This article is concerned with the influence of surface treatment on the strength of single lap joints. The tensile tests were carried out in order to find the surface treatments which maximize joint strength using polypropylene reinforced glass fiber as adherents. The maximum shear strength was obtained with the trichlorethylene plus primer treatment when using a cyanoacrylate adhesive. The pretreatment effectiveness was evaluated in terms of environmental durability and an important decrease in static strength of adhesive joints occurred when they were immersed in water.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Mechanical Behavior of Composites · Structural Analysis of Composite Materials · Material Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Electromechanical Engineering, University of Beira Interior, Covilhã, Portugal

CEMUC, Department of Mechanical Engineering, University of Coimbra, Portugal

Department of Mechanical and Design Engineering, University of Portsmouth, United Kingdom

References (31)

Show source-provided references
1. 10.1007/978-1-4615-5133-110.1007/978-1-4615-5133-1 ↗
2. Lees W.A. · International Journal of Materials and Product Technology · 1987 · 2 · 168
3. 10.1016/S0266-3538(02)00082-910.1016/S0266-3538(02)00082-9 ↗
4. 10.1016/j.compstruct.2004.01.01810.1016/j.compstruct.2004.01.018 ↗
5. 10.1016/0143-7496(94)90039-610.1016/0143-7496(94)90039-6 ↗
6. 10.1016/0143-7496(87)90092-310.1016/0143-7496(87)90092-3 ↗
7. 10.1016/S0143-7496(99)00032-910.1016/S0143-7496(99)00032-9 ↗
8. 10.1016/S0143-7496(97)00056-010.1016/S0143-7496(97)00056-0 ↗
9. Hattori T. · JSME International Journal · 1991 · 34 · 326
10. 10.1163/15685610074210410.1163/156856100742104 ↗
11. 10.1080/0021846990801723110.1080/00218469908017231 ↗
12. 10.1016/0143-7496(90)90025-S10.1016/0143-7496(90)90025-S ↗
13. 10.1016/j.ijadhadh.2010.12.00310.1016/j.ijadhadh.2010.12.003 ↗
14. 10.1002/pen.76029190410.1002/pen.760291904 ↗
15. 10.1016/0010-4361(82)90168-910.1016/0010-4361(82)90168-9 ↗
16. 10.1016/0143-7496(93)90036-910.1016/0143-7496(93)90036-9 ↗
17. 10.1016/0143-7496(94)90009-410.1016/0143-7496(94)90009-4 ↗
18. 10.1163/15685610074309510.1163/156856100743095 ↗
19. 10.1016/S0143-7496(00)00044-010.1016/S0143-7496(00)00044-0 ↗
20. 10.1007/BF0027463810.1007/BF00274638 ↗
21. 10.1007/BF0126227310.1007/BF01262273 ↗
22. 10.1002/app.1971.07015022310.1002/app.1971.070150223 ↗
23. 10.1080/0021846890804820610.1080/00218468908048206 ↗
24. 10.1080/0021846930802655910.1080/00218469308026559 ↗
25. 10.1163/15685610074218610.1163/156856100742186 ↗
26. 10.1163/156856196X0056210.1163/156856196X00562 ↗
27. 10.1016/0143-7496(92)90048-Z10.1016/0143-7496(92)90048-Z ↗
28. 10.1016/S0167-8442(98)00068-810.1016/S0167-8442(98)00068-8 ↗
29. 10.1016/0143-7496(86)90002-310.1016/0143-7496(86)90002-3 ↗
30. Grassie N., Scott G. (1985). Polymer Degradation and Stabilisation, pp. 44–48, Cambridge University Press, Cambridge, UK.
31. 10.1002/app.1993.07047060810.1002/app.1993.070470608 ↗