A new approach for fabrication of titanium-titanium boride periodic composite via additive manufacturing and pressure-less sintering

Esmat Sheydaeian, Ehsan Toyserkani

Publisher page

Abstract

Abstract This study proposes a new additive manufacturing (AM) based methodology to fabricate periodic metal matrix composite architectures, with a focus on titanium (Ti)-titanium boride whisker (TiBw) composites. The manufacturing method includes binder jetting AM of the titanium matrix reinforced periodically by the extrusion of a custom-developed highly loaded resin, containing titanium di-boride (TiB2) particles. A low-temperature pressure-less sintering method was then applied to increase the mechanical strength of green samples produced from the additive manufacturing step. The sintering process also fosters the chemical reaction between the matrix and ceramic, resulting in the growth of titanium boride whisker (TiBw). The ceramic volume fraction and sintering protocol were studied as two main input variables in the design and fabrication steps. Investigating the influence of input parameters on the volume fraction and morphology (whisker formation) of TiB determined that the physical properties of the specimens, such as stiffness, were affected. The data analysis suggested a higher possibility for the formation and growth of TiBw as the temperature elevated in the sintering step (1400 °C). The ranges of 1.6 ± 0.2 GPa–3.7 ± 0.4 GPa and 83.9 ± 18.7 MPa–165 ± 13.2 MPa for the Young's modulus and Yield stress of the specimens were obtained, respectively. The stiffness of the samples was enhanced significantly by increasing the temperature and volume fraction. In particular, those samples sintered up to 1400 °C displayed 6.4%–15.2% improvement in the stiffness, although only a small fraction of the ceramic material was incorporated into the design: 2% and 4%, respectively. The similar trend of the improvement in density of the porous matrix was observed (i.e., 4.5%–19%). The range of mechanical and structural properties of the periodic composite developed in this study demonstrated the relevance of applying this method to the fabrication of biomedical and other lightweight titanium composite structures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
2. The production and application of metal matrix composite materials10.1016/S0924-0136(00)00639-7 ↗
3. Processing and properties of titanium-titanium boride (TiBw) matrix composites - a review10.1007/s10853-006-0776-2 ↗
4. Titanium particulate metal matrix composites reinforcement, production methods, and mechanical properties **10.1002/(SICI)1527-2648(200003)2:3<85::AID-ADEM85>3.0.CO;2-U ↗
5. Material properties of titanium diboride10.6028/jres.105.057 ↗
6. Titanium-titanium boride ( Ti-TiB ) functionally graded materials through reaction Sintering: synthesis, microstructure, and properties10.1007/s11661-003-0164-3 ↗
7. Pressure-less and current-activated pressure-assisted sintering of titanium dual matrix composites: effect of reinforcement particle size10.1016/j.msea.2008.11.046 ↗
8. TiB w -reinforced Ti Composites: processing, properties, application prospects, and Research needs10.1007/s11837-004-0127-1 ↗
9. Viability of titanium-titanium boride composite as a biomaterial10.5402/2013/970535 ↗
10. Surface & Coatings Technology In-situ formation of laser Ti6Al4V – TiB composite coatings on Ti6Al4V alloy for biomedical application10.1016/j.surfcoat.2015.10.079 ↗
11. Corrosion behavior of titanium boride composite coating fabricated on commercially pure titanium in Ringer ’ s solution for bioimplant applications10.1016/j.msec.2014.12.002 ↗
12. Additive manufacturing of carbon fiber reinforced thermoplastic composites using fused deposition modeling10.1016/j.compositesb.2015.06.013 ↗
13. Laser deposition-additive manufacturing of TiB-Ti composites with novel three-dimensional quasi-continuous network microstructure: effects on strengthening and toughening10.1016/j.compositesb.2017.09.019 ↗
14. Composites: Part B NiTi – Al interface strength in ultrasonic additive manufacturing composites10.1016/j.compositesb.2013.10.024 ↗
15. A progressive intraply material deterioration and delamination based failure model for the crashworthiness of fabric composite corrugated beam: parameter sensitivity analysis10.1016/j.compositesb.2017.09.072 ↗
16. Design methodology for porous composites with tunable thermal expansion produced by multi-material topology optimization and additive manufacturing10.1016/j.compositesb.2017.07.054 ↗
17. Sustainable composite fused deposition modelling fi lament using recycled pre-consumer polypropylene10.1016/j.compositesb.2017.10.005 ↗
18. CIRP annals - manufacturing technology materials for additive manufacturing
19. Optics & Laser Technology Microhardness and microstructure evolution of TiB 2 reinforced Inconel 625/TiB 2 composite produced by selective laser melting10.1016/j.optlastec.2016.01.010 ↗
20. Rapid fabrication of bulk-form TiB 2/316L stainless steel nanocomposites with novel reinforcement architecture and improved performance by selective laser melting10.1016/j.jallcom.2016.04.156 ↗
21. In-situ TiB/near α Ti matrix composites manufactured by selective laser melting10.1016/j.addma.2016.04.001 ↗
22. Li · 2017 · vol. 113 · 342
23. Effect of glycerol concentrations on the mechanical properties of additive manufactured porous calcium polyphosphate structures for bone substitute applications
24. Multiple material additive manufacturing – Part 1: a review10.1080/17452759.2013.778175 ↗
25. A system for selectively encapsulating porogens inside the layers during additive manufacturing: from conceptual design to the first prototype10.1016/j.jmapro.2017.03.001 ↗
26. Toyserkani · 2014
27. Mohan · 2017 · vol. 2759
28. Additive manufacturing in unmanned aerial vehicles ( UAVs ): challenges and potential10.1016/j.ast.2016.12.019 ↗
29. Characterization of mechanical properties and fracture mode of additively manufactured carbon fi ber and glass fi ber reinforced thermoplastics10.1016/j.matdes.2017.10.021 ↗
30. Ultraviolet curing of highly loaded ceramic suspensions for stereolithography of ceramics
31. Material process development for the fabrication of heterogeneous titanium structures with selective pore morphology by a hybrid additive manufacturing process10.1016/j.matdes.2017.09.025 ↗
32. Characterizations of additive manufactured porous titanium implants10.1002/jbm.b.32764 ↗
33. Influence of shear thinning and material flow on robotic dispensing of poly(ethylene glycol) diacrylate/poloxamer 407 hydrogels10.1002/app.45083 ↗
34. Standard test methods of compression testing of metallic materials at room temperature
35. On the effect of throughout layer thickness variation on properties of additively manufactured cellular titanium structures10.1016/j.addma.2017.08.017 ↗
36. 2017 · 1
37. Application of the rule of mixtures and halpin-tsai equations to woven fabric reinforced epoxy composites
38. The kinetics and mechanism of interfacial reaction in sigma fibre-reinforced Ti MMCs10.1016/S1359-835X(96)00105-4 ↗
39. Evolution of microstructure and phases in in situ processed Ti-TiB composites containing high volume fractions of TiB whiskers10.1557/JMR.1999.0571 ↗
40. On the influence of sintering protocols and layer thickness on the physical and mechanical properties of additive manufactured titanium porous bio-structures10.1016/j.jmatprotec.2016.07.037 ↗
41. Biomaterials Topological design and additive manufacturing of porous metals for bone scaffolds and orthopaedic implants: a review10.1016/j.biomaterials.2016.01.012 ↗
42. Highly porous titanium scaffolds for orthopaedic applications10.1002/jbm.b.31682 ↗
43. Mechanical properties and osteoconductivity of porous bioactive titanium10.1016/j.biomaterials.2005.03.019 ↗