Modeling of size, aspect ratio, and orientation of flattened precipitates in the context of Zr-H system under external stress
Source abstract
Abstract
Abstract A model that simulates detailed morphology of flattened precipitates has been developed and applied for the Zr-H thermodynamic system as an example. The mathematical representation of the model is the system of six ordinary differential equations which are solved numerically. The model is based on the classical heterogeneous nucleation approximation to simulate the length, aspect ratio, and orientation of inclusions precipitated during cooling or dissolving during heating in the presence of external mechanical load. This model is directly appliable to the modeling of mechanical properties of zirconium alloys, which are widely used in the nuclear industry. In this practical case, hydrides, formed from hydrogen released during water corrosion, substantially affect the structural component reliability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Aaronson · 2010
2. Microstructure and property evolution of Fe-N ferrite undergoing early-stages of precipitation10.1016/j.msea.2017.04.046 ↗
3. Grain boundary precipitation behavior of δ-Ni3Nb (D0a) phase in a Ni-Nb-Fe ternary model alloy10.1016/j.jallcom.2018.05.169 ↗
4. Puls · 2012
5. Hydrogen in zirconium alloys: a review10.1016/j.jnucmat.2019.02.042 ↗
6. A review on hydride precipitation in zirconium alloys10.1016/j.jnucmat.2015.07.014 ↗
7. Z. Zhao et al., Identification and characterization of a new zirconium hydride, J. Microsc., 232 (3) (2008) 410–421, doi: 10.1111/j.1365-2818.2008.02136.x.10.1111/j.1365-2818.2008.02136.x ↗
8. Investigations of deformation-induced δ → ζ phase transformation in zirconium hydride by in situ high-energy X-ray diffraction10.1016/j.actamat.2017.08.047 ↗
9. Evidence of stress-induced hydrogen ordering in zirconium hydrides10.1016/j.actamat.2008.08.061 ↗
10. Kinetics of the δ to γ zirconium hydride transformation in Zr-2.5Nb10.1016/S1359-6454(03)00004-1 ↗
11. The precipitation of zirconium hydride in zirconium and zircaloy-210.1016/0022-3115(72)90021-9 ↗
12. Formation of nanocrystalline δ-ZrH x in Zircoloy-4: orientation relationship and twinning10.1016/j.jallcom.2015.10.256 ↗
13. Observation of the δ to ε Zr-hydride transition by in-situ synchrotron X-ray diffraction: Observation of the δ to ε Zr-hydride transition by in-situ synchrotron X-ray diffraction10.1002/crat.201600234 ↗
14. Study on the effects of matrix yield strength on hydride phase stability in Zircaloy-2 and Zr 2.5wt% Nb10.1016/j.jnucmat.2011.10.051 ↗
15. Hydrogen contribution to the thermal expansion of hydrided Zircaloy-4 cladding tubes10.1016/j.jnucmat.2013.04.039 ↗
16. Evaluating zirconium–zirconium hydride interfacial strains by nano-beam electron diffraction10.1016/j.jnucmat.2012.08.003 ↗
17. In situ observation of γ-ZrH formation by X-ray diffraction10.1016/j.jallcom.2016.11.337 ↗
18. The habit planes of zirconium hydride in zirconium and zircaloy10.1016/0022-3115(68)90072-X ↗
19. Hydride precipitation in α/β zirconium alloys10.1016/0001-6160(83)90008-1 ↗
20. The stress orientation of hydride in zirconium alloys10.1016/0022-3115(70)90214-X ↗
21. Effects of misfit and external stresses on terminal solid solubility in hydride-forming metals10.1016/B978-0-08-034813-1.50066-8 ↗
22. Stress reorientation of hydrides in zirconium−2.5% niobium10.1016/0022-3115(75)90132-4 ↗
23. Hydride embrittlement in ZIRCALOY-4 plate: Part II. interaction between the tensile stress and the hydride morphology10.1007/BF02652294 ↗
24. J.Y.R. Rashid, A.J. Machiels, Hydride precipitation in spent fuel cladding during storage, 2005.
25. J. Rashid, A. Machiels, Threat of hydride re-orientation to spent fuel integrity during transportation accidents: Myth or reality?, Am. Nucl. Soc. - 2007 LWR Fuel Performance/Top Fuel, 2007, pp. 464–471.
26. Stress orientation of second-phase in alloys: Hydrides in zirconium alloys10.1016/j.commatsci.2009.05.025 ↗
27. A micromechanical model for predicting hydride embrittlement in nuclear fuel cladding material10.1016/0022-3115(95)00160-3 ↗
28. Effect of applied load on nucleation and growth of γ-hydrides in zirconium10.1016/S0927-0256(01)00226-9 ↗
29. Mesoscale modeling of coherent zirconium hydride precipitation under an applied stress10.1016/j.jnucmat.2013.02.034 ↗
30. Phase-field modeling of stacking structure formation and transition of δ-hydride precipitates in zirconium10.1016/j.actamat.2018.12.009 ↗
31. Formation path of δ hydrides in zirconium by multiphase field modeling10.1016/j.actamat.2016.10.056 ↗
32. D. Xu, H. Xiao, Cluster dynamics model for the hydride precipitation kinetics in zirconium cladding, Miner. Met. Mater. Ser., pp. 1759–1768, 2019, doi: 10.1007/978-3-030-04639-2_118.10.1007/978-3-030-04639-2_118 ↗
33. Integrated Computational Modeling of Water Side Corrosion in Zirconium Metal Clad Under Nominal LWR Operating Conditions10.1007/s11837-016-2129-1 ↗
34. Atomic-scale Ab-initio study of the Zr-H system: I. Bulk properties10.1016/S1359-6454(02)00173-8 ↗
35. Atomic-scale ab initio study of the Zr–H system: II. Interaction of H with plane defects and mechanical properties10.1016/j.actamat.2003.11.031 ↗
36. Ab initio thermodynamics of zirconium hydrides and deuterides10.1016/j.commatsci.2014.01.043 ↗
37. Structure and thermodynamic properties of zirconium hydrides by structure search method and first principles calculations10.1016/j.commatsci.2018.03.066 ↗
38. M.A. Louchez, R. Besson, L. Thuinet, A. Legris, Interfacial properties of hydrides in μ-Zr: A theoretical study, J. Phys. Condens. Matter, 29 (41) (2017), doi: 10.1088/1361-648X/aa7f8a.10.1088/1361-648X/aa7f8a ↗
39. Anisotropic hydrogen diffusion in α-Zr and Zircaloy predicted by accelerated kinetic Monte Carlo simulations
40. Modeling of hydrogen behavior in spent fuel claddings during dry storage10.1016/j.jnucmat.2018.06.012 ↗
41. The modeling of the hydrogen solid solubility hysteresis in zirconium alloys10.1016/j.actamat.2019.07.044 ↗
42. The terminal solid solubility of hydrogen and deuterium in Zr-2.5Nb alloys10.1016/S0022-3115(95)00217-0 ↗
43. Terminal solid solubility of hydrogen of optimized-Zirlo and its effects on hydride reorientation mechanisms under dry storage conditions10.1016/j.net.2020.01.022 ↗
44. Nucleation: theory and applications to protein solutions and colloidal suspensions
45. First-principles study of interfacial energy between alpha-zirconium and zirconium hydride10.1063/1.5102176 ↗
46. Characterizing the crystal structure and formation induced plasticity of γ-hydride phase in zirconium10.1016/j.mtla.2019.100454 ↗
47. Precipitation and dissolution peaks of hydride in Zr–2.5Nb during quasistatic thermal cycles10.1016/S0925-8388(00)01028-8 ↗
48. T. Aliev, M. Kolesnik, Analytical approach to DHC description in zirconium alloys, Int. J. Fract., in press, 2020.10.1007/s10704-021-00515-0 ↗
49. In situ study of hydride precipitation kinetics and re-orientation in Zircaloy using synchrotron radiation10.1016/j.actamat.2010.07.018 ↗
50. Synchrotron diffraction study of dissolution and precipitation kinetics of hydrides in Zircaloy-410.1016/j.jnucmat.2011.11.009 ↗
51. Terminal cool-down temperature-dependent hydride reorientations in Zr–Nb Alloy claddings under dry storage conditions10.1016/j.jnucmat.2014.02.007 ↗
52. Cooling rate- and hydrogen content-dependent hydride reorientation and mechanical property degradation of Zr–Nb alloy claddings10.1016/j.jnucmat.2013.06.006 ↗
53. Effect of hydrides on mechanical properties and failure morphology of BWR fuel cladding at very high strain rate
54. Ductile-to-brittle transition temperature for high-burnup cladding alloys exposed to simulated drying-storage conditions10.1016/j.jnucmat.2012.10.002 ↗
55. Hydride orientation in Zr-2.5% Nb; how it is affected by stress, temperature and heat treatment
56. Evaluation of hydride reorientation behavior and mechanical properties for high-burnup fuel-cladding tubes in interim dry storage10.1520/JAI101262 ↗
57. M.C. Billone, T.A. Burtseva, Z. Han, Y.Y. Liu, Effects of Multiple Drying Cycles on High-Burnup PWR Cladding Alloys, FCRD-UFD-2014-000052,“ 2014. [Online]. Available: https://www.energy.gov/sites/prod/files/2014/11/f19/FCRDUFD2014000052NosigDryCladAlloy.pdf.10.2172/1159911 ↗
58. Effects of hydride precipitation on the mechanical property of cold worked zirconium alloys in fully recrystallized condition10.1016/j.net.2019.07.032 ↗
59. Criteria for fracture initiation at hydrides in zirconium alloys I. Sharp crack tip10.1016/0022-3115(94)90332-8 ↗
60. The elastic strain energy of coherent ellipsoidal precipitates in anisotropic crystalline solids10.1007/BF02661580 ↗