Study on interlaminar performance of CNTs/epoxy film enhanced GFRP under low-temperature cycle
Source abstract
Abstract
Abstract The laminates of unidirectional (UD) Glass Fiber Reinforced Plastic (GFRP) were prepared by inserting Toner/epoxy film (as a comparison) and CNTs/epoxy film between layers to optimize the interlaminar performance. The effect of temperature variation on the interlaminar properties of materials has yet to be identified in practical applications. To explore the impact of low-temperature cycle (21 cycles between −58 °C and RT) on the specimens and the strengthening mechanism of the two epoxy films, interlaminar shear strength (ILSS) test, end notch flexure (ENF) test and double cantilever beam (DCB) test were prepared and carried out. The results showed that the interlaminar fracture toughness of GFRP embedded with the CNTs/epoxy film was superior to that of GFRP without film and embedded with the Toner/epoxy film in modes I (based on DCB) and II (based on ENF). The interlaminar shear strength was greatly enhanced by the interlaminar integration of CNTs/epoxy film. The impact of low-temperature cycle on the interlaminar performance of CNTs/epoxy enhanced GFRP was not significant, and the effect on the interlaminar properties of CNTs/epoxy enhanced GFRP was minimal compared with the other two kinds of specimens. The microstructure of the interlaminar strengthening interface was further studied by scanning electron microscopy (SEM).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical Behavior of Composites · Structural Analysis of Composite Materials · Advanced Fiber Optic Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Fracture behaviour of carbon fibre/epoxy composites interleaved by MWCNT- and graphene nanoplatelet-doped thermoplastic veils10.1016/j.compstruct.2019.111767 ↗
2. A review of strategies for improving the degradation properties of laminated continuous-fiber/epoxy composites with carbon-based nanoreinforcements10.1016/j.carbon.2012.01.059 ↗
3. Poly(phenylene sulphide) and poly(ether ether ketone) composites reinforced with single-walled carbon nanotube buckypaper: II–mechanical properties, electrical and thermal conductivity10.1016/j.compositesa.2011.11.003 ↗
4. Mode II interfacial fracture characterization of foam core sandwich materials at elevated temperatures: the effects of frictional stresses between the crack edges10.1016/j.ijsolstr.2020.02.001 ↗
5. Thermosetting CFRP interlaminar toughening with multi-layers graphene and MWCNTs under mode I fracture10.1016/j.compscitech.2019.107829 ↗
6. Interlaminar toughening of unidirectional CFRP with multilayers graphene and mwcnts for mode II fracture10.1016/j.compstruct.2020.111888 ↗
7. Interlaminar properties of GFRP laminates toughened by CNTs buckypaper interlaminar10.1016/j.compstruct.2018.10.002 ↗
8. Mode II interlaminar fracture toughness of carbon nanotubes/epoxy film-interleaved carbon fiber composites10.1016/j.compstruct.2019.111808 ↗
9. Effect of cristobalite formation on the delamination resistance of an oxide/si/(sic/sic) environmental barrier coating system after cyclic high temperature thermal exposure10.1016/j.scriptamat.2017.06.006 ↗
10. Influence of the temperature in the delamination under mode I of fracture and dynamic loading of two carbon-epoxy composites10.1016/j.compositesb.2014.08.051 ↗
11. Influence of low-temperatures on the phenomenon of delamination of mode I fracture in carbon-fibre/epoxy composites under fatigue loading10.1016/j.compstruct.2014.02.007 ↗
12. Temperature effects on mixed mode I/II delamination under quasi-static and fatigue loading of a carbon/epoxy composite10.1016/j.compositesa.2015.05.016 ↗
13. Mode I fatigue delamination growth in GFRP woven laminates at low-temperatures10.1016/j.engfracmech.2006.03.015 ↗
14. Delamination and kink-band failure of pultruded gfrp laminates under elevated temperatures and compression10.1016/j.compstruct.2010.07.010 ↗
15. Fatigue delamination growth in woven glass/epoxy composite laminates under mixed-mode II/III loading conditions at cryogenic temperatures10.1016/j.cryogenics.2013.10.001 ↗
16. Experimental torsional shear properties of carbon fiber reinforced epoxy composites containing carbon nanotubes10.1016/j.compstruct.2013.04.033 ↗
17. Enhanced dielectric and mechanical properties in chlorine-doped continuous CNT sheet reinforced sandwich polyvinylidene fluoride film10.1016/j.carbon.2016.05.068 ↗
18. Effects of loading rates on mode i interlaminar fracture toughness of carbon/epoxy composite toughened by carbon nanotube films10.1016/j.compositesb.2020.108270 ↗
19. Mechanical and electrical properties of laminated composites containing continuous carbon nanotube film interleaves10.1016/j.compscitech.2016.02.032 ↗
20. Elastic-plastic fracture assessment of CNT-reinforced epoxy/nanocomposite specimens weakened by U-shaped notches under mixed mode loading10.1016/j.compositesb.2019.107114 ↗
21. Noncovalent side-wall functionalization of single-walled carbon nanotubes Macromolecules10.1021/ma021417n ↗
22. High weight fraction surfactant solubilization of single-wall carbon nanotubes in water10.1021/nl025924u ↗
23. A simple and fast method to disperse long single-walled carbon nanotubes introducing few defects10.1016/j.carbon.2011.03.040 ↗
24. Enhancing interlaminar fracture characteristics of woven CFRP prepreg composites through CNT dispersion10.1177/0021998311410472 ↗
25. Mode I and II interlaminar critical energy release rates in all-carbon interlayer unidirectional fibre-hybrids based on ultrahigh-modulus and high-strength fibres
26. Enhancing Mode I and Mode II interlaminar fracture toughness of flax fibre reinforced epoxy composites with nano TiO210.1016/j.compositesa.2019.105505 ↗
27. Thermal cycles effects on interlaminar shear strength (ILSS) and impact behaviour of carbon/PEI composites10.1007/s10853-005-3661-5 ↗
28. Interlaminar shear strength of fibre metal laminates after thermal cycles10.1016/j.compstruct.2018.09.001 ↗