Effect of different curing regimes and durations on early strength development of reactive powder concrete
Source abstract
Abstract
Abstract The early strength development of Reactive Powder Concrete (RPC) has been investigated under different curing regimes and compared with standard water curing condition. Four different curing regimes have been considered: ambient air curing, hot air curing, hot water bath curing and accelerated curing. The effect of hot air curing on strength development of RPC at different temperatures and durations are studied in detail. The present study is focused on the effect of combined curing regimes on the early strength development of RPC. Test results indicate that, among the four different curing regimes, hot water bath curing gives higher strength. The combined curing regime has considerably enhanced the compressive strength of RPC by about 63% as is evident by the rise in compressive strength from 110 MPa (standard curing) to 180 MPa (combined curing). Microstructure studies were also conducted to understand the arrangements of hydrated particles and development of other secondary hydrated products under different curing conditions using scanning electron microscope and X-ray diffraction spectroscopy respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Composition of reactive powder concretes10.1016/0008-8846(95)00144-2 ↗
2. Mechanical properties of reactive powder concretes10.1007/BF02485945 ↗
3. Preparation of ultra-high performance concrete with common technology and materials10.1016/j.cemconcomp.2011.11.005 ↗
4. Optimal conditions for producing reactive powder concrete10.1680/macr.2010.62.10.701 ↗
5. Influence of mixing method, speed and duration on the fresh and hardened properties of reactive powder concrete10.1016/j.conbuildmat.2017.03.009 ↗
6. Mechanical properties and durability of two industrial reactive powder concretes
7. T. Teichmann, M. Schmidt, Influence of the packing density of fine particles on structure, strength and durability of UHPC, in: First Int Symp Ultra High Perform Concr, Die Duetsche Bibliothek, Kassel, 2004, pp. 313–325.
8. İ.B. Topçu, C. Karakurt, Reaktif pudra beton lari, TMH – TÜRKÝYE MÜHENDÝSLÝK HABERLERÝ SAYI, 437, 2005, pp. 25–30, http://www.imo.org.tr/resimler/dosya_ekler/08c4c72401a4149_ek.pdf.
9. Optimization of mechanical properties and durability of reactive powder concrete
10. Mechanical properties of reactive powder concrete containing mineral admixtures under different curing regimes10.1016/j.conbuildmat.2008.08.003 ↗
11. Effects of high-pressure/temperature curing on reactive powder concrete microstructure formation10.1016/j.conbuildmat.2015.12.147 ↗
12. The effect of autoclave pressure, temperature and duration time on mechanical properties of reactive powder concrete10.1016/j.conbuildmat.2013.01.003 ↗
13. M. S?mer, M. Saribiyik, Effect of pre-setting pressure applied to mechanical behaviours of reactive powder concrete during setting phase10.1016/j.conbuildmat.2010.06.056 ↗
14. The effect of pre-setting pressure applied flexural strength and fracture toughness of reactive powder concrete during the setting phase10.1016/j.conbuildmat.2011.06.045 ↗
15. Effect of polycarboxylate and crushed quartz in UHPC: microstructural investigation10.1016/j.conbuildmat.2013.03.077 ↗
16. Investigation of hydration and pozzolanic reaction in reactive powder concrete (RPC) using 29Si NMR10.1016/0008-8846(95)00197-2 ↗
17. The effect of curing conditions on compressive strength of ultra high strength concrete with high volume mineral admixtures10.1016/j.buildenv.2006.03.013 ↗
18. A study on delayed deformations of an ultra-high strength cementitious material
19. Mechanical properties of modified reactive powder concrete
20. Silica fume distribution and reactivity in reactive powder concretes
21. The effect of the heat-treatment regime on the properties of reactive powder concrete10.1680/adcr.2007.19.1.25 ↗
22. Fire performance of highly flowable reactive powder concrete10.1016/j.conbuildmat.2008.08.022 ↗
23. Non-destructive testing of ultra high performance fibre reinforced concrete (UHPFRC): a feasibility study for using ultrasonic and resonant frequency testing techniques10.1016/j.conbuildmat.2012.04.047 ↗
24. Ultra-high strength concrete mixtures using local materials
25. Studying the production process and mechanical properties of reactive powder concrete: a Hong Kong study10.1680/macr.9.00063 ↗
26. Very-high-performance concrete with ultrafine powders10.1016/S0008-8846(01)00732-3 ↗
27. Influence of aggregate and curing regime on the mechanical properties of ultra-high performance fibre reinforced concrete (UHPFRC)10.1016/j.conbuildmat.2008.11.012 ↗
28. Microstructural behaviour of reactive powder concrete under different heating regimes10.1680/macr.2012.64.3.259 ↗
29. Influence of condensed silica fume on the pore-size distribution of concretes10.1021/i300010a024 ↗
30. THE SVANHOLM GROUP OF COMPANIES, 2009, http://www.svanholm.se/index.html.
31. Hydrothermal formation of the calcium silicate hydrates, tobermorite (Ca5Si6O16(OH)2·4H2O) and xonotlite (Ca6Si6O17(OH)2): an in situ synchrotron study10.1016/S0009-2541(99)00205-3 ↗
32. Hebel AAC, 2009, http://www.hebel.co.nz/about/index.php.
33. Microstructural analysis of RPC (Reactive Powder Concrete)10.1016/0008-8846(95)00143-Z ↗
34. D. Heinz, H.M. Ludwig, Heat treatment and the risk of DEF delayed ettringite formation in UHPC, in: Int Symp Ultra-High Perform Concr, Kassel University Press, Kassel, Germany, 2004, pp. 717–730.
35. Synthesis of normal and anomalous tobermorites10.1016/0008-8846(77)90071-0 ↗
36. Effects of microstructure on fracture behavior of hardened cement paste10.1557/PROC-370-99 ↗