journal article·2026-03

Effect of Post-heat Treatment on the Load-Dependent Wear Mechanisms of AISI D2 Tool Steel Manufactured by Laser Direct Energy Deposition

Jung-Hyun Park, Kyu-Sik Kim, Yong-Mo Koo, Jong-Bae Jeon, Kee-Ahn Lee

Journal of Thermal Spray Technology· Volume 35· Issue 2-3
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Y.K. Chou and C.J. Evans, Tool Wear Mechanism in Continuous Cutting of Hardened Tool Steels, Wear, 1997, 212, p 59–65.10.1016/S0043-1648(97)00139-7 ↗
2. T.S. Srivatsan, R. Annigeri, and A. Prakash, Tensile Deformation and Fracture Behaviour of a Tool-Steel-Based Metal-Matrix Composite, Compos. Part A Appl. Sci. Manuf., 1997, 28, p 377–385.10.1016/S1359-835X(96)00137-6 ↗
3. S. Kheirandish and A. Noorian, Effect of Niobium on Microstructure of Cast AISI H13 Hot Work Tool Steel, J. Iron. Steel Res. Int., 2008, 15, p 61–66.10.1016/S1006-706X(08)60145-4 ↗
4. M.A.S.B.A. Rahim, M.B. Minhat, N.I.S.B. Hussein, and M.S.B. Salleh, A Comprehensive Review on Cold Work of AISI D2 Tool Steel, Metall. Res. Technol., 2018, 115, p 104.10.1051/metal/2017048 ↗
5. M.B. Mhamdi, S.B. Salem, M. Boujelbene, and E. Bayraktar, Experimental Study of the Chip Morphology in Turning Hardened AISI D2 Steel, J. Mech. Sci. Technol., 2013, 27, p 3451–3461.10.1007/s12206-013-0869-1 ↗
6. T. Nykiel and T. Hryniewicz, Effect of High-Temperature Heating on Chemical Changes in M7C3 Carbides of AISI D2 Tool Steel, Int. Lett. Chem. Phys. Astron., 2014, 17, p 258–271.10.56431/p-6203wy ↗
7. C.M. Garzón, A.R. Franco, and A.P. Tschiptschin, Thermodynamic Analysis of M7C3 Carbide Dissolution During Plasma Nitriding of an AISI D2 Tool Steel, ISIJ Int., 2017, 57, p 737–745.10.2355/isijinternational.ISIJINT-2016-553 ↗
8. S. Kahrobaee and M. Kashefi, Electromagnetic Nondestructive Evaluation of Tempering Process in AISI D2 Tool Steel, J. Magn. Magn. Mater., 2015, 382, p 359–365.10.1016/j.jmmm.2015.02.007 ↗
9. H.G. Nanesa and M. Jahazi, Alternative Phase Transformation Path in Cryogenically Treated AISI D2 Tool Steel, Mater. Sci. Eng. A, 2015, 634, p 32–36.10.1016/j.msea.2015.03.028 ↗
10. S.J. Gobbi, V.J. Gobbi, G. Reinke, P.V. Muterlle, and D.M. Rosa, Ultra-Low-Temperature Process Effects on Microscale Abrasion of Tool Steel AISI D2, Mater. Sci. Technol., 2019, 35, p 1355–1364.10.1080/02670836.2019.1624018 ↗
11. D. Das, A.K. Dutta, and K.K. Ray, Influence of Varied Cryotreatment on the Wear Behavior of AISI D2 Steel, Wear, 2009, 266, p 297–309.10.1016/j.wear.2008.07.001 ↗
12. L. Tang, C. Gao, J. Huang, H. Zhang, and W. Chang, Dry Sliding Friction and Wear Behaviour of Hardened AISI D2 Tool Steel with Different Hardness Levels, Tribol. Int., 2013, 66, p 165–173.10.1016/j.triboint.2013.05.006 ↗
13. K. Singh, R.K. Khatirkar, and S.G. Sapate, Microstructure Evolution and Abrasive Wear Behavior of D2 Steel, Wear, 2015, 328, p 206–216.10.1016/j.wear.2015.02.019 ↗
14. V. Braga, R.H.M. Siqueira, I. Atilio, R. Mansur, D. Vieira, D.L. Chen, and M.S.F. Lima, Microstructural and Mechanical Aspects of Laser Metal Deposited H13 Powder for Die Repair, Mater. Today Commun., 2021, 29, 102945.10.1016/j.mtcomm.2021.102945 ↗
15. Y. Zeng, L. Li, W. Huang, Z. Zhao, W. Yang, and Z. Yue, Effect of Thermal Cycles on Laser Direct Energy Deposition Repair Performance of Nickel-Based Superalloy: Microstructure and Tensile Properties, Int. J. Mech. Sci., 2022, 221, 107173.10.1016/j.ijmecsci.2022.107173 ↗
16. I.H. Kim, Y.J. Jung, H.G. Kim, and J.I. Jang, Oxidation-Resistant Coating of FeCrAl on Zr-Alloy Tubes Using 3D Printing Direct Energy Deposition, Surf. Coat. Technol., 2021, 411, 126915.10.1016/j.surfcoat.2021.126915 ↗
17. W. Li, M.N. Kishore, R. Zhang, N. Bian, H. Lu, Y. Li, D. Qian, and X. Zhang, Comprehensive Studies of SS316L/IN718 Functionally Gradient Material Fabricated with Directed Energy Deposition: Multi-Physics & Multi-Materials Modelling and Experimental Validation, Addit. Manuf., 2023, 61, 103358.
18. D.D. Singh, S. Arjula, and A.R. Reddy, Functionally Graded Materials Manufactured by Direct Energy Deposition: A Review, Mater. Today: Proc., 2021, 47, p 2450–2456.
19. V. Brøtan, O.Å. Berg, and K. Sørby, Additive Manufacturing for Enhanced Performance of Molds, Procedia CIRP, 2016, 54, p 186–190.10.1016/j.procir.2016.05.074 ↗
20. J. Leunda, C. Soriano, C. Sanz, and V.G. Navas, Laser Cladding of Vanadium-Carbide Tool Steels for Die Repair, Phys. Procedia, 2011, 12, p 345–352.10.1016/j.phpro.2011.03.044 ↗
21. G.Y. Baek, G.Y. Shin, E.M. Lee, D.S. Shim, K.Y. Lee, H.S. Yoon, and M.H. Kim, Mechanical Characteristics of a Tool Steel Layer Deposited by Using Direct Energy Deposition, Met. Mater. Int., 2017, 23, p 770–777.10.1007/s12540-017-6442-1 ↗
22. A. Ankara and H.B. Ari, Determination of Hot Crack Susceptibility in Various Kinds of Steels, Mater. Des., 1996, 17, p 261–265.10.1016/S0261-3069(97)00019-8 ↗
23. Q. Yan, K. Tang, Z.D. Wang, M.Z. Chen, G.F. Sun, and Z.H. Ni, Surface Roughness Optimization and High-Temperature Wear Performance of H13 Coating Fabricated by Extreme High-Speed Laser Cladding, Opt. Laser Technol., 2022, 149, 107823.10.1016/j.optlastec.2021.107823 ↗
24. M. Sorgato, R. Bertolini, A. Ghiotti, and S. Bruschi, Tool Wear Assessment When Drilling AISI H13 Tool Steel Multilayered Claddings, Wear, 2023, 524, 204853.10.1016/j.wear.2023.204853 ↗
25. M. Pellizzari, Z. Zhao, P. Bosetti, and M. Perini, Optimizing Direct Laser Metal Deposition of H13 Cladding on CuBe Alloy Substrate, Surf. Coat. Technol., 2022, 432, 128084.10.1016/j.surfcoat.2022.128084 ↗
26. L. Zhu, S. Wang, H. Pan, C. Yuan, and X. Chen, Research on Remanufacturing Strategy for 45 Steel Gear Using H13 Steel Powder Based on Laser Cladding Technology, J. Manuf. Process., 2020, 49, p 344–354.10.1016/j.jmapro.2019.12.009 ↗
27. J.H. Park, K.S. Kim, J.Y. Kim, J.B. Jeon, Y.M. Koo, and K.A. Lee, Microstructure and Tensile Properties of Bulk AISI D2 Tool Steel Fabricated by Direct Energy Deposition, Mater Charact, 2022, 194, 112355.10.1016/j.matchar.2022.112355 ↗
28. J.H. Park, K.S. Kim, Y.M. Koo, J.Y. Kim, M.C. Kim, and K.A. Lee, Effect of Post-Heat Treatment on the Impact Toughness and Crack Propagation Mechanism of AISI D2 Tool Steel Manufactured by Direct Energy Deposition, Arch. Metall. Mater., 2023, 68, p 119–122.10.24425/amm.2023.141483 ↗
29. Y.K. Park, K.S. Ha, K.Y. Shin, K.Y. Lee, D.J. Kim, S.H. Kwon, and W.J. Lee, Wear Resistance of Direct-Energy–Deposited AISI M2 Tool Steel with and Without Post-Heat Treatment, Int. J. Adv. Manuf. Technol., 2021, 116, p 3917–3931.10.1007/s00170-021-07741-9 ↗
30. J. Zeisig, N. Schädlich, L. Giebeler, J. Sander, J. Eckert, and U. Kühn, Microstructure and Abrasive Wear Behavior of a Novel FeCrMoVC Laser Cladding Alloy for High-Performance Tool Steels, Wear, 2017, 382, p 107–112.10.1016/j.wear.2017.04.021 ↗
31. D.S. Shim, G.Y. Baek, S.B. Lee, J.H. Yu, Y.S. Choi, and S.H. Park, Influence of Heat Treatment on Wear Behavior and Impact Toughness of AISI M4 Coated by Laser Melting Deposition, Surf. Coat. Technol., 2017, 328, p 219–230.10.1016/j.surfcoat.2017.08.059 ↗
32. S. Yadav, K. Dileep, A.N. Jinoop, C.P. Paul, A.K. Rai, R. Singh, and K.S. Bindra, Laser Directed Energy Deposition of High-Carbon High-Chromium D2 Tool Steel Structures: Processing, Heat Treatment and Material Behavior, J. Mater. Eng. Perform., 2023, 32, p 4881–4891.10.1007/s11665-022-07470-4 ↗
33. K.W. Kim, G.S. Ham, S.H. Park, J.W. Cho, and K.A. Lee, Direct energy Deposition of Ultrastrong WC-12Co Cemented Carbide: Fabrication, Microstructure and Compressive Properties, Int. J. Refract. Met. Hard Mater., 2021, 99, 105591.10.1016/j.ijrmhm.2021.105591 ↗
34. B. Rouxel, S. Mischler, R.E. Logé, and A. Igual Munoz, Wear Behaviour of Novel Copper Alloy as An Alternative to Copper-Beryllium, Wear, 2023, 524, 204817.10.1016/j.wear.2023.204817 ↗
35. G. Telasang, J.D. Majumdar, G. Padmanabham, and I. Manna, Wear and Corrosion Behavior of Laser Surface Engineered AISI H13 Hot Working Tool Steel, Surf. Coat. Technol., 2015, 261, p 69–78.10.1016/j.surfcoat.2014.11.058 ↗
36. ASTM International (2010) Standard Test Method for Linearly Reciprocating Ball-on-Flat Sliding Wear, ASTM G133-05, ASTM International, West Conshohocken, PA
37. N.R. Rundora, D.E.P. Klenam, S. Polat, N.M. Mathabathe, J. van der Merwe, and M.O. Bodunrin, Dry Sliding Wear Behavior of Experimental Low-Cost Titanium Alloys, Tribology Trans., 2024, 67, p 560–572.10.1080/10402004.2024.2357288 ↗
38. A. Jana, N. Dandapat, M. Das, V.K. Balla, S. Chakraborty, R. Saha, and A.K. Mallik, Severe Wear Behaviour of Alumina Balls Sliding Against Diamond Ceramic Coatings, Bull. Mater. Sci., 2016, 39, p 573–586.10.1007/s12034-016-1166-2 ↗
39. H.A. Abboodi, H. Fan, I.A. Mhmood, and M.A. Bahrani, The dry sliding Wear Rate of a Fe-Based Amorphous Coating Prepared on Mild Steel by HVOF Thermal Spraying, J. Mater. Res. Technol., 2022, 18, p 1682–1691.10.1016/j.jmrt.2022.03.081 ↗
40. G. Lacob, V.G. Ghica, M. Buzatu, T. Buzatu, and M.I. Petrescu, Studies on Wear Rate and Micro-Hardness of the Al/Al2O3/Gr Hybrid Composites Produced Via Powder Metallurgy, Compos. B Eng., 2015, 69, p 603–611.10.1016/j.compositesb.2014.07.008 ↗
41. J.S. Park, M.G. Lee, Y.J. Cho, J.H. Sung, M.S. Jeong, S.K. Lee, Y.J. Choi, and D.H. Kim, Effect of Heat Treatment on the Characteristics of Tool Steel Deposited by the Directed Energy Deposition Process, Met. Mater. Int., 2016, 22, p 143–147.10.1007/s12540-016-5372-7 ↗
42. S.H. Lim, K.H. Ryou, K.S. Jang, W.S. Choi, H.M. Lee, and P.P. Choi, Hot Cracking Behavior of Additively Manufactured D2 Steel, Mater Charact, 2021, 178, 111217.10.1016/j.matchar.2021.111217 ↗
43. L. Bourithis, G.D. Papadimitriou, and J. Sideris, Comparison of Wear Properties of Tool Steels AISI D2 and O1 with the Same Hardness, Tribol. Int., 2006, 39, p 479–489.10.1016/j.triboint.2005.03.005 ↗
44. S. Kibey, J.B. Liu, M.J. Curtis, D.D. Johnson, and H. Sehitoglu, Effect of Nitrogen on Generalized Stacking Fault Energy and Stacking Fault Widths in High Nitrogen Steels, Acta Mater., 2006, 54, p 2991–3001.10.1016/j.actamat.2006.02.048 ↗
45. Y. Jiao, B. Tang, J. Wang, P. Jin, and X. Jiang, Effects of the T6 Heat Treatment on the Tribological Behaviors of SiCp/7055Al Composites, Mater. Today Commun., 2022, 33, 104670.10.1016/j.mtcomm.2022.104670 ↗
46. H.-W. Wu, Y.-Y. Chen, and J.-H. Horng, The Analysis of Three-Body Contact Temperature Under the Different Third Particle Size, Density, and Value of Friction, Micromachines, 2017, 8, 302.10.3390/mi8100302 ↗
47. J.C. Jaeger, Moving Sources of Heat, and the Temperature at Sliding Contacts, Proc. Roy. Soc. N. S. W., 1942, 76, p 203–224.
48. M. Federici, G. Straffelini, and S. Gialanella, Pin-on-disc Testing of low-Metallic Friction Material Sliding Against HVOF Coated Cast Iron: Modelling of the Contact Temperature Evolution, Tribol. Lett., 2017, 65, 121.10.1007/s11249-017-0904-y ↗
49. N. Tenwick, and S.W.E. Earles, A Simplified Theory for the Oxidative Wear of Steels, Wear, 1971, 18, p 381–391.10.1016/0043-1648(71)90002-0 ↗
50. J. Choudhry, A. Almqvist, and R. Larsson, Validation of a Multi-Scale Contact Temperature Model for Dry Sliding Rough Surfaces, Lubricants, 2022, 10, 41.10.3390/lubricants10030041 ↗
51. Z. Zhu, Y. Liang, C. Yin, X. Ren, M. Yang, and J. Zou, Influence of Friction-Induced Retained Austenite Transformation to Martensite on the Wear Properties of a Carburized Layer of 23CrNi3MoA Steel, Appl. Surf. Sci., 2022, 595, 153548.10.1016/j.apsusc.2022.153548 ↗
52. Q. Luo, J. Li, Q. Yan, W. Li, Y. Gao, M. Kitchen, L. Bowen, N. Farmilo, and Y. Ding, Sliding Wear of Medium-Carbon bainitic/martensitic/austenitic Steel Treated by Short-Term Low-Temperature Austempering, Wear, 2021, 476, 203732.10.1016/j.wear.2021.203732 ↗
53. D.C. Ko, S.G. Kim, and B.M. Kim, Influence of Microstructure on Galling Resistance of Cold-Work Tool Steels with Different Chemical Compositions When Sliding Against Ultra-High-Strength Steel Sheets Under Dry Condition, Wear, 2015, 338, p 362–371.10.1016/j.wear.2015.07.014 ↗
54. J. Sander, J. Hufenbach, L. Giebeler, M. Bleckmann, J. Eckert, and U. Kühn, Microstructure, Mechanical Behavior, and Wear Properties of FeCrMoVC Steel Prepared by Selective Laser Melting and Casting, Scr. Mater., 2017, 126, p 41–44.10.1016/j.scriptamat.2016.07.029 ↗
55. S.F. Gnyusov, E.A. Fedin, and S.Y. Tarasov, The Effect of Counterbody on Tribological Adaptation of an Electron Beam Deposited HSS M2 Steel Coating in a Range of Sliding Speeds and Normal Loads, Tribol. Int., 2021, 161, 107109.10.1016/j.triboint.2021.107109 ↗
56. H. Torkamani, S.H. Raygan, and J. Rassizadehghani, Comparing Microstructure and Mechanical Properties of AISI D2 Steel After Bright Hardening and Oil Quenching, Mater. Des., 2014, 54, p 1049–1055.10.1016/j.matdes.2013.09.043 ↗
57. D. Das, R. Sarkar, A.K. Dutta, and K.K. Ray, Influence of Sub-Zero Treatments on Fracture Toughness of AISI D2 Steel, Mater. Sci. Eng. A, 2010, 528, p 589–603.10.1016/j.msea.2010.09.057 ↗
58. S.H. Wang, J.Y. Chen, and L. Xue, A Study of the Abrasive Wear Behaviour of Laser-Clad Tool Steel Coatings, Surf. Coat. Technol., 2006, 200, p 3446–3458.10.1016/j.surfcoat.2004.10.125 ↗
59. S. Yin, C. Chen, X. Yan, X. Feng, R. Jenkins, P. O’Reilly, M. Liu, H. Li, and R. Rupoi, The Influence of Aging Temperature and Aging Time on the Mechanical and Tribological Properties of Selective Laser Melted Maraging 18Ni-300 Steel, Addit. Manuf., 2018, 22, p 592–600.