journal article·2022-12Open access

Densification of timber: a review on the process, material properties, and application

John Paul Cabral, Bidur Kafle, Mahbube Subhani, Johannes Reiner, Mahmud Ashraf

Journal of Wood Science· Volume 68· Issue 1

Abstract

Abstract Timber densification is a process that has been around since the early 1900s and is predominantly used to enhance the structural properties of timber. The process of densification provides the timber with a greater mechanical strength, hardness, abrasion resistance, and dimensional stability in comparison to its virgin counterparts. It alters the cellular structure of the timber through compression, chemical impregnation, or the combination of the two. This in turn closes the voids of the timber or fills the porosity of the cell wall structure, increasing the density of the timber and, therefore, changing its properties. Several processes are reported in literature which produce densified timber, considering the effect of various parameters, such as the compression ratio, and the temperature on the mechanical properties of the densified timber. This paper presents an overview of the current processes of timber densification and its corresponding effects. The material properties of densified timber, applications, and possible future directions are also explored, as the potential of this innovative material is still not fully realised.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Bamboo properties and applications · Lignin and Wood Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Sandberg D, Kutnar A, Mantanis G (2017) Wood modification technologies—a review. IForest 10:895–908. https://doi.org/10.3832/ifor2380-01010.3832/ifor2380-010 ↗
2. Sotayo A, Bradley D, Bather M, Sareh P, Oudjene M, El-Houjeyri I, Harte A, Mehra S, O’Ceallaigh C, Haller P, Namari S, Makradi A, Belouettar S, Bouhala L, Deneufbourg F, Guan Z (2020) Review of state of the art of dowel laminated timber members and densified wood materials as sustainable engineered wood products for construction and building applications. Develop Built Environ 1:100004. https://doi.org/10.1016/j.dibe.2019.10000410.1016/j.dibe.2019.100004 ↗
3. Kutnar A, Sernek M (2007) Densification of wood. Zbornik Gozdarstva Lesarstva 82:53–62
4. Institute A, of Timber Construction, Linville J.D. (eds) (2012) Timber construction manual, 6th edn. Wiley, New York
5. Elsener R (2014) Material characterization of timber utility poles using experimental approaches. Timber. 168:8
6. Holmberg S, Persson K, Petersson H (1999) Nonlinear mechanical behaviour and analysis of wood and fibre materials. Comput Struct 72:459–480. https://doi.org/10.1016/S0045-7949(98)00331-910.1016/S0045-7949(98)00331-9 ↗
7. Bootle KR (1983) Wood in Australia: types, properties and uses. McGraw-Hill Education, New York
8. Crews KI (2016) 12 - Nonconventional timber construction. In: Harries KA, Sharma B (eds) Nonconventional and Vernacular Construction Materials. Woodhead Publishing, pp 335–36310.1016/B978-0-08-100038-0.00012-3 ↗
9. Salmén L (2004) Micromechanical understanding of the cell-wall structure. CR Biol 327:873–880. https://doi.org/10.1016/j.crvi.2004.03.01010.1016/j.crvi.2004.03.010 ↗
10. Laine K (2014) Improving the properties of wood by surface densification. Dissertation, Aalto University
11. Fengel D, Wegener G (1983) Wood : chemistry, ultrastructure, reactions10.1515/9783110839654 ↗
12. Ramage MH, Burridge H, Busse-Wicher M, Fereday G, Reynolds T, Shah D, Wu G, Yu L, Fleming P, Densley-Tingley D, Allwood J, Dupree P, Linden PF, Scherman O (2017) The wood from the trees: The use of timber in construction. Renew Sustain Energy Rev 68:333–359. https://doi.org/10.1016/j.rser.2016.09.10710.1016/j.rser.2016.09.107 ↗
13. Winandy J, Rowell R (1984) The chemistry of wood strength. handbook of wood chemistry and wood composites, second edition. https://doi.org/10.1021/ba-1984-0207.ch00510.1021/ba-1984-0207.ch005 ↗
14. Shmulsky R, Jones PD (2019) Forest products and wood science: an introduction. Wiley, Newark10.1002/9781119426400 ↗
15. Salmén L (1982) Temperature and water induced softening behaviour of wood fiber based materials. Dissertation, The Royal Institute of Technology
16. Back E, Salmén L (1982) Glass transitions of wood components hold implications for molding and pulping processes. Tappi J 65:107110
17. Kelley SS, Rials TG, Glasser WG (1987) Relaxation behaviour of the amorphous components of wood. J Mater Sci 22:617–624. https://doi.org/10.1007/BF0116077810.1007/BF01160778 ↗
18. Lenth CA, Kamke FA (2001) Moisture dependent softening behavior of wood. Wood Fiber Sci 33:492–507
19. Kultikova EV (1999) Structure and properties relationships of densified wood. Dissertation, Virginia Tech
20. Seborg RM, Millett MA, Stamm AJ (1956) Heat-stabilized compressed wood (staypak). Forest Products Laboratory, Wisconsin
21. Seborg RM, Tarkow H, Stamm AJ (1953) Effect of heat upon the dimensional stabilization of wood. J For Products Res Soc 3(9):59–67
22. Stamm AJ, Alfred J, Seborg RM (1955) Forest products laboratory resin-treated, laminated, compressed wood (compreg). Forest Products Laboratory, Wisconsin
23. Navi P, Girardet F (2000) Effects of thermo-hydro-mechanical treatment on the structure and properties of wood. Holzforschung 54:287–293. https://doi.org/10.1515/HF.2000.04810.1515/HF.2000.048 ↗
24. Norimoto M, Ota C, Akitsu H, Yamada T (1993) Permanent fixation of bending deformation in wood by heat treatment. Wood Res 79:23–33
25. Tabarsa T, Chui YH (1997) Effects of hot-pressing on properties of white spruce. For Prod J 47:71–76
26. Dwianto W, Norirnoto M, Morooka T, Tanaka F, Inoue M, Liu Y (1998) Radial compression of sugi wood (Cryptomeria japonica D. Don). Holz als Roh- und Werkstoff 56:403–411. https://doi.org/10.1007/s00107005034210.1007/s001070050342 ↗
27. Zhou Y, Fushitani M, Sato K, Ozawa M (2000) Bending creep behavior of hot-pressed wood under cyclic moisture change conditions. J Wood Sci 46:423–430. https://doi.org/10.1007/BF0076579910.1007/BF00765799 ↗
28. Kubojima Y, Ohtani T, Yoshihara H (2004) Effect of shear deflection on vibrational properties of compressed wood. Wood Sci Technol 38:237–244. https://doi.org/10.1007/s00226-004-0237-510.1007/s00226-004-0237-5 ↗
29. Tanaka K, Demoto Y, Ouchi J, Inoue M (2010) Strength property of densified sugi adopted as material of connector. In: Proceedings of the World Conference on Timber Engineering (WCTE), Trentino, 2010
30. Anshari B, Guan ZW, Kitamori A, Jung K, Hassel I, Komatsu K (2011) Mechanical and moisture-dependent swelling properties of compressed japanese cedar. Constr Build Mater 25:1718–1725. https://doi.org/10.1016/j.conbuildmat.2010.11.09510.1016/j.conbuildmat.2010.11.095 ↗
31. Hill CAS, Ramsay J, Keating B et al (2012) The water vapour sorption properties of thermally modified and densified wood. J Mater Sci 47:3191–319710.1007/s10853-011-6154-8 ↗
32. Santos CMT, Menezzi CHD, de Souza MR (2012) Properties of thermo-mechanically treated wood from pinus caribaea var. hondurensis. BioResources 7:1850–186510.15376/biores.7.2.1850-1865 ↗
33. Kiaei M, Rad MB, Amani N (2018) Influence of densification temperature on some physical and mechanical properties of pterocarya fraxinifolia wood. Wood Industry / Drvna Industrija 69:283–287. https://doi.org/10.5552/drind.2018.175010.5552/drind.2018.1750 ↗
34. Pelit H, Yorulmaz R (2019) Influence of densification on mechanical properties of thermally pretreated spruce and poplar wood. BioResources 14:9739–9754. https://doi.org/10.15376/biores.14.4.9739-975410.15376/biores.14.4.9739-9754 ↗
35. Sözbir GD, Bektaş İ, Ak AK (2019) Influence of combined heat treatment and densification on mechanical properties of poplar wood. Maderas 21:481–492. https://doi.org/10.4067/S0718-221X201900500040510.4067/S0718-221X2019005000405 ↗
36. Inoue M, Norimoto M, Tanahashi M, Rowell RM (1993) Steam or heat fixation of compressed wood. Wood Fiber Sci 25:224–235
37. Inoue M, Sekino N, Morooka T, Rowell RM, Norimoto M (2008) Fixation of compressive deformation in wood by pre-steaming. J Trop For Sci 20:273–281
38. Heger F, Groux M, Girardet F, Welzbacher C, Rapp AO, Navi P (2004) Mechanical and durability performance of thm-densified wood. In: Final Workshop Cost Action E22: Environmental Optimization of Wood Protection, Lisboa, 2004
39. Navi P, Heger F (2004) Combined densification and thermo-hydro-mechanical processing of wood. MRS Bull 29:332–336. https://doi.org/10.1557/mrs2004.10010.1557/mrs2004.100 ↗
40. Bao M, Huang X, Jiang M, Yu W, Yu Y (2017) Effect of thermo-hydro-mechanical densification on microstructure and properties of poplar wood (populus tomentosa). J Wood Sci 63:591–605. https://doi.org/10.1007/s10086-017-1661-010.1007/s10086-017-1661-0 ↗
41. Yoshihara H, Tsunematsu S (2007) Bending and shear properties of compressed sitka spruce. Wood Sci Technol 41:117–131. https://doi.org/10.1007/s00226-006-0091-810.1007/s00226-006-0091-8 ↗
42. Fang C-H, Mariotti N, Cloutier A, Koubaa A, Blanchet P (2012) Densification of wood veneers by compression combined with heat and steam. Eur J Wood Prod 70:155–163. https://doi.org/10.1007/s00107-011-0524-410.1007/s00107-011-0524-4 ↗
43. Chen S, Obataya E, Matsuo-Ueda M (2018) Shape fixation of compressed wood by steaming: a mechanism of shape fixation by rearrangement of crystalline cellulose. Wood Sci Technol 52:1229–1241. https://doi.org/10.1007/s00226-018-1026-x10.1007/s00226-018-1026-x ↗
44. Skyba O, Schwarze F, Niemz P (2009) Physical and mechanical properties of Thermo-hygromechanically (THM) - Densified wood. Wood Research 54:1–18
45. Balasso M, Kutnar A, Niemelä EP, Mikuljan M, Nolan G, Kotlarewski N, Hunt M, Jacobs A, O’Reilly-Wapstra J (2020) Wood properties characterisation of thermo-hydro mechanical treated plantation and native tasmanian timber species. Forests 11:1–15. https://doi.org/10.3390/f1111118910.3390/f11111189 ↗
46. Cao R, Marttila J, Möttönen V, Heräjärvi H, Ritvanen P, Verkasalo E (2020) Mechanical properties and water resistance of Vietnamese acacia and rubberwood after thermo-hygro-mechanical modification. Eur J Wood Wood Products 78:841–848. https://doi.org/10.1007/s00107-020-01552-710.1007/s00107-020-01552-7 ↗
47. Kamke F, Sizemore H (2004) Viscoelastic thermal compression of wood. US Patent 7,404,422 B2, 5 Feb 2004
48. Rautkari L, Laine K, Laflin N, Hughes M (2011) Surface modification of scots pine: the effect of process parameters on the through thickness density profile. J Mater Sci 46:4780–4786. https://doi.org/10.1007/s10853-011-5388-910.1007/s10853-011-5388-9 ↗
49. Tarkow H, Seborg RM (1968) Surface densification of wood. For Prod J 18:104–107
50. Rautkari L, Kutnar A, Hughes M, Kamke F (2010) Wood surface densification using different methods. In: 11th World Conference on Timber Engineering, Riva del Garda, 20–24 June 2010
51. Rautkari L, Properzi M, Pichelin F, Hughes M (2010) Properties and set-recovery of surface densified Norway spruce and European beech. Wood Sci Technol 44:679–691. https://doi.org/10.1007/s00226-009-0291-010.1007/s00226-009-0291-0 ↗
52. Gong M, Lamason C, Li L (2010) Interactive effect of surface densification and post-heat-treatment on aspen wood. J Mater Process Technol 210:293–296. https://doi.org/10.1016/j.jmatprotec.2009.09.01310.1016/j.jmatprotec.2009.09.013 ↗
53. Kutnar A, Rautkari L, Laine K, Hughes M (2012) Thermodynamic characteristics of surface densified solid Scots pine wood. Eur J Wood Wood Products 70:727–734. https://doi.org/10.1007/s00107-012-0609-810.1007/s00107-012-0609-8 ↗
54. Laine K, Belt T, Rautkari L et al (2013) Measuring the thickness swelling and set-recovery of densified and thermally modified Scots pine solid wood. J Mater Sci 48:8530–8538. https://doi.org/10.1007/s10853-013-7671-410.1007/s10853-013-7671-4 ↗
55. Laine K, Rautkari L, Hughes M (2013) The effect of process parameters on the hardness of surface densified Scots pine solid wood. Eur J Wood Prod 71:13–16. https://doi.org/10.1007/s00107-012-0649-010.1007/s00107-012-0649-0 ↗
56. Laine K, Rautkari L, Hughes M, Kutnar A (2013) Reducing the set-recovery of surface densified solid Scots pine wood by hydrothermal post-treatment. Eur J Wood Prod 71:17–23. https://doi.org/10.1007/s00107-012-0647-210.1007/s00107-012-0647-2 ↗
57. Laskowska A (2017) The influence of process parameters on the density profile and hardness of surface-densified birch wood (betula pendula roth). BioResources 12:6011–602310.15376/biores.12.3.6011-6023 ↗
58. Zhou Q, Chen C, Tu D, Zhu Z, Li K (2019) Surface densification of poplar solid wood: effects of the process parameters on the density profile and hardness. BioResources 14(2):4814–483110.15376/biores.14.2.4814-4831 ↗
59. Wang J, Cooper PA (2005) Vertical density profiles in thermally compressed balsam fir wood. For Prod J 55:65–68
60. Wang JY, Cooper PA (2005) Effect of grain orientation and surface wetting on vertical density profiles of thermally compressed fir and spruce. Holz als Roh - und Werkstoff 63:397–402. https://doi.org/10.1007/s00107-005-0034-310.1007/s00107-005-0034-3 ↗
61. Rowell R (1983) Chemical Modification of Wood. For Prod Abstr. https://doi.org/10.3139/9783446442504.02210.3139/9783446442504.022 ↗
62. Rowell R, Tillman A-M, Simonson R (1986) A simplified procedure for the acetylation of hardwood and softwood flaxes for flakeboard production. J Wood Chem Technol 6:427–448. https://doi.org/10.1080/0277381860808523610.1080/02773818608085236 ↗
63. Youngquist J, Krzysik A, Rowell R (1986) Dimensional stability of acetylated aspen flakeboard. Wood Fibre Sci 18(1):90–98
64. Rowell R, Youngquist J, Rowell J, Hyatt J (1991) Dimensional stability of aspen fiberboard made from acetylated fiber. Wood Fibre Sci 23(4):558–566
65. Larsson P, Simonson R (1994) A study of strength, hardness and deformation of acetylated Scandinavian softwoods. Holz als Roh-und Werkstoff 52:83–86. https://doi.org/10.1007/BF0261547010.1007/BF02615470 ↗
66. Ramsden MJ, Blake FSR, Fey NJ (1997) The effect of acetylation on the mechanical properties, hydrophobicity, and dimensional stability of Pinus sylvestris. Wood SciTechnol 31:97–104. https://doi.org/10.1007/BF0070592510.1007/BF00705925 ↗
67. Inoue M, Morooka T, Rowell RM, Norimoto M, Englund F (2008) Mechanism of partial fixation of compressed wood based on a matrix non-softening method. Wood Mat Sci Eng 3:126–130. https://doi.org/10.1080/1748027090302034710.1080/17480270903020347 ↗
68. Rowell R (2014) Acetylation of wood–a review. Int J Lignocellulosic Products 1(1):1–27
69. Stamm AJ, Alfred J, Seborg RM (1942) Forest products laboratory resin-treated wood (impreg). Forest Products Laboratory, Wisconsin
70. Stamm AJ, Burr HK, Kline AA (1955) Heat stabilized wood (staybwood). Forest Products Laboratory, Wisconsin
71. Inoue M, Morooka T, Norimoto M, Rowell R, Egawa G (1992) Permanent fixation of compressive deformation of wood. FRI Bulletin 176:181–189
72. Shams MdI, Yano H (2011) Compressive deformation of phenol formaldehyde (PF) resin-impregnated wood related to the molecular weight of resin. Wood Sci Technol 45:73–81. https://doi.org/10.1007/s00226-010-0310-110.1007/s00226-010-0310-1 ↗
73. Yue K, Wu J, Xu L, Tang Z, Chen Z, Liu W, Wang L (2020) Use impregnation and densification to improve mechanical properties and combustion performance of Chinese fir. Constr Build Mater 241:118101. https://doi.org/10.1016/j.conbuildmat.2020.11810110.1016/j.conbuildmat.2020.118101 ↗
74. Schwarzkopf M (2021) Densified wood impregnated with phenol resin for reduced set-recovery. Wood Mat Sci Eng 16:35–41. https://doi.org/10.1080/17480272.2020.172923610.1080/17480272.2020.1729236 ↗
75. Inoue M, Ogata S, Kawai S, Rowell R, Norimoto M (1993) fixation of compressed wood using melamine-formaldehyde resin. Wood Fiber Sci 25:404–410
76. Gindl W, Zargar-Yaghubi F, Wimmer R (2003) Impregnation of softwood cell walls with melamine-formaldehyde resin. Biores Technol 87:325–330. https://doi.org/10.1016/S0960-8524(02)00233-X10.1016/S0960-8524(02)00233-X ↗
77. Lykidis C, Kotrotsiou K, Tsichlakis A (2020) Reducing set-recovery of compressively densified poplar wood by impregnation–modification with melamine–formaldehyde resin. Wood Mat Sci Eng 15:269–277. https://doi.org/10.1080/17480272.2019.159436510.1080/17480272.2019.1594365 ↗
78. Lykidis C, Moya R, Tenorio C (2020) The effect of melamine formaldehyde impregnation and hot-pressing parameters on the density profile of densified poplar wood. Eur J Wood Prod 78:433–440. https://doi.org/10.1007/s00107-020-01515-y10.1007/s00107-020-01515-y ↗
79. Esteves BM, Pereira HM (2008) Wood modification by heat treatment: A review. BioRes 4:370–404. https://doi.org/10.15376/biores.4.1.370-40410.15376/biores.4.1.370-404 ↗
80. Laine K, Segerholm K, Walinder M, Rautkari L, Hughes M (2016) Wood densification and thermal modification: hardness, set-recovery and micromorphology. Wood Sci Technol. https://doi.org/10.1007/s00226-016-0835-z10.1007/s00226-016-0835-z ↗
81. Dwianto W, Inoue M, Tanaka F, Norimoto M (1997) Fixation of compressive deformation of wood by heat treatment. J Japan Wood Res Soc 43(4):303–309
82. Pelit H, Sönmez A, Budakçı M (2014) Effects of Thermowood® process combined with thermo-mechanical densification on some physical properties of scots pine (pinus sylvestris l.). BioResources 9:4552–456710.15376/biores.9.3.4552-4567 ↗
83. Pelit H, Budakci M, Sonmez A (2016) Effects of heat post-treatment on dimensional stability and water absorption behaviours of mechanically densified uludag fir and black poplar woods. BioResources 11:3215–322910.15376/biores.11.2.3215-3229 ↗
84. Kutnar A, Kamke FA, Sernek M (2008) The mechanical properties of densified VTC wood relevant for structural composites. Holz Roh Werkst 66:439–446. https://doi.org/10.1007/s00107-008-0259-z10.1007/s00107-008-0259-z ↗
85. Neyses B (2019) Surface densification of solid wood paving the way towards industrial implementation. Dissertation, Luleå University of Technology
86. Welzbacher CR, Wehsener J, Rapp AO, Haller P (2008) Thermo- mechanical densification combined with thermal modification of Norway spruce (Picea abies Karst) in industrial scale – dimensional stability and durability aspects. Holz als Roh - und Werkstoff 66:39–49. https://doi.org/10.1007/s00107-007-0198-010.1007/s00107-007-0198-0 ↗
87. Alen R, Kotilainen R, Zaman A (2002) Thermochemical behavior of Norway spruce (Picea abies) at 180–225 °C. 9. https://doi.org/10.1007/s00226-001-0133-110.1007/s00226-001-0133-1 ↗
88. Ulker O, Imirzi O, Burdurlu E (2012) The effect of densification temperature on some physical and mechanical properties of scots pine (pinus sylvestris l). BioResources 7:5581–5592. https://doi.org/10.15376/biores.7.4.5581-559210.15376/biores.7.4.5581-5592 ↗
89. Kutnar A, Kamke FA (2012) Compression of wood under saturated steam, superheated steam, and transient conditions at 150°C, 160°C, and 170°C. Wood Sci Technol 46:73–88. https://doi.org/10.1007/s00226-010-0380-010.1007/s00226-010-0380-0 ↗
90. Kutnar A, Kamke FA (2012) Influence of temperature and steam environment on set recovery of compressive deformation of wood. Wood Sci Technol 46:953–964. https://doi.org/10.1007/s00226-011-0456-510.1007/s00226-011-0456-5 ↗
91. Shams MI, Yano H, Endou K (2004) Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin I: effects of pressing pressure and pressure holding. J Wood Sci 50:337–342. https://doi.org/10.1007/s10086-003-0570-610.1007/s10086-003-0570-6 ↗
92. Shams MI, Yano H (2004) Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin II: effects of processing parameters. J Wood Sci 50:343–350. https://doi.org/10.1007/s10086-003-0571-510.1007/s10086-003-0571-5 ↗
93. Shams MdI, Kagemori N, Yano H (2006) Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin IV: Species dependency. J Wood Sci 52:179–183. https://doi.org/10.1007/s10086-005-0746-310.1007/s10086-005-0746-3 ↗
94. Song J, Chen C, Zhu S et al (2018) Processing bulk natural wood into a high-performance structural material. Nature 554:224–228. https://doi.org/10.1038/nature2547610.1038/nature25476 ↗
95. Bouhala L, Fiorelli D, Makradi A, Belouettar S, Sotayo A, Bradley DF, Guan Z (2020) Advanced numerical investigation on adhesive free timber structures. Compos Struct 246:112389. https://doi.org/10.1016/j.compstruct.2020.11238910.1016/j.compstruct.2020.112389 ↗
96. Lamason C, Gong M (2007) Optimization of pressing parameters for mechanically surface-densified aspen. For Prod J 57:64–68
97. Rautkari L, Properzi M, Pichelin F, Hughes M (2008) An innovative thermo densification method for wooden surfaces. In: Proceedings of 10th World Conference on Timber Engineering
98. Rautkari L, Laine K, Kutnar A, Medved S, Hughes M (2013) Hardness and density profile of surface densified and thermally modified Scots pine in relation to degree of densification. J Mater Sci 48:2370–2375. https://doi.org/10.1007/s10853-012-7019-510.1007/s10853-012-7019-5 ↗
99. Laine K, Segerholm K, Wålinder M, Rautkari L, Hughes M, Lankveld C (2016) Surface densification of acetylated wood. Eur J Wood Prod 74:829–835. https://doi.org/10.1007/s00107-016-1077-310.1007/s00107-016-1077-3 ↗
100. Shams MdI, Yano H, Endou K (2005) Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin III: effects of sodium chlorite treatment. J Wood Sci 51:234–238. https://doi.org/10.1007/s10086-004-0638-y10.1007/s10086-004-0638-y ↗