Bending strength and internal bond strength of wood-based boards subjected to various exposure conditions
Source abstract
Abstract
Phenol–formaldehyde resin-bonded particleboard (PF board), methylene diphenyl diisocyanate resin-bonded particleboard (MDI board), aspen oriented strand board (aspen board), Scots pine oriented strand board (pine board), methylene diphenyl diisocyanate resin-bonded medium-density fiberboard (F-MDI board), and melamine–urea–formaldehyde resin-bonded medium-density fiberboard (F-MUF board)—six board types overall—were subjected to high relative humidity (90 %, 20 °C) or cyclic humidity of high/low relative humidity (90/45 %, 20 °C) for 5 years. The PF board and aspen board showed reduction in bending strength [modulus of rupture (MOR)] and internal bond strength (IB); however, the MDI board, pine board, F-MDI board, and F-MUF board showed almost no reduction. Furthermore, the boards were subjected to outdoor exposure and Test B (boiling for 2 h) from the Japanese Industrial Standard (JIS); the results showed large reduction in the MOR and IB of the PF board and aspen board. In contrast, outdoor exposure did not greatly reduce the MOR and IB of the F-MUF board and F-MDI board. Although the IB of the F-MUF board reduced after the JIS Test B because of using low-durability resin, the IB retention was as high as 87.8 % for 5-year outdoor exposure.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Postharvest Quality and Shelf Life Management
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Okkonen EA, River BH (1996) Outdoor aging of wood-based panels and correlation with laboratory aging: part 2. Forest Prod J 46(3):68–74
2. River BH (1994) Outdoor aging of wood-based panels and correlation with laboratory aging. Forest Prod J 44(11/12):55–65
3. Hann RA, Black JM, Blomquist RF (1962) How durable is particleboard. Forest Prod J 12:577–584
4. Suzuki S (2001) Evaluation of wood-based panel durability (in Japanese). Wood Ind 56:7–12
5. Korai H, Sekino N, Saotome H (2012) Effects of outdoor exposure angle on the deterioration of wood-based board properties. Forest Prod J 62:184–19010.13073/0015-7473-62.3.184 ↗
6. Korai H (2012) Durability of medium density fiberboard subjected to outdoor exposure (in Japanese). Mokuzai Gakkaishi 58:347–35610.2488/jwrs.58.347 ↗
7. Korai H, Adachi K, Saotome H (2013) Deterioration of wood-based boards subjected to outdoor exposure in Tsukuba. J Wood Sci 59:24–3410.1007/s10086-012-1291-5 ↗
8. Korai H, Hattori K (2013) Effects of surface coating on durability improvement of particleboard subjected to outdoor exposure (in Japanese). Mokuzai Gakkaishi 59:361–36610.2488/jwrs.59.361 ↗
9. Korai H, Saotome H, Ohmi M (2014) Effects of water soaking and outdoor exposure on modulus of rupture and internal bond strength of particleboard. J Wood Sci 60:127–13310.1007/s10086-013-1374-y ↗
10. Korai H, Saotome H (2014) Effects of water soaking and outdoor exposure on nail joint properties of particleboard. J Wood Sci 60:134–14010.1007/s10086-013-1375-x ↗
11. Korai H, Watanabe K, Nogami H, Fukino M, Fujimoto Y (2014) Simple and useful index for analyzing particleboard subjected to outdoor exposure. J Adhes Soc Jpn 50:260–26710.11618/adhesion.50.260 ↗
12. Korai H, Watanabe K (2014) Effectiveness of principal component analysis for analyzing particleboard subjected to outdoor exposure. J Wood Sci 61:151–158
13. Kojima Y, Norita H, Suzuki S (2009) Evaluating the durability of wood-based panels using thickness swelling results from accelerated aging treatments. Forest Prod J 59(5):35–41
14. Kojima Y, Suzuki S (2011) Evaluating the durability of wood-based panels using internal bonding strength results from accelerated aging treatments. J Wood Sci 57:7–1310.1007/s10086-010-1131-4 ↗
15. Kojima Y, Suzuki S (2011) Evaluating the durability of wood-based panels using bending properties after accelerated aging treatments. J Wood Sci 57:126–13310.1007/s10086-010-1146-x ↗
16. Kojima Y, Shimoda T, Suzuki S (2012) Modified method for evaluating weathering intensity using outdoor exposure tests on wood-based panels. J Wood Sci 58:525–53110.1007/s10086-012-1287-1 ↗
17. Sekino N, Sato H, Adachi K (2014) Evaluation of particleboard deterioration under outdoor exposure using several different types of weathering intensity. J Wood Sci 60:141–15110.1007/s10086-013-1384-9 ↗
18. Sekino N, Okuma M (1985) Performance over time of construction particleboard I. Fatigue behavior in bending (in Japanese). Mokuzai Gakkaishi 31:801–806
19. Sekino N, Okuma M (1986) Performance of construction particleboard II. Bending in service as underlayment of flowers (in Japanese). Mokuzai Gakkaishi 32:163–169
20. Wu Q, Lee JN (2002) Thickness swelling of oriented strandboard under long-term cyclic humidity exposure condition. Wood Fiber Sci 34:125–139
21. JIS A 5908 (2003) JIS standard specification for particleboard. Japanese Standards Association, Tokyo
22. JIS A 5905 (2003) JIS standard specification for fiberboard. Japanese Standards Association, Tokyo
23. Korai H (2012) Improvement of acetylated fiberboard by ozonization (in Japanese). J Adhes Soc Japan 48:30–3510.11618/adhesion.48.30 ↗
24. The Timber Research and Development Association (TRADA) (1980) Timbers of the world. The Construction Press, Bath, pp 182–183
25. The Timber Research and Development Association (TRADA) (1980) Timbers of the world. The Construction Press, Bath, pp 133–134
26. Kawai S, Suda H, Sasaki H (1987) Production technology for low-density particleboard IV. Effects of particle density and compaction ratio on board properties (in Japanese). Mokuzai Gakkaishi 33:385–392
27. Ikeda M, Suzuki S (1999) Evaluation of the durability performance of wood-based panels subjected to outdoor exposure. Bulletin of the Shizuoka University Forests No: 23, pp 25–35