journal article·2024-11

Analysis of the fracture behavior and mechanism of PIP-C/SiC composites at high temperatures

Kunjie Wang, Chenghai Xu, Bo Gao, Leying Song, Songhe Meng

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Advances in ultra-high temperature ceramics composites, and coatings10.1007/s40145-021-0550-6 ↗
2. Krenkel · 2008
3. Potential application of ceramic matrix composites to aero-engine components10.1016/S1359-835X(98)00139-0 ↗
4. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
5. Ceramic composites: A review of toughening mechanisms and demonstration of micropillar compression for interface property extraction
6. Fracture behaviour of 2D-weaved, silica-silica continuous fibre-reinforced, ceramic-matrix composites (CFCCs)10.1016/j.engfracmech.2004.02.005 ↗
7. Mechanical behavior of 2D and 3D weaved SiC-matrix, carbon-continuous-fibre-reinforced composites: Part 2. Fracture toughness under static loading conditions10.1016/j.engfracmech.2017.07.003 ↗
8. Fracture toughness of 2-D woven SiC/SiC CVI-composites with multilayered interphases10.1111/j.1151-2916.1996.tb08516.x ↗
9. Toughening behavior of a two-dimensional SiC/SiC woven composite at ambient temperature: I, damage initiation and R-curve behavior10.1111/j.1151-2916.1998.tb02462.x ↗
10. Mode I and Mode II interfacial fracture energy of SiC/BN/SiC CMCs10.1016/j.actamat.2021.117125 ↗
11. Large scale bridging in brittle matrix composites10.1016/0956-7151(90)90301-V ↗
12. Remarks on crack-bridging concepts10.1115/1.3119764 ↗
13. Fracture behaviour of SiC/SiC ceramic matrix composite at room temperature10.1016/j.jeurceramsoc.2022.01.060 ↗
14. Effect of fiber directionality on the static and dynamic mechanical properties of 3D SiCf/SiC composites10.1016/j.msea.2016.02.006 ↗
15. Effect of SiC content on the mechanical behaviour of a three-dimensional needled C/SiC composite10.1016/j.ceramint.2021.05.237 ↗
16. Evaluation of fracture toughness of ceramic matrix composites using small specimens10.1016/S0920-3796(02)00150-3 ↗
17. Elastic crack growth in finite elements with minimal remeshing10.1002/(SICI)1097-0207(19990620)45:5<601::AID-NME598>3.0.CO;2-S ↗
18. A finite element method for crack growth without remeshing10.1002/(SICI)1097-0207(19990910)46:1<131::AID-NME726>3.0.CO;2-J ↗
19. Yielding of steel sheets containing slits10.1016/0022-5096(60)90013-2 ↗
20. The mathematical theory of equilibrium cracks in brittle fracture10.1016/S0065-2156(08)70121-2 ↗
21. Numerical experiments in revisited brittle fracture10.1016/S0022-5096(99)00028-9 ↗
22. The variational approach to fracture10.1007/s10659-007-9107-3 ↗
23. Predicting effective fracture toughness of ZrB2-based ultra-high temperatures ceramics by phase-field modeling
24. Characterization and modeling of tensile properties of continuous fiber reinforced C/C-SiC composite at high temperatures10.1016/j.jeurceramsoc.2020.09.043 ↗
25. Thermal-mechanical behavior of a SiC/SiC CMC subjected to laser heating10.1016/j.compstruct.2018.11.046 ↗
26. Mechanical and oxidation properties of C/SiC corrugated lattice core composite sandwich panels10.1016/j.compstruct.2016.09.034 ↗
27. High-temperature flexural strength of I-CVI processed Cf/SiC composites with variable interphases10.1016/j.jeurceramsoc.2020.08.075 ↗
28. Construction of continuous heat conductive channel, a double harvest strategy to enhance thermal conductance and bending strength of C/SiC composites10.1016/j.jmst.2021.06.063 ↗
29. Interlaminar shear behaviors of 2D needled C/SiC composites under compressive and tensile loading10.1016/j.ceramint.2020.10.071 ↗
30. The dynamic tensile properties of 2D-C/SiC composites at elevated temperatures10.1016/j.ijimpeng.2014.10.006 ↗
31. Tensile properties of 2D-C/SiC composites at temperatures up to 1873 K at wide-ranging strain rates10.1016/j.compstruct.2023.117110 ↗
32. Comparison of cyclic fatigue behavior between C/SiC and SiC/SiC ceramic-matrix composites at elevated temperatures using hysteresis dissipated energy10.1016/j.compstruct.2016.05.006 ↗
33. Tensile properties of two-dimensional carbon fiber reinforced silicon carbide composites at temperatures up to 2300 ℃10.1016/j.jeurceramsoc.2019.10.030 ↗
34. Interlaminar shear damage mechanisms of a 2D-C/SiC composite at elevated temperature in vacuum10.1016/j.vacuum.2014.02.017 ↗
35. Internal damage evolution investigation of C/SiC composites using in-situ tensile X-ray computed tomography testing and digital volume correlation at 1000 ℃10.1016/j.compositesa.2022.107247 ↗
36. ASTM E399-23. Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness of Metallic Materials. West Conshohocken, PA: ASTM International; 2023.
37. Fabrication and properties of 3-D Cf/ZrB2–ZrC–SiC composites via polymer infiltration and pyrolysis10.1016/j.ceramint.2012.11.074 ↗
38. ASTM C1341-13. Standard Test Method for Flexural Properties of Continuous Fiber-Reinforced Advanced Ceramic Composites. West Conshohocken, PA: ASTM International; 2018.
39. Transverse and longitudinal coefficient of thermal expansion of carbon fibers at high temperatures (300–2500 K)10.1016/j.carbon.2008.07.035 ↗
40. Tensile behavior of 2D-C/SiC composites at elevated temperatures: Experiment and modeling10.1016/j.jeurceramsoc.2016.11.011 ↗
41. Modeling matrix multi-fracture in SiC/SiC ceramic-matrix composites at elevated temperatures10.1007/s41779-019-00326-6 ↗
42. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
43. Thermomechanical properties of carbon fibres at high temperatures (up to 2000 ℃)10.1016/S0266-3538(01)00140-3 ↗
44. Experimental description of thermomechanical properties of carbon fiber-reinforced TiC matrix composites10.1016/S0261-3069(03)00124-9 ↗
45. Temperature dependence of fracture effects in self-bonded SiC10.1007/PL00020375 ↗
46. Enhancing both strength and toughness of carbon/carbon composites by heat-treated interface modification10.1016/j.jmst.2018.09.055 ↗
47. Influence of graphitization temperature on microstructure and mechanical property of C/C-SiC composites with highly textured pyrolytic carbon10.1016/j.jeurceramsoc.2021.12.046 ↗
48. Thermal residual stresses in ceramic matrix composites—I. Axisymmetrical model and finite element analysis10.1016/0956-7151(94)00429-3 ↗
49. In situ stable crack growth at the micron scale10.1038/s41467-017-00139-w ↗
50. Tensile properties of ultrahigh strength PAN-based, ultrahigh modulus pitch-based and high ductility pitch-based carbon fibers10.1016/j.carbon.2007.11.001 ↗
51. Experimental and numerical investigation on SiC coating delamination from C/SiC composites10.1016/j.compscitech.2015.02.012 ↗
52. The performance transition of C/SiC composites induced by redistribution of residual stress10.1016/j.carbon.2023.118782 ↗
53. Collaborative multiscale phase-field model for trans-scale fracture propagation of fiber-reinforced composites10.1016/j.jmps.2024.105686 ↗
54. Finite element-based phase-field simulation of interfacial damage in unidirectional composite under transverse tension10.1088/1361-651X/ab1f63 ↗
55. Davidge RW. Chapter 13 - The Mechanical Properties and Fracture Behaviour of Ceramic-Matrix Composites (CMC) Reinforced With Continuous Fibres. Composite Materials Series 1989;6:547–569.10.1016/B978-0-444-87286-9.50017-6 ↗
56. Influence of the carbonization temperature on the mechanical properties of thermoplastic polymer derived C/C-SiC composites10.1016/j.jeurceramsoc.2016.09.005 ↗
57. α-Silicon carbide/β-silicon carbide particulate composites via polymer infiltration and pyrolysis (PIP) processing using polymethylsilane10.1016/S0955-2219(99)00177-6 ↗
58. Effect of SiC coating and heat treatment on the thermal radiation properties of C/SiC composites10.1016/j.jeurceramsoc.2013.12.012 ↗
59. Laser ablation behavior and mechanism of Cf/C-SiC composites under different laser energy densities10.1016/j.compositesb.2024.111359 ↗
60. Mechanical properties of chemically vapor deposited nonoxide ceramics