Study of some parameters responsible for the efficiency of hindered amine light stabilizers
Source abstract
Abstract
Abstract The photooxidation of a styrene‐butadiene‐styrene block copolymer previously hydroperoxidized by reaction with singlet oxygen has been studied by measuring the increase of the carbonyl absorbance at 1720 cm −1 . Five different hindered amine light stabilizers (HALS) have been introduced into the polymer by diffusion from methanolic solutions, and their efficiencies as inhibitors of the photooxidation have been compared. The sequence of efficiency observed is: tert. amine > sec. amine > amino ether Under the experimental conditions used HALS are localized preferentially in oxidized regions of the polymer, and their efficiency can be correlated with their ability to catalyze the decomposition of clustered hydroperoxides. As a consequence, HALS are oxidized to nitroxy radicals that are the actual inhibitors of the photooxidation. A high local concentration of HALS in oxidized regions of the polymer also contributes to their efficiency, and this effect justifies the observation that some tertiary amines are more efficient than others.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Polymer Synthesis and Characterization · Photopolymerization techniques and applications · Water Quality Monitoring and Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. 10.1002/pol.1982.17020023110.1002/pol.1982.170200231 ↗
2. 10.1016/0141-3910(88)90014-610.1016/0141-3910(88)90014-6 ↗
3. 10.1016/0141-3910(93)90099-510.1016/0141-3910(93)90099-5 ↗
4. 10.1016/0141-3910(93)90208-Z10.1016/0141-3910(93)90208-Z ↗
5. 10.1002/masy.1989027010510.1002/masy.19890270105 ↗
6. 10.1002/bscb.1990099112710.1002/bscb.19900991127 ↗
7. 10.1080/0091403940802854710.1080/00914039408028547 ↗
8. 10.1080/0091403920803540610.1080/00914039208035406 ↗
9. Gratten D. W. · Polym. Degrad. Stab. · 1979 · 1 · 85
10. 10.1016/0141-3910(87)90037-110.1016/0141-3910(87)90037-1 ↗
11. Geuskens G. · Polym. Degrad. Stab. · 1996 · 51 · 277
12. 10.1016/0014-3057(91)90026-K10.1016/0014-3057(91)90026-K ↗
13. 10.1016/0014-3057(93)90104-N10.1016/0014-3057(93)90104-N ↗
14. 10.1021/ma60012a00710.1021/ma60012a007 ↗
15. 10.1021/ja01878a07010.1021/ja01878a070 ↗
16. Crank J. · 1975 · 238
17. Naylor T. D. · 1989
18. 10.1016/0141-3910(95)00085-Z10.1016/0141-3910(95)00085-Z ↗
19. 10.1021/ja01571a06810.1021/ja01571a068 ↗
20. Hiatt R. · 1971
21. 10.1016/0141-3910(90)90097-Q10.1016/0141-3910(90)90097-Q ↗
22. 10.1021/ma00087a02210.1021/ma00087a022 ↗