Evaluating dimensional stability in solid wood: a review of current practice
Source abstract
Abstract
The degree with which wood shrinks and swells with changing moisture content is an important property which determines its suitability for different applications. This property, known as dimensional stability, is often a target property for improvement in wood modification research. Its importance makes it a commonly quantified wood property. Despite this, methods for measuring dimensional stability are not standardised, and there is little consensus on appropriate test methods. Dimensional stability tests can be classified according to the method used to change the moisture content of the wood (liquid water or water vapour) and the duration of the test (until equilibrium is reached, or a shorter duration). Each class of test represents a situation that wood products may encounter in service, and different types of wood (modified or otherwise) may respond differently to each situation. This means that comparative performance between different wood types may be dependent on the test used (and may not be valid for some situations encountered in service). In this paper, standard test methods and methods described in the literature are compared, and recommendations are given for selecting an appropriate dimensional stability test and for minimising sources of bias and measurement uncertainty in the test. It is expected that this will also encourage the adoption of more standardised test methods, enabling comparisons to be made between different studies and different wood types.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Tree Root and Stability Studies · Bamboo properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Van Acker J (2003) Assessing performance potential of modified wood focussing on dimensional stability and biological durability. Paper presented at the First European Conference on Wood Modification, 3–4 April 2003, Ghent, Belgium
2. Sargent R, Durbin GJ, Dunningham EA (2015) Measurement of dimensional stability. Paper presented at the 8th European Conference on Wood Modification, 24–25th October, Helsinki, Finland
3. Hill CAS (2006) Wood modification. Chemical, thermal and other processes. Wiley, Chichester10.1002/0470021748 ↗
4. WDMA (2009) T.M. 2—1999 Test method to determine the short term anti-swell effectiveness of treating systems. The Window & Door Manufacturers Association, Chicago, IL
5. Skaar C (1988) Wood-water relations. Springer series in wood science. Springer, Berlin10.1007/978-3-642-73683-4 ↗
6. Noack D, Schwab E, Bartz A (1973) Characteristics for a judgment of the sorption and swelling behavior of wood. Wood Sci Technol 7:218–23610.1007/BF00355552 ↗
7. Bak M, Németh R (2012) Changes in swelling properties and moisture uptake rate of oil-heat-treated poplar (Populus × euramericana cv. pannónia) wood. BioResources 7:5128–513710.15376/biores.7.4.5128-5137 ↗
8. Hill CAS, Farahani MRM, Hale MDC (2004) The use of organo alkoxysilane coupling agents for wood preservation. Holzforschung 58:316–32510.1515/HF.2004.049 ↗
9. Vukusic SB, Katovic D, Grgac SF, Trajkovic J, Sefc B, Voncina B (2010) Study of the wood modification process with polycarboxylic acids and microwave tratment. Wood Res-Slovakia 55:121–130
10. Hill C, Jones D (1996) The dimensional stabilisation of corsican pine sapwood by reaction with carboxylic acid anhydrides. Holzforschung 50:457–46210.1515/hfsg.1996.50.5.457 ↗
11. Šefc B, Trajkovic J, Hasan M, Katovic D, Vukusic SB, Martina F (2009) Dimensional stability of wood modified by citric acid using different catalysts/Stabilnost dimenzija drva modificiranoga limunskom kiselinom uz razlicite katalizatore. Drvna Ind 60:23
12. Gündüz G, Korkut S, Korkut DS (2008) The effects of heat treatment on physical and technological properties and surface roughness of Camiyani Black Pine (Pinus nigra Arn. subsp. pallasiana var. pallasiana) wood. Bioresource Technol 99:2275–228010.1016/j.biortech.2007.05.015 ↗
13. Dubey MK, Pang S, Walker J (2012) Changes in chemistry, color, dimensional stability and fungal resistance of Pinus radiata D. Don wood oil heat-treatment. Holzforschung 66:49–5710.1515/HF.2011.117 ↗
14. Fredriksson M, Wadsö L, Ulvcrona T (2010) Moisture sorption and swelling of Norway spruce [Picea abies (L.) Karst.] impregnated with linseed oil. Wood Mat Sci Eng 5:135–14210.1080/17480272.2010.484102 ↗
15. Ohmae K, Minato K, Norimoto M (2002) The analysis of dimensional changes due to chemical treatments and water soaking for hinoki (Chamaecyparis obtusa) wood. Holzforschung 56:98–10210.1515/HF.2002.016 ↗
16. García Esteban L, Gril J, Palacios De Palacios De, Guindeo Casasús A (2005) Reduction of wood hygroscopicity and associated dimensional response by repeated humidity cycles. Ann For Sci 62:275–284. https://doi.org/10.1051/forest:200502010.1051/forest:2005020 ↗
17. Almeida G, Hernández RE (2007) Dimensional changes of beech wood resulting from three different re-wetting treatments. Holz Roh Werkst 65:193–19610.1007/s00107-006-0151-7 ↗
18. Naderi N, Hernández RE (1997) Effect of re-wetting treatment on the dimensional changes of sugar maple wood. Wood Fiber Sci 29:340–344
19. Rowell R (1983) Chemical modification of wood. For Prod Abstr 6:363–382
20. Čermák P, Rautkari L, Horáček P, Saake B, Rademacher P, Sablík P (2015) Analysis of dimensional stability of thermally modified wood affected by re-wetting cycles. BioResources 10:3242–3253. https://doi.org/10.15376/biores.10.2.3242-325310.15376/biores.10.2.3242-3253 ↗
21. Chafe SC (1995) Preheating and continous and intermittent drying in boards of Eucalyptus-regnans f muell. 1. Effect on internal checking, shrinkage and collapse. Holzforschung 49:227–233. https://doi.org/10.1515/hfsg.1995.49.3.22710.1515/hfsg.1995.49.3.227 ↗
22. DIN 52 184 (1979) Testing of wood; determination of swelling and shrinkage
23. ASTM D2395 (2014) Standard test methods for density and specific gravity (relative density) of wood and wood-based materials
24. Schmidt EL, Murphy TP, Cheeks CN, Ross AS, Chiu TS, Williams RS (2002) Comparisons of interlaboratory swellometer testing of two water-repellent preservative formulations for millwork. For Prod J 52:82–84
25. Khalil HPSA, Amouzgar P, Jawaid M, Abdullah CK, Issam AM, Zainudin ES, Paridah MT, Hassan A (2013) Physical and thermal properties of microwave-dried wood lumber impregnated with phenol formaldehyde resin. J Compos Mater 47:3565–3571. https://doi.org/10.1177/002199831246738610.1177/0021998312467386 ↗
26. ASTM D4446 M (2013) Anti-swelling effectiveness of water-repellent formulations and differential swelling of untreated wood when exposed to liquid water environments
27. Anonymous (2010) Wood Handbook—wood as and engineering material. General technical report FPL-GTR-190. U.S. Department of Agriculture, Forest Service, Forest Products Laboratory, Madison, WI
28. ISO 4469 (1981) Wood—determination of radial and tangential shrinkage
29. Bekhta P, Niemz P (2003) Effect of high temperature on the change in color, dimensional stability and mechanical properties of spruce wood. Holzforschung 57:539–54610.1515/HF.2003.080 ↗
30. Mazzanti P, Togni M, Uzielli L (2012) Drying shrinkage and mechanical properties of poplar wood (Populus alba L.) across the grain. J Cult Herit 13:S85–S8910.1016/j.culher.2012.03.015 ↗
31. Lande S, Westin M, Schneider M (2004) Properties of furfurylated wood. Scand J For Res 19(Supplement 5):22–3010.1080/0282758041001915 ↗
32. Esteves BM, Pereira HM (2009) Wood modification by heat treatment: a review. BioResources 4:370–40410.15376/biores.4.1.370-404 ↗
33. Awoyemi L (2004) Effects of microwave modification on the shrinkage properties of Eucalyptus obliqua wood. J I Wood Sci 16:199–203
34. Sik HS, Choo KT, Zakaria S, Ahmad S, How SS, Chia CH, Yusoff M (2010) Dimensional stability of high temperature-dried rubberwood solid lumber at two equilibrium moisture content conditions. Dry Technol 28:1083–109010.1080/07373937.2010.506162 ↗
35. Rautkari L, Hill CAS (2014) Effect of initial moisture content on the anti-swelling efficiency of thermally modified Scots pine sapwood treated in a high-pressure reactor under saturated steam. Holzforschung 68:323–32610.1515/hf-2013-0078 ↗
36. Hoffmeyer P, Engelund ET, Thygesen LG (2011) Equilibrium moisture content (EMC) in Norway spruce during the first and second desorptions. Holzforschung 65:875–88210.1515/HF.2011.112 ↗
37. Weise U, Paulapuro H (1998) Relation between fiber shrinkage and hornification. Prog Pap Recycl 7:14–21
38. Östlund Å, Köhnke T, Nordstierna L, Nydén M (2010) NMR cryoporometry to study the fiber wall structure and the effect of drying. Cellulose 17:321–32810.1007/s10570-009-9383-0 ↗
39. Pönni R, Vuorinen T, Kontturi E (2012) Proposed nano-scale coalescence of cellulose in chemical pulp fibers during technical treatments. BioResources 7:6077–610810.15376/biores.7.4.6077-6108 ↗
40. Hill CAS, Ramsay J, Laine K, Rautkari L, Hughes M (2013) Water vapour sorption behaviour of thermally modified wood. Int Wood Prod J 4:191–19610.1179/2042645313Y.0000000040 ↗
41. Rowell RM, Wang RHS, Hyatt JA (1986) Flakeboards made from aspen and southern pine wood flakes reacted with gaseous ketene. J Wood Chem and Technol 6:449–47110.1080/02773818608085237 ↗
42. Edvardsen K, Sandland KM (1999) Increased drying temperature—its influence on the dimensional stability of wood. Holz Roh Werk 57:207–20910.1007/s001070050042 ↗
43. Ding T, Gu L, Li T (2011) Influence of steam pressure on physical and mechanical properties of heat-treated Mongolian pine lumber. Eur J Wood Wood Prod 69:121–12610.1007/s00107-009-0406-1 ↗
44. Ishimaru Y, Arai K, Mizutani M, Oshima K, Iida I (2001) Physical and mechanical properties of wood after moisture conditioning. J W Sci 47:185–19110.1007/BF01171220 ↗
45. Rafidah KS, Hill CAS, Ormondroyd GA (2006) Dimensional stabilization of rubberwood (Hevea brasiliensis) with acetic or hexanoic anhydride. J Trop For Sci 18:261–268
46. BS/EN 318 (2002) Wood based panels. Determination of changes associated with changes in relative humidity
47. AS/NZS 4266.14 (2004) Reconstituted wood-based panels—methods of test
48. Barkas WW (1949) The swelling of wood under stress. Forest Products Research Laboratory; Department of Scientific and Industrial Research, London
49. Pfriem A, Grothe T, Wagenführ A (2007) Influence of thermal modification on the unsteady sorption behavior of Norway spruce (Picea abies (L.) Karst.). Holz Roh Werkst 65:321–32310.1007/s00107-006-0167-z ↗
50. Harris JM (1961) The dimensional stability shrinkage intersection point and related properties of new zealand timbers. Forest Research Institute, New Zealand Forest Service
51. Haslett AN (1986) Properties and utilisation of exotic specialty timbers grown in New Zealand