journal article·1999-05

Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites

F Lamouroux, S Bertrand, R Pailler, R Naslain, M Cataldi

Composites Science and Technology· Volume 59· Issue 7
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. The concept of layered interphases in SiC/SiC
2. Chollon G. Fibres ceramiques à base de carbure de silicium et à faible taux d’oxygène. Ph.D. thesis no. 1280, University of Bordeaux I, France, 1995.
3. Creep behaviour and structural characterization at high temperaturesof Nicalon SiC fibers10.1007/BF02396938 ↗
4. Bodet R. Comportement à la rupture à chaud et en fluage, évolution microstructurale defibres issues de précurseurs organosiliciés. Ph.D. thesis no. 986, University of Bordeaux I, 1993.
5. Property-structure characterization of continuousfine alumina-silica fibre10.1016/0266-3538(90)90093-K ↗
6. Tressler R, DiCarlo J. High temperature mechanical properties of advanced ceramic fibers. In: Naslain R, Lamon J, Doumeingts J, editors. Proc of HT CMC1. Abington Cambridge: Woodhead, 1993. p 33–49.
7. DiCarlo J, Yun H. Creep and rupture behavior of advanced fibers. Proc of ICCM-10. Vancouver, British Columbia, 1995. p. 315–22.
8. Abbé F. Fluage en flexion d’un composite 2D SiC–SiC. Ph.D. thesis, University of Caen, France, 1990.
9. Holmes J, Chermant JL. Creep behaviour of fiber-reinforced ceramic matrix composites. In: Naslain R, Lamon J, Doumeingts J, editors. Proc of HT-CMC1. Abington Cambridge: Woodhead, 1993. p. 633–47.
10. Kervadec D. Comportement en fluage sous flexion et microstructure d’un SiC-MLAS 1D. PhD thesis, University of Caen, France, 1992.
11. Uniaxial tensile creep behaviour of an alumina fiber-reinforced ceramic matrix composite: I. experimental study10.1016/0955-2219(94)90124-4 ↗
12. Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D Nicalon/C/SiC composites. Part 110.1016/S0955-2219(96)00067-2 ↗
13. Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D Nicalon/C/SiC composites. Part 210.1016/S0955-2219(96)00204-X ↗
14. Carrere P. Comportement thermomécanique d’un composite de type SiC/SiC. Ph.D. thesis no. 1592, University of Bordeaux I, France, 1996.
15. Filipuzzi L. Oxydation des composites SiC/SiC et de leurs constituants: approcheexpérimentale, modélisation et influence sur le comportement mécanique. Ph.D. thesis no. 593, University of Bordeaux I, France, 1991.
16. Oxidizing ageing effects on SiC-SiC composites10.1007/BF01105277 ↗
17. Cutard T, Huger M, Fargeot D, Gault C. Ultrasonic characterization at high temperature of damage in ceramic composites subjected to tensile stresses. In: Naslain R, Lamon J, Doumeingts J, editors. Proc of HT-CMC1. Abington Cambridge: Woodhead, 1993. p. 33–49.
18. Oxidation effects on the mechanical properties of 2D woven silicon carbide composites10.1016/0955-2219(94)90105-8 ↗
19. Unexpected behaviour of interfacial carbon in SiC/SiC composites during oxidation
20. Ceramics coating for carbon-carbon composites
21. Carbon-carbon composites: oxidation behaviour and coating protection
22. Critical review on oxidation protection for carbon-based composites
23. Courtright EL. A review of fundamental coating issues for high temperature composites. Surface and Coatings Technology 1994;68–69:116–25.10.1016/0257-8972(94)90148-1 ↗
24. Oxidation behavior and protection of carbon/carbon composites10.1016/0008-6223(87)90197-7 ↗
25. Oxidation tests of carbonaceous composites protected by Si–B–C coatings10.1016/0040-6090(94)90882-6 ↗
26. Oxidation protection for 3D carbon/carbon composites10.1016/0094-5765(94)00085-Z ↗
27. Particulate-containing glass sealants for carbon/carbon composites10.1016/0008-6223(94)00174-X ↗
28. Antioxidation of carbon-carbon composites by SiC concentration gradient and zircon overcoating10.1016/0008-6223(94)00159-W ↗
29. The oxidation behaviour of two- and three-dimensional C/SiC thermostructural materials protected by chemical-vapour-deposition polylayers coatings10.1007/BF00354562 ↗
30. Multilayer coating for carbon-carbon composites10.1016/0008-6223(94)00158-V ↗
31. Multilayered coatings for protecting carbon–carbon composites from oxidation10.1016/0008-6223(94)00157-U ↗
32. Silicon-carbide/boron-containing coatings for the oxidation protection of graphite10.1016/0008-6223(94)00178-3 ↗
33. Lamouroux F, Heurtevent F, Pailler R, Naslain R, Cataldi M. Oxidation protection of carbon fiber reinforced cmc: I—Concept of a functional matrix. J Europ Ceram Soc, in press.
34. Lamouroux F, Heurtevent F, Pailler R, Naslain R, Goujard S. Oxidation protection of carbon fiber reinforced cmc: II—An effective matrix. J Europ Ceram Soc, in press.
35. Lamouroux F, Pailler R, Naslain R, Cataldi M. Matériaux composites thermostructuraux avec renforts en fibres carbone ou revétues de carbone, ayant une résistance accrue á l’oxydation. French patent no. 9514843, 1995.
36. Mechanical behaviour and damage evolution during cyclic fatigue tests at high temperature of a 2.5D C/SiC composite
37. Jacques S. Elaboration et caractérisation de matériaux C(B). Application en tant qu’interphase dans les composites SiC/SiC. Ph.D. thesis no. 1398, University of Bordeaux I, France, 1995.
38. The influence of boron content on the fine microstructure of pyrolytic graphite10.1007/BF00550890 ↗
39. Gas pulse impregnation of graphite with carbon10.13182/NT70-A28648 ↗
40. Pulse CVI of porous carbon10.1007/BF01729344 ↗
41. Pulse chemical vapor infiltration of SiC in porous or SiC particulate preform using a r. f. heating system10.1007/BF00581116 ↗
42. Dupel P. CVD/CVI pulsée de pyrocarbone: application aux matériaux composites thermostructuraux. Ph.D. thesis no. 927, University of Bordeaux, 24 May 1993.
43. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: 1—experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗
44. Kinetics and mechanisms of oxidation of 2D woven C/SiC composites: 2—theoretical approach10.1111/j.1151-2916.1994.tb07097.x ↗