journal article·2018-11Open access

Impact of fillers (short glass fibers and rubber) on the hydrolysis-induced embrittlement of polyamide 6.6

Pierre-Yves Le Gac, Bruno Fayolle

Abstract

Abstract This study deals with the durability of composites based on polyamide 6.6 (PA6.6) in a humid environment, and more especially, with the loss of fracture properties. It is known that PA6.6 undergoes plasticization in the presence of water, but hydrolysis also occurs. This hydrolysis leads to a sharp decline in fracture properties in resin. The aim of this study is thus to understand the behavior of two PA6.6-based composites, one containing short glass fibers and the other both glass fibers and a rubber. The results showed the transition from ductile to brittle behavior as a function of hydrolysis time in resin. For composites, the drop in elongation breaking with the macromolecular chain length was linear for all ageing conditions considered here without marked transition. The results presented here can be used for lifetime prediction of PA6.6-based composites in a humid environment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · Polymer crystallization and properties · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Autoxidation of N-alkyl amides. Part III. Mechanism of thermal oxidation10.1039/j29670001047 ↗
2. Auto-oxidation of aliphatic polyamides10.1016/j.polymdegradstab.2013.04.012 ↗
3. Influence of temperature and stabilization on oxygen diffusion limited oxidation profiles of polyamide 610.1016/j.polymdegradstab.2016.05.024 ↗
4. Kinetics of the acid hydrolysis of cyclic oligomers from nylon 6 and nylon 6.610.1002/macp.1959.020300110 ↗
5. Modelling the non Fickian water absorption in polyamide 610.1016/j.polymdegradstab.2016.09.001 ↗
6. Yield stress changes induced by water in polyamide 6: characterization and modeling10.1016/j.polymdegradstab.2017.02.003 ↗
7. Study of the water absorption and its influence on the Young's modulus in a commercial polyamide10.1016/j.polymertesting.2012.10.003 ↗
8. Molecular weight distribution and mass changes during polyamide hydrolysis10.1016/S0032-3861(97)00414-X ↗
9. Degradation-induced embrittlement in semi-crystalline polymers having their amorphous phase in rubbery state10.1007/s10853-008-3005-3 ↗
10. The stiffness and strength of a polyamide thermoplastic reinforced with glass and carbon fibres10.1007/BF00647783 ↗
11. Failure and fracture of short glass fibre-reinforced nylon composites10.1016/0010-4361(85)90617-2 ↗
12. Multiaxial fatigue models for short glass fiber reinforced polyamide–Part I: nonlinear anisotropic constitutive behavior for cyclic response10.1016/j.ijfatigue.2012.03.012 ↗
13. Effect of glass fiber and maleated ethylene–propylene rubber content on the impact fracture parameters of nylon 610.1016/S0032-3861(01)00068-4 ↗
14. Moisture sorption in polyamide 6.6: experimental investigation and comparison to four physical-based models10.1016/j.polymertesting.2015.02.004 ↗
15. Nylon 6.6 accelerating aging studies: II. Long-term thermal-oxidative and hydrolysis results10.1016/j.polymdegradstab.2010.06.018 ↗
16. Molar mass analysis of polyamides-11 and-12 by size exclusion chromatography in HFiP10.1016/j.polymer.2008.08.017 ↗
17. Molecular and macromolecular structure changes in polyamide 11 during thermal oxidation–Kinetic modeling10.1016/j.polymdegradstab.2015.06.005 ↗
18. Water absorption and leaching effects in cellulose diacetate10.1016/S0032-3861(97)00277-2 ↗
19. A new kinetic model for predicting polyamide 6-6 hydrolysis and its mechanical embrittlement10.1016/j.polymdegradstab.2012.03.003 ↗
20. Characterizing and modeling the hydrolysis of polyamide-11 in a pH 7 water environment10.1021/ma010541o ↗
21. Hydrolytic ageing of polyamide 11. 1. Hydrolysis kinetics in water10.1016/S0032-3861(02)00583-9 ↗
22. The hygrothermal behaviour of glass fibre reinforced PA66 composites: a study of the effect of water absorption on their mechanical properties10.1007/BF01160550 ↗
23. Review of polymer oxidation and its relationship with materials performance and lifetime prediction10.1016/j.polymdegradstab.2013.06.024 ↗
24. Influence of temperature on the thermo-oxidative degradation of polyamide 6 films10.1016/j.polymdegradstab.2010.02.030 ↗
25. Thermo oxidative stability of polyamide 6 films I. Mechanical and chemical characterisation10.1016/S0141-3910(99)00122-6 ↗
26. Adhesion and fracture of interfaces between immiscible polymers: from the molecular to the continuum scal
27. Investigation of polyamide 11 embrittlement during oxidative degradation10.1016/j.polymer.2015.11.025 ↗
28. Fracture behavior of injection-molded short and long glass fiber—polyamide 6.6 composites10.1016/0266-3538(88)90067-X ↗
29. Microfailure behaviour of randomly dispersed short fibre reinforced thermoplastic composites obtained by direct SEM observation10.1007/BF01184987 ↗
30. In situ X-ray tomography investigation on damage mechanisms in short glass fibre reinforced thermoplastics: effects of fibre orientation and relative humidity10.1016/j.compositesb.2016.10.043 ↗
31. Influence of the fibre/matrix interface on ageing mechanisms of glass fibre reinforced thermoplastic composites (PA-6, 6, PET, PBT) in a hygrothermal environment10.1016/j.polymdegradstab.2009.04.009 ↗
32. In situ damage mechanisms investigation of PA66/GF30 composite: effect of relative humidity10.1016/j.compositesb.2013.11.001 ↗
33. Fracture toughness of polymer interface reinforced with diblock copolymer: effect of homopolymer molecular weight10.1021/ma960533l ↗