Zn-doped CuAlS2 transparent p-type conductive thin films deposited by pulsed plasma deposition
Source abstract
Abstract
CuAl 0.90 Zn 0.10 S 2 thin films were deposited by pulsed plasma deposition. The dependence of structural, surface morphology, electrical, and optical properties of the films on substrate temperature was investigated. X-ray diffraction patterns reveal that the film be amorphous structure. The electrical properties are sensitive to the substrate temperature. A typical sample with conductivity of 50.9 S cm−1, carrier mobility of 3.13 cm2 V−1 s−1, carrier concentration of 1.41×1019 cm−3, and average transmission of 74% in visible range of 400–700 nm was obtained. A transparent p-CuAlS2:Zn/n-In2O3:W heterogeneous diode was also fabricated and exhibits rectifying current-voltage characteristics. The ratio of forward current to the reverse current exceeds 80 within the range of applied voltages of −3.0–+3.0 V and the turn-on voltage is approximately 0.5–0.8 V.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Copper-based nanomaterials and applications · ZnO doping and properties · Chalcogenide Semiconductor Thin Films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Fudan University Department of Materials Science, , 220 Han-Dan Road, Shanghai 200433, People’s Republic of China
References (25)
Show source-provided references
1. Prog. Cryst. Growth Charact. Mater. · 2005 · 50 · 5210.1016/j.pcrysgrow.2005.10.001 ↗
2. Nature (London) · 1997 · 389 · 93910.1038/40087 ↗
3. J. Appl. Phys. · 2001 · 89 · 802210.1063/1.1372636 ↗
4. J. Appl. Phys. · 2001 · 89 · 179010.1063/1.1337587 ↗
5. Appl. Phys. Lett. · 2001 · 78 · 158310.1063/1.1355673 ↗
6. Appl. Phys. Lett. · 2000 · 77 · 132510.1063/1.1289906 ↗
7. Chem. Mater. · 2004 · 16 · 562310.1021/cm048982k ↗
8. Appl. Phys. Lett. · 2007 · 91 · 09212310.1063/1.2778755 ↗
9. Appl. Phys. Lett. · 1998 · 73 · 22010.1063/1.121761 ↗
10. Appl. Phys. Lett. · 2000 · 77 · 270110.1063/1.1319507 ↗
11. Appl. Phys. Lett. · 2004 · 84 · 87910.1063/1.1646221 ↗
12. Thin Solid Films · 1993 · 236 · 2710.1016/0040-6090(93)90636-4 ↗
13. Physica B · 2001 · 302–303 · 14010.1016/S0921-4526(01)00419-7 ↗
14. Appl. Phys. Lett. · 2004 · 84 · 54110.1063/1.1644331 ↗
15. Appl. Phys. Lett. · 2004 · 85 · 313410.1063/1.1803935 ↗
16. Appl. Phys. Lett. · 2002 · 80 · 439310.1063/1.1485133 ↗
17. Scr. Mater. · 2007 · 57 · 113310.1016/j.scriptamat.2007.08.015 ↗
18. Appl. Phys. Lett. · 2007 · 90 · 07210910.1063/1.2591415 ↗
19. J. Vac. Sci. Technol. A · 2005 · 23 · 135010.1116/1.1991871 ↗
20. Surf. Coat. Technol. · 1995 · 74–75 · 58010.1016/0257-8972(95)08308-1 ↗
21. J. Appl. Phys. · 1999 · 86 · 712910.1063/1.371802 ↗
22. JCPDS Card No. 75-0100.
23. Phys. Rev. · 1954 · 93 · 63210.1103/PhysRev.93.632 ↗
24. J. Vac. Sci. Technol. A · 2006 · 24 · 186610.1116/1.2333572 ↗
25. Semicond. Sci. Technol. · 2007 · 22 · 90010.1088/0268-1242/22/8/013 ↗