journal article·2018-03

Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels

Akihide Nagao, Mohsen Dadfarnia, Brian P. Somerday, Petros Sofronis, Robert O. Ritchie

Publisher page

Abstract

Abstract Hydrogen embrittlement of lath martenistic steels is characterized by intergranular and “quasi-cleavage” transgranular fracture. Recent transmission electron microscopy (TEM) analyses (Nagao et al., 2012a, 2014a, 2014b, 2014c) of samples lifted from beneath fracture surfaces through focused ion beam machining (FIB) revealed a failure mechanism that can be termed hydrogen-enhanced-plasticity mediated decohesion. Fracture occurs by the synergistic action of the hydrogen-enhanced localized plasticity and decohesion. In particular, intergranular cracking takes place by dislocation pile-ups impinging on prior austenite grain boundaries and “quasi-cleavage” is the case when dislocation pile-ups impinge on block boundaries. These high-angle boundaries, which have already weakened by the presence of hydrogen, debond by the pile-up stresses. The micromechanical model of Novak et al. (2010) is used to quantitatively describe and predict the hydrogen-induced failure of these steels. The model predictions verify that introduction of nanosized (Ti,Mo)C precipitates in the steel microstructure enhances the resistance to hydrogen embrittlement. The results are used to discuss microstructural designs that are less susceptible to hydrogen-induced failure in systems with fixed hydrogen content (closed systems).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. Empirical formulae for the calculation of some transformation temperatures
2. Hydrogen trapping behavior in vanadium-added steel10.2355/isijinternational.43.527 ↗
3. Hydrogen-induced cracking in 4340-type steel: effects of composition, yield strength and H2 pressure10.1007/BF02644292 ↗
4. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)
5. Hydrogen-enhanced localized plasticity–a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
6. Mechanisms of hydrogen related fracture—a review
7. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
8. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
9. Hydrogen interaction with multiple traps: can it be used to mitigate embrittlement? Int10.1016/j.ijhydene.2011.05.027 ↗
10. A critical-strain criterion for hydrogen embrittlement of cold-drawn, ultrafine pearlitic steel10.1007/s11661-002-0217-z ↗
11. Thermal desorption spectroscopy study of experimental Ti/S containing steels10.1179/1743284712Y.0000000141 ↗
12. 2012
13. Quasi-cleavage and martensite habit plane10.1016/0001-6160(84)90190-1 ↗
14. Crack growth from internal hydrogen–temperature and microstructural effects in 4340 steel10.1007/BF02662593 ↗
15. Hydrogen induced cracking mechanisms - are there critical experiments?
16. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
17. Hirth · 1982
18. On the thermodynamics of adsorption at interfaces as it influences decohesion10.1007/BF02654514 ↗
19. The measurement of the trap binding energy by the thermal analysis technique10.1016/0036-9748(83)90242-9 ↗
20. The interaction of hydrogen and the cementite–ferrite interface in carbon steel10.1007/BF00543835 ↗
21. Trapping against hydrogen embrittlement
22. Dislocation transport of hydrogen in iron single crystals10.1016/0001-6160(86)90209-9 ↗
23. The effect of hydrogen atoms on the screw dislocation mobility in bcc iron: a first-principles study10.1016/j.actamat.2013.07.064 ↗
24. A microscopic theory of brittle fracture in deformable solids: a relation between ideal work to fracture and plastic work10.1016/0001-6160(80)90048-6 ↗
25. Numerical analysis of hydrogen trap state by TiC and V4C3 in bcc-Fe10.2355/isijinternational.52.1693 ↗
26. Ab-initio investigation of hydrogen trap state by cementite in bcc-Fe10.2355/isijinternational.53.709 ↗
27. The nature of quasiclevage fracture in tempered 5.5Ni steel after hydrogen charging10.1007/BF02645559 ↗
28. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
29. Crystallographic features of lath martensite in low-carbon steel10.1016/j.actamat.2005.11.001 ↗
30. Krauss · 1990
31. Deep trapping states for hydrogen in deformed iron10.1016/0001-6160(80)90038-3 ↗
32. Over the mechanisms of steel hardening
33. Effect of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
34. A Trapping theory of hydrogen in pure iron10.1080/01418618708214387 ↗
35. Hydrogen trapping by TiC particles in iron10.1016/0001-6160(84)90210-4 ↗
36. Hydrogen trap states in ultrahigh-strength AERMET 100 steel10.1007/s11661-004-0011-1 ↗
37. Micromechanics and numerical modelling of the hydrogen-particle-matrix interactions in nickel-base alloys10.1088/0965-0393/11/4/308 ↗
38. A statistical model of brittle fracture by transgranular cleavage10.1016/0022-5096(86)90013-X ↗
39. A fractographic study of gaseous hydrogen embrittlement and liquid-metal embrittlement in a tempered-mertensitic steel10.1016/0001-6160(84)90204-9 ↗
40. Role of Nb in low interstitial 13Cr super martensitic stainless steel10.1016/j.msea.2011.05.065 ↗
41. Strain gradient plasticity-based modeling of hydrogen environment assisted cracking10.1016/j.actamat.2016.07.022 ↗
42. Thermodynamics and diffusion behavior of interstitial solute atoms in non-perfect solvent crystals10.1016/0001-6160(79)90047-6 ↗
43. The morphology and crystallography of lath martensite in alloy steels10.1016/j.actamat.2006.07.009 ↗
44. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
45. Hydrogen embrittlement: Mechanisms
46. Effect of uniform distribution of fine cementite on hydrogen embrittlement of low carbon martensitic steel plates10.2355/isijinternational.52.213 ↗
47. Hydrogen microprint technique applied to observe impurity hydrogen in aluminum during deformation.
48. The effect of nanosized (Ti,Mo)C precipitates on hydrogen embrittlement of tempered lath martensitic steel10.1016/j.actamat.2014.04.051 ↗
49. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
50. Interpretation of hydrogen-induced fracture surface morphologies for lath martensitic steel10.1016/j.mspro.2014.06.274 ↗
51. The role of plasticity in hydrogen embrittlement fracture of lath martensitic steel.
52. Function of hydrogen in intergranular fracture of martensitic steels10.1080/01418610208240452 ↗
53. Physical chemistry of the groups IVa (Ti, Zr), Va (V, Nb, Ta) and the rare earth elements in steel10.2355/isijinternational1966.15.145 ↗
54. Nelson · 1973
55. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
56. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
57. Hydrogen the versatile embrittler10.5006/1.3583875 ↗
58. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
59. Equilibrium and kinetic studies of hydrogen-assisted cracking of steel10.1016/0001-6160(77)90126-2 ↗
60. The effect of hot rolling condition and chemical composition on the onset temperature of γ-α transformation after hot rolling10.2355/isijinternational1966.22.214 ↗
61. Embrittlement of interfaces by solute segregation10.1016/0921-5093(89)90372-9 ↗
62. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(99)00094-6 ↗
63. Hydrogen effects on plasticity
64. Direct measurement of mobility of edge and screw dislocations in 3% silicon-iron by high voltage transmission electron microscopy10.1143/JPSJ.32.702 ↗
65. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
66. The influence of palladium on the hydrogen-assisted cracking resistance of PH 13-8 Mo stainless steel10.1007/BF02665009 ↗
67. Influence of traps on the deuterium behaviour in the low activation martensitic steels F82H and Batman10.1016/S0022-3115(97)00021-4 ↗
68. Fracture surface topography analysis of the hydrogen-related fracture propagation process in martensitic steel10.1007/s10704-017-0182-6 ↗
69. The nucleation and growth of cleavage microcracks in mild steel.
70. Mechanics of the hydrogen-dislocation-impurity interactions–I. increasing shear modulus10.1016/0022-5096(94)00056-B ↗
71. Hydrogen induced shear localization of the plastic flow in metals and alloys10.1016/S0997-7538(01)01179-2 ↗
72. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
73. Micromechanical modeling of hydrogen transport–a review
74. 2014
75. The interaction of hydrogen and dislocations in iron10.1016/0001-6160(69)90097-2 ↗
76. The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography10.1016/j.scriptamat.2010.03.012 ↗
77. Identification of hydrogen desorption peak temperatures, binding energies, and occupation ratios at vacancies, dislocations and grain boundaries in iron and steel
78. Special issue on common bases for hydrogen embrittlement studies10.2355/isijinternational.52.167 ↗
79. Hydrogen transport by dislocations10.1007/BF02644079 ↗
80. The role of hydrogen and other interstitials in the mechanical behavior of metals
81. Ultragrain refinement of plain low carbon steel by cold-rolling and annealing of martensite10.1016/S1359-6454(02)00260-4 ↗
82. Effect of hydrogen environment on the separation of Fe grain boundaries10.1016/j.actamat.2016.01.067 ↗
83. Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum10.1007/s11663-004-0057-x ↗
84. Hydrogen absorption of incoherent TiC particles in iron from environment at high temperatures10.1007/s11661-004-0060-5 ↗
85. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
86. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
87. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum10.1080/14786435608238074 ↗
88. The cooperative relation between temper embrittlement and hydrogen embrittlement in a high strength steel10.1007/BF02644103 ↗