An innovative TiB whisker architecture of titanium matrix composite devised by scanning electron beam remodeling
59. The Interdependence Theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
60. Achieving strength-ductility combination and anisotropy elimination in additively manufactured TiB/Ti6Al4V by in-situ synthesized network architecture with fine grains10.1016/j.compositesb.2023.110822 ↗
61. Simultaneously improved strength and ductility in aluminum matrix composite with heterogeneous structures under impact loadings10.1016/j.jmrt.2022.12.187 ↗