The present work deals with determination of the mechanical properties in the temperature range of 25 to 300 °C of a Mg-10(vol.%)Ti composite. The composite material was processed through powder metallurgical route by mixing pure titanium and magnesium powders followed by hot extrusion. Titanium reinforcement after extrusion presents two different morphologies: highly deformed small elongated particles and practically non-deformed coarse particles. The latter results from large titanium particles or aggregates of Ti particles, which practically did not deform during the extrusion. In addition, fine magnesium oxide particles, less than 1 μm, decorating original boundaries of magnesium particles are present. The mechanical properties at different temperatures were studied by tensile and jump strain rate tests. Although the magnesium matrix shows a relatively large grain size, the composite shows a high strength (160 MPa), with a high elongation at room temperature (8%), higher than most of ceramic reinforced magnesium composites. The stress exponent calculated in the 100-300°C temperature range was about 13 indicating that the deformation is dominated by dislocation slip. Titanium particles strengthen the matrix by load transfer that is manifested by fracture of titanium particles. Furthermore, progress of cracks throughout hard titanium particles results in an increase of the ductility, since propagation of the crack is delayed or even arrested. The effectiveness of titanium reinforcement decreases with increasing the temperature. © 2003 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Project of platform science and technology for advanced magnesium alloys10.2320/matertrans.42.1154 ↗
2. The grain size and texture dependence of tensile properties in extruded Mg–9Al–1Zn10.2320/matertrans.42.1182 ↗
3. Superplastic deformation mechanism in powder metallurgy magnesium alloys and composites10.1016/S1359-6454(01)00101-X ↗
4. Structure and mechanical properties of rapidly solidified Mg-Y based alloys10.1016/S0921-5093(97)80089-5 ↗
5. Effect of yttrium on high temperature strength of magnesium10.2320/matertrans.42.1332 ↗
6. Microstructure and mechanical properties of a Mg–4Y–3RE alloy processed by thermo-mechanical treatment10.1016/S0921-5093(98)00853-3 ↗
7. Mechanical properties of a powder metallurgy processed Mg–5Y–6RE alloy10.1016/S0921-5093(00)01241-7 ↗
8. Focused development of magnesium alloys using the calphad approach10.1002/1527-2648(200112)3:12<947::AID-ADEM947>3.0.CO;2-P ↗
9. High strength and high strain rate superplasticity in a Mg–Mg2Si composite10.1016/0956-716X(95)00140-Q ↗
10. Effect of elevated temperature on ultimate tensile strength and failure modes of short carbon fibre reinforced magnesium composite10.1179/026708302225002083 ↗
11. Microstructure and mechanical properties of magnesium containing high volume fractions of yttria dispersoids10.1016/S0921-5093(99)00074-X ↗
12. Fabrication and mechanical properties of SiCw/ZK51A magnesium matrix composite by two-step squeeze casting10.1016/S0921-5093(99)00608-5 ↗
13. Microstructure and mechanical properties of elemental and reinforced magnesium synthesized using a fluxless liquid-phase process10.1016/S0025-5408(99)00120-8 ↗
14. Magnesium strengthened by SiC nanoparticles10.1016/S0921-5093(00)01283-1 ↗
15. Development of a novel magnesium-copper based composite with improved mechanical properties10.1016/S0025-5408(01)00772-3 ↗
16. Development of ductile magnesium composite materials using titanium as reinforcement10.1016/S0925-8388(02)00413-9 ↗
17. Compressive mechanical properties of Mg–Ti–C nanocomposite synthesised by mechanical milling10.1016/S1359-6462(01)00925-3 ↗
18. Structure and properties of Mg–Al–Ti–B alloys synthesized via mechanical alloying10.1016/S0921-5093(01)01790-7 ↗
19. Development of a novel magnesium/nickel composite with improved mechanical properties10.1016/S0925-8388(01)01841-2 ↗
20. Enhancing the microstructural and mechanical response of a Mg/SiC formulation by the method of reducing extrusion temperature10.1016/S0025-5408(01)00750-4 ↗
21. Activation energies for high temperature creep of polycrystalline magnesium10.1016/0001-6160(61)90166-3 ↗
22. Deformation mechanisms in H.C.P. metals at elevated temperatures-I. Creep behavior of magnesium10.1016/0001-6160(81)90034-1 ↗
23. Deformation mechanisms in H.C.P. metals at elevated temperatures-II. Creep behavior of a Mg-0.8%Al solid solution alloy10.1016/0001-6160(82)90009-8 ↗
24. Analysis of the creep behaviour of a thixoformed AZ91 magnesium alloy10.1016/S0921-5093(00)00911-4 ↗
25. Creep and microstructure of magnesium-aluminum-calcium based alloys10.1007/s11661-002-0118-1 ↗
26. Creep strength of magnesium-based alloys10.1007/s11661-002-1020-6 ↗
27. Creep processes in magnesium alloys and their composites10.1007/s11661-002-1021-5 ↗
28. Creep of magnesium strengthened with high volume fractions of yttria dispersoids10.1016/S0921-5093(00)01781-0 ↗
29. High temperature creep mechanisms in magnesium10.1016/0001-6160(70)90005-2 ↗