Chemical behaviour of ground waste glass when used as partial cement replacement in mortars
Source abstract
Abstract
Abstract This paper deals with the pozzolanic activity of finely ground waste glass, when used as partial cement replacement in mortars. The behaviour of this by-product was examined through two sets of tests: a lime–glass test to assess and explain the pozzolanic phenomena and a compressive strength test carried out to monitor the strength development. Analyses by DSC, XRD and SEM of samples containing 25% Ca(OH)2 and 75% of ground glass demonstrated that this admixture induced the formation of calcium silicate and calcium aluminosilicate hydrates at the expense of lime as well as hydrated sodium carbonate. The formation of the latter phase allowed us to explain the size stability of prepared mortars by hydrated sodium silicate formation. Compressive strength of mortars containing ground glass with particles size in the range 100–80 μm; 80–40 μm;
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Chesner WH, Coollins RJ. Mackay M.H., User guidelines for waste and by-product materials in pavement construction. US Department of transportation, federal highway administration, Publication No. FHWA-RD; 1997. p. 97–148.
2. Meyer C, Egosi N, Andela C. Concrete with waste glass as aggregate. In: Recycling and reuse of glass cullet. In: Proceedings of the international symposium. Concrete technology unit of ASCE and University of Dendee; 2001.
3. Properties of concrete containing waste glass10.1016/j.cemconres.2003.07.003 ↗
4. Relative strength of green glass cullet concrete10.1680/macr.2004.56.5.293 ↗
5. Studies on mechanical properties of concrete containing waste glass aggregate10.1016/j.cemconres.2004.02.006 ↗
6. Glass recycling in cement production-an innovative approach10.1016/S0956-053X(02)00047-8 ↗
7. Use of recycled glass as a raw material in the manufacture of Portland cement10.1007/BF02483139 ↗
8. Durability of mortar using waste glass powder as cement replacement10.1016/j.conbuildmat.2012.04.027 ↗
9. Characterization and pozzolanic reactivity of glass powders10.1016/j.cemconres.2004.05.015 ↗
10. Chemical reactions of glass cullet used as cement component10.1061/(ASCE)0899-1561(2001)13:6(412) ↗
11. Performance of glass powder as a pozzolanic material in concrete: a field trial on concrete slabs10.1016/j.cemconres.2005.12.012 ↗
12. Influence of fine glass powder on the durability characteristics of concrete and its comparison to fly ash10.1016/j.cemconcomp.2008.02.001 ↗
13. The potential pozzolanic activity of glass and red-clay ceramic waste as cement mortars components10.1016/j.conbuildmat.2011.12.110 ↗
14. Meyer C, Baxter S, Jin W. Potential of waste glass for concrete masonary blocks. In: Proceedings of the 4th Materials engineering conference, Washington; 1996. p. 666–673.
15. American Society for Testing and Materials, ASTM C 311-02; Standard test methods for sampling and testing fly ash or natural pozzolans for use in Portland-cement concrete.
16. Participation of coloured glass cullet in cementitious materials10.1016/j.cemconcomp.2004.02.021 ↗
17. American society for testing and materials, C 618–02. Standard specification for Coal fly ash and raw or calcined natural pozzolan for use in concrete.
18. Alkalies in cement: A review10.1016/0008-8846(78)90056-X ↗
19. Ambroise J, Martin Calle S, Péra J. Pozzolanic behavior of thermally activated Kaolin. 4th Int. Conf Istambul Turkey SP; 1992. p.132–140.
20. Influence of MK on the reaction kinetics in MK/lime and MK-blended cement system at 20°C10.1016/S0008-8846(00)00465-8 ↗
21. Reaction between silica and calcium hydroxide solutions. I. Kinetics in the temperature range 30 to 85 °C10.1021/j100819a005 ↗