journal article·2022-12Open access

Studies on pre-treatment by compression for wood impregnation III: effects of the solid content of low-molecular-weight phenol formaldehyde resin on the impregnation

Huifang Wang, Youke Zhao

Journal of Wood Science· Volume 68· Issue 1

Abstract

Abstract There is increasing interests in the significant improvement of impregnation amount and efficiency in wood by the pre-treatment of compression. Thus, attention is paid to pre-treatment by compression for harder impregnation with resin because of the large viscosity and relatively large molecular weight of the resin. Low-molecular-weight phenol formaldehyde (PF) resin of solid content of 10–48% were impregnated by pre-treatment of compression at a compression ratio of 60% and 40% for poplar and Chinese fir, respectively, to systematically study the effects of solid content on the impregnation amount, weight gain percentage (WGP). In addition, the distribution of resin in wood was analyzed by profile density and was observed by confocal laser scanning microscope (CLSM), and the change of crystallinity index (CrI) of resin-impregnated wood was investigated by X-ray diffractometer. The results showed: (1) compared with immersion impregnation without compression, the impregnation by pre-treatment of compression, was much larger in amount and higher in efficiency for resins in all solid contents. In a solid content range of 10–48% and at a molecular weight of about 517, there was no significant difference of impregnation amount by compression among the resins at different solid content. (2) The WGP of poplar and Chinese fir increased with the increase of resin solid content. When the resin solid content increased from 10 to 48%, the WGP increased from 8.9 to 44.2% and from 5.2 to 24.9% for poplar and Chinese fir, respectively. (3) Resin is mainly distributed in vessels and tracheids despite a few being distributed in the fiber near the longitudinal end of the poplar specimens. With the increase of solid content, the resin distribution gradually changed from diffusing on the wall to depositing in the vessel or tracheid, while the resin distribution evenness along the longitudinal direction decreased. There was more resin deposited near the longitudinal end of Chinese fir at deeper depth than that of poplar. (4) The resin can be impregnated into the amorphous area of wood without causing any change in the crystallization area. The CrI decreases with the increase of resin solid content. After all, it is concluded that the pre-treatment by compression for wood impregnation with low-molecular-weight PF resin is effective for all the solid contents for both poplar and Chinese fir. The WGP increased with the increase of resin solid content, despite the decrease of evenness of resin distribution at high solid content.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Bamboo properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Xie Y, Fu Q, Wang Q, Xiao Z, Militz H (2013) Effects of chemical modification on the mechanical properties of wood. Eur J Wood Wood Prod 71:401–41610.1007/s00107-013-0693-4 ↗
2. Zhao Y, Wang Z, Iida I, Huang R, Lu J, Jiang J (2015) Studies on pre-treatment by compression for wood drying I: effects of compression ratio, compression direction and compression speed on the reduction of moisture content in wood. J Wood Sci 61:113–11910.1007/s10086-014-1451-x ↗
3. Zhao Y, Wang Z, Iida I, Huang R, Lu J, Jiang J (2016) Studies on pre-treatment by compression for wood drying II: effects of compression ratio, compression direction and compression speed on the recovery rate and mechanical properties of wood. J Wood Sci 62:226–23210.1007/s10086-016-1552-9 ↗
4. Zhao Y (2017) Studies on pre-treatment by compression for wood drying III: the reduction of moisture content, the recovery rate, and mechanical properties of wood compressed at different moisture content conditions. J Wood Sci 63:209–21510.1007/s10086-017-1612-9 ↗
5. Zhao Y, Wang Z, Iida I, Guo J (2018) Studies on pre-treatment by compression for wood impregnation I: effects of compression ratio, compression direction, compression speed and compression-unloading place on the liquid impregnation of wood. J Wood Sci 64:551–55610.1007/s10086-018-1735-7 ↗
6. Zhao Y, Zhao X, Iida I, Guo J (2019) Studies on pre-treatment by compression for wood impregnation II: the impregnation of wood compressed at different moisture content conditions. J Wood Sci 65:2810.1186/s10086-019-1808-2 ↗
7. Iida I, Yusuf S, Watanabe U, Imamura Y (2002) Liquid penetration of precompressed wood VII: combined treatment of precompression and extraction in hot water on the liquid penetration of wood. J Wood Sci 48:81–8510.1007/BF00766243 ↗
8. Iida I, Takayama C, Miyagawa O, Imamura Y (1992) Liquid penetration of precompressed wood, 1: effects of compressive deformation and recovery upon liquid uptake. J Japan Wood Res Soc 38:233–240
9. Wu Y, Matsui H (2003) Study on the impregnation of phenol resin in Chinese Fir and its improvement. Sci Silvae Sin 39:136–140
10. Luo J, Zhao Y, Guo J, Wang H (2021) Impregnating low-molecular-weight phenol formaldehyde resin into Chinese fir wood under different compression ratio. J Northwest Agric For Univ 49:50–58 (in Chinese)
11. Wang X, Chen X, Xie X, Yuan Z, Cai S (2019) Effect of phenol formaldehyde resin penetration on the quasi-static and dynamic mechanics of wood cell walls using nanoindentation. Nanomaterials (Basel) 9:140910.3390/nano9101409 ↗
12. Wang X, Chen X, Xie X, Cai S, Yuan Z, Li Y (2019) Multi-scale evaluation of the effect of phenol formaldehyde resin impregnation on the dimensional stability and mechanical properties of pinus massoniana lamb. Forests 10:64610.3390/f10080646 ↗
13. Pizzi A (2015) Synthetic adhesives for wood panels chemistry and technology. In: Mittal KL (ed) Progress in adhesion and adhesives. Wiley, Hoboken
14. Yusof N, Tahir P, Seng H, Khan M, James R (2019) Mechanical and physical properties of cross-laminated timber made from Acacia mangium wood as function of adhesive types. J Wood Sci 65:2010.1186/s10086-019-1799-z ↗
15. SandBeRg D, Kutnar A, Mantanis G (2017) Wood modification technologies—a review. iForest 10:895–90810.3832/ifor2380-010 ↗
16. Yue K, Chen Z, Lu W, Liu W, Li M, Shao Y, Tang L, Wan L (2017) Evaluating the mechanical and fire-resistance properties of modified fast-growing Chinese fir timber with boric–phenol–formaldehyde resin. Constr Build Mater 154:956–96210.1016/j.conbuildmat.2017.08.035 ↗
17. Khalil H, Amouzgar P, Jawaid M, Abdullah C, Issam A, Zainudin E, Paridah M, Hassan A (2013) Physical and thermal properties of microwave-dried wood lumber impregnated with phenol formaldehyde resin. J Compos Mater 47:3565–357110.1177/0021998312467386 ↗
18. Huang Y, Fei B, Zhao R (2014) Investigation of low-molecular weight phenol formaldehyde distribution in tracheid cell walls of Chinese fir wood. BioResources 9:4150–4158
19. Johnson S, Kamke F (1992) Quantitative analysis of gross adhesive penetration in wood using fluorescence microscopy. Adhesion 40:47–6110.1080/00218469208030470 ↗
20. Yuan J, Hu Y, Li L, Cheng F (2013) The mechanical strength change of wood modified with DMDHEU. BioResources 8:1076–1088
21. Segal LC, Creely JJ, Martin AE, Conrad CM (1959) An empirical method for estimating the degree of crystallinity of native cellulose using the X-ray diffractometer. Text Res J 29:786–79410.1177/004051755902901003 ↗
22. Siau JF (1995) Wood: influence of moisture on physical properties. Department of Wood Science and Forest Products, Virginia Polytechnic Institute and State University, Blacksburg
23. Watanabe U, Imamura Y, Iida I (1998) Liquid penetration of precompressed wood VI: anatomical characterization of pit fractures. J Wood Sci 44:158–16210.1007/BF00526263 ↗
24. Bao F, Lu J, Avramidis S (1999) On the permeability of main wood species in China. Holzforschung 53:350–35410.1515/HF.1999.058 ↗
25. Hansmann C, Gindl W, Wimmer R, Teischinger A (2002) Permeability of wood—a review. Drev Vysk Res 47:1–16
26. Furuno T, Imamura Y, Kajita H (2004) The modification of wood by treatment with low molecular weight phenol-formaldehyde resin: a properties enhancement with neutralized phenolic-resin and resin penetration into wood cell walls. Wood Sci Technol 37:349–36110.1007/s00226-003-0176-6 ↗
27. Wan H, Kim MG (2008) Distribution of phenol–formaldehyde resin in impregnated southern pine and effects on stabilization. Wood Fiber Sci 40:181–189
28. Cai M, Fu Z, Cai Y, Li Z, Xu G, Xu C, Li S (2018) Effect of impregnation with maltodextrin and 1,3-dimethylol-4,5-dihydroxyethyleneurea on poplar wood. Forests 9:67610.3390/f9110676 ↗
29. So S, Teh JW, Rudin A et al (1990) Effects of resole phenol adhesives on the crystallinity of cellulose. J Appl Polym Sci 39:531–53810.1002/app.1990.070390304 ↗
30. Wada M, Okano T, Sugiyama J (2001) Allomorphs of native crystalline cellulose I evaluated by two equatorial d-spacings. J Wood Sci 47:124–12810.1007/BF00780560 ↗