Abstract

Abstract The role of low‐melting sulfate glasses (LMSG) as additives on the flame retardant and smoke suppressant properties of semirigid poly(vinyl chloride) (PVC), as well as the mechanism for flame retardancy and smoke suppression, were studied through the Limiting Oxygen Index (LOI) test. Smoke Density Rating (SDR) test, DTA‐TG, and SEM. The results show that the LMSG have good smoke suppressant properties. When the PVC compound contains 40 parts of LMSG, the SDR value will be reduced by about 45%. The Cu 2+ , Zn 2+ , Mn 2+ , and Ni 2+ sulfates, as well as MoO 3 , cause PVC to crosslink and form char, and the melt can protect not only the char formed during combustion and thermal degradation, but also undecomposed polymer. That is the main mechanism for flame retardation and smoke suppression when the additives melt. The mechanical properties of the PVC compounds containing different levels of LMSG were also studied.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Flame retardant materials and properties · Polymer Science and PVC · Synthesis and properties of polymers

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Paul Y. · Plast. Eng. · 1997 · 11 · 61
2. Hookanson S. H. · Wire J. Int. · 1982 · 8 · 74
3. 10.1002/ijch.19820005410.1002/ijch.198200054 ↗
4. 10.1016/0014-3057(83)90099-X10.1016/0014-3057(83)90099-X ↗
5. 10.1016/S0040-6031(00)00524-410.1016/S0040-6031(00)00524-4 ↗
6. 10.1016/0141-3910(86)90035-210.1016/0141-3910(86)90035-2 ↗
7. Kelwin S. K. · Recent Adv. Flame Retard. Polym. Mater. · 1995 · 6 · 239
8. S. K.Kelwin Proc. Int. Conf. Fire Saf. 224(1996).
9. Bin L. · Chin. Sci. Bull. · 1998 · 43 · 1094
10. 10.1016/0165-2370(85)80023-110.1016/0165-2370(85)80023-1 ↗
11. Nelson E. D. · J. Fire Flammability · 1982 · 13 · 79
12. Paul A. C. · Polym. Degrad. Stab. · 1986 · 4 · 307
13. Lum R. M. · Org. Coat. Plast. Chem. · 1980 · 43 · 176
14. 10.1021/ma60071a00110.1021/ma60071a001 ↗
15. 10.1002/app.1981.07026041210.1002/app.1981.070260412 ↗
16. 10.1007/BF0055324110.1007/BF00553241 ↗
17. 10.1002/app.1992.07046031410.1002/app.1992.070460314 ↗
18. 10.1111/j.1151-2916.1965.tb14658.x10.1111/j.1151-2916.1965.tb14658.x ↗
19. Kirk O. · 1986
20. Steven R. G. · Wire J. Int. · 2000 · 4 · 215
21. R. P.LattimerandW. J.Kroenke Anal. Pyrol. 453(1984).10.1016/B978-0-408-01417-5.50019-6 ↗
22. 10.1016/0014-3057(86)90205-310.1016/0014-3057(86)90205-3 ↗
23. 10.1016/0141-3910(92)90133-P10.1016/0141-3910(92)90133-P ↗
24. Khan M. S. · J. Chem. Soc. Pak. · 1997 · 19 · 8
25. 10.1016/0141-3910(95)00209-X10.1016/0141-3910(95)00209-X ↗
26. 10.1002/pol.1969.16007101210.1002/pol.1969.160071012 ↗
27. Troitzsch J. H. · Prog. Org. Coat. · 1983 · 41 · 69
28. Fred M. W. · Polym. Sci. · 1984 · 26 · 215
29. 10.1007/978-1-4615-1761-010.1007/978-1-4615-1761-0 ↗