Fatigue behavior of filament wound E-glass/epoxy composite tubes damaged by low velocity impact
Source abstract
Abstract
Abstract In this paper, filament wound glass fiber reinforced plastic (GRP) tubes were studied. Impact tests were realized at 5 J and 10 J energy levels. Force–time and force–displacement curves were obtained and damage zones were also examined. The burst strengths of tubes were found in accordance with ASTM-D 1599 before and after impact. For fatigue tests, PLC controlled hydraulic inner-pressure fatigue test rig was set up. Damaged and non-damaged tubes were subjected to the fatigue test in accordance with ASTM-D 2992. The samples were exposed to five different stress levels; 30%, 35%, 40%, 50%, 60% of the burst strength. Number of cycles occurred up to the final failure was recorded and S – N diagrams were plotted. The burst strength and the fatigue life of the damaged GRP pipes were decreased as the impact energy increased. Also the decrease in the fatigue life was greater than that of the burst strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical Behavior of Composites · Structural Response to Dynamic Loads · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Biaxial fatigue behaviour of multidirectional filament wound glass-fiber epoxy pipe10.1016/S0266-3538(00)00215-3 ↗
2. Strength of filament wound GRP pipes with surface crack10.1016/S1359-8368(00)00037-8 ↗
3. Initiation and growth of transverse and longitudinal cracks in composite cross ply laminates10.1016/S0263-8223(01)00002-2 ↗
4. Application of the Paris equation to the fatigue growth of transverse ply cracks10.1177/002199838902300706 ↗
5. Henaff- Garden · 1990
6. Impact and fatigue behaviour of hemp fiber composites10.1016/j.compscitech.2007.03.039 ↗
7. Uniaxial fatigue behaviour of filament wound glass-fiber epoxy composite tubes10.1016/S0266-3538(01)00084-7 ↗
8. Bredemo R. Damage development during uniaxial fatigue of filament wound tubes. SICOMP report 92-001. Pitea (Sweden), Swedish Institute of Composites; 1992.
9. Interaction between plasticity and damage in the behaviour of fiber reinforced composite pipes in biaxial loading (internal pressure and tension)10.1016/S1359-8368(98)00030-4 ↗
10. Fatigue damage evaluation through stiffness measurement in boron/epoxy laminates10.1177/002199838101500105 ↗
11. Fatigue of composites–fatigue modulus concept and life prediction10.1177/002199838602000203 ↗
12. Long term fatigue behaviour of composite materials
13. A reliability method for optimization of [+, −]n fiber reinforced composite pipes10.1016/S0951-8320(00)00002-8 ↗
14. Wang SS, Srinivasan S, Cole B. Long term leakage failure and life prediction fiber composite laminate tubing under combined internal pressure and axial loading. Theory and experiments 2nd International conference on composite materials for offshore operations. CMOO-2 University of Houston, Houston TX; 1997.
15. Fatigue behavior of surface-notched composite pipes repaired by composite patches
16. Residual failure pressures and fatigue life of filament-wound composite pipes subjected to lateral impact10.1177/0021998311425717 ↗
17. ASTM Standard D1599, 1999 (2001). Standard test method for resistance to short-time hydraulic pressure of plastic pipe, tubing, and fittings. ASTM International, West Conshohocken, PA, 2006 http://dx.doi.org/10.1520/D1599-99R11, .10.1520/D1599-99R11 ↗
18. ASTM Standard D2992 (2012). Standard practice for obtaining hydrostatic or pressure design basis for fiberglass (glass-fiber-reinforced thermosetting-resin) pipe and fittings. ASTM International, West Conshohocken, PA, 2012. http://dx.doi.org/10.1520/D2992-12, www.astm.org.10.1520/D2992-12 ↗
19. Dynamic response of laminated composites subjected to low-velocity impact10.1177/0021998307079971 ↗
20. ASTM Standard D2584 (2011). Standard Test Method for Ignition Loss of Cured Reinforced Resins. ASTM International, West Conshohocken, PA, 2011. http://dx.doi.org/10.1520/D2584-11, .10.1520/D2584-11 ↗
21. Abrate · 1998 · 135