Waste glass as a precursor in alkaline activation: Chemical process and hydration products
Source abstract
Abstract
This paper discusses the results of alkali-activating waste glass in pursuit of a new type of alkali activated materials (AAMs). Waste glass pastes were prepared with different alkaline activators (NaOH, NaOH/ Na2CO3, sodium silicate hydrate and KOH) with different concentrations and cured for 20 h at 85 C and at 99% or 6.5% relative humidity to assess the effect of these variables on paste mechanical strength and microstructure. Compressive strength performance was better at the higher alkaline concentrations and when the pastes were cured at low relative humidity (6.5%), which induced low porosity (MIP) and high specific surface (BET). Irrespective of the type of activator or curing process, the main reaction product was a Si-high, Al-low gel. As a raw material for alkaline cement manufacture, waste glass delivered compact, high-strength cementitious skeletons.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. The action of alkalis on blast-furnace slag
2. High strength slag-alkaline cements
3. Slag-alkaline cements and concretes structures, properties, technological and economic aspects of the use
4. Davidovits · 2008
5. Activation of metakaolin/slag blends using alkaline solutions based on chemically modified silica fume and rice husk ash10.1007/s12649-011-9093-3 ↗
6. Chemical stability of cementitious materials based on metakaolin10.1016/S0008-8846(99)00074-5 ↗
7. Alkaline activation of metakaolin and calcium hydroxide mixtures: influence of temperature, activator concentration and solids ratio10.1016/S0167-577X(00)00212-3 ↗
8. Natural pozzolan-and granulated blast furnace slag-based binary geopolymers10.3989/mc.2016.03615 ↗
9. Cementos de escorias activadas alcalinamente: Situación actual y perspectivas de futuro10.3989/mc.1995.v45.i239.553 ↗
10. A model for the C-A-S-H gel formed in alkali-activated slag cements10.1016/j.jeurceramsoc.2011.04.036 ↗
11. Escorias de alto horno: composición y comportamiento hidráulico
12. MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders10.1016/j.cemconres.2013.12.003 ↗
13. Shi · 2006
14. A review on alkaline activation: new analytical perspectives
15. Properties of fly ash and metakaolín based geopolymer panels under fire resistance tests10.3989/mc.2015.06114 ↗
16. Stabilization/solidification of hazardous and radioactive wastes with alkali-activated cements10.1016/j.jhazmat.2006.05.008 ↗
17. Overview of the potential of urban waste glass as a cementitious material in alternative chemically activated binders
18. Ecovidrio, Ecovidrio, http://www.ecovidrio.es/, 2015.
19. Binary silicate glasses in the study of alkali-aggregate reaction
20. Alkali-aggregate reaction tests on glass used for exposed aggregate wall panel work
21. Waste glass as coarse aggregate for concrete10.1520/JTE10117J ↗
22. Alkali-aggregate reaction in concrete with waste glass as aggregate
23. Use of recycled glass and fly ash for precast concrete10.1061/(ASCE)0899-1561(1999)11:2(89) ↗
24. Potential for using waste glass in portland cement concrete10.1061/(ASCE)0899-1561(1998)10:4(210) ↗
25. Fracture mechanics of ASR in concretes with waste glass particles of different sizes
26. Waste glass as concrete aggregate and pozzolan
27. Properties of concrete containing waste glass
28. Waste E-glass Particles used in cementitious mixtures10.1016/j.cemconres.2005.12.010 ↗
29. Glass recycling in cement production–an innovative approach10.1016/S0956-053X(02)00047-8 ↗
30. A review on the use of waste glasses in the production of cement and concrete10.1016/j.resconrec.2007.01.013 ↗
31. Use of recycled glass as a raw material in the manufacture of Portland cement10.1007/BF02483139 ↗
32. Chemical behaviour of ground waste glass when used as partial cement replacement in mortars10.1016/j.conbuildmat.2013.02.040 ↗
33. Use of glass waste as an activator in the preparation of alkali-activated slag. Mechanical strength and paste characterisation10.1016/j.cemconres.2013.12.005 ↗
34. Waste glass in the geopolymer preparation. Mechanical and microstructural characterisation10.1016/j.jclepro.2014.11.074 ↗
35. Sodium silicate solutions from dissolution of glass wastes: statistical analysis
36. Durability of alkali-activated slag concretes prepared using waste glass as alternative activator
37. Reuse of urban and industrial waste glass as novel activator for alkali-activated slag cement pastes: a case study
38. Geopolymer binders from metakaolin using sodium waterglass from waste glass and rice husk ash as alternative activators: a comparative study10.1016/j.conbuildmat.2016.03.184 ↗
39. Carbon dioxide equivalent (CO2) emissions: a comparison between geopolymer and OPC cement concrete10.1016/j.conbuildmat.2013.01.023 ↗
40. Effect of calcium on the alkaline activation of aluminosilicate glass10.1016/j.ceramint.2016.01.184 ↗
41. Alkaline activation of synthetic aluminosilicate glass10.1016/j.ceramint.2013.10.146 ↗
42. Phase evolution of C-(N)-A-S-H/N-A-S-H gel blends investigated via alkali-activation of synthetic calcium aluminosilicate precursors10.1016/j.cemconres.2016.08.010 ↗
43. Phase evolution of Na2O–Al2O3 –SiO2 –H2O gels in synthetic aluminosilicate binders10.1039/C5DT04878H ↗
44. Properties of inorganic polymer (geopolymer) mortars made of glass cullet10.1007/s10853-011-6107-2 ↗
45. Microstructure, strength, and moisture stability of alkali activated glass powder-based binders10.1016/j.cemconcomp.2013.09.011 ↗
46. Investigation of novel waste glass and limestone binders using statistical methods10.1016/j.conbuildmat.2015.02.085 ↗
47. Alkali activated composite binders of waste silica soda lime glass and blast furnace slag: strength as a function of the composition10.1016/j.conbuildmat.2016.05.064 ↗
48. Alkali-activated fly ash: effect of thermal curing conditions on mechanical and microstructural development-Part II10.1016/j.fuel.2006.07.010 ↗
49. Fly ash based zeolite cements. Innovations and developments in concrete materials and construction
50. Heat-resistant fly ash based geocements
51. Kovalchuk · 2002
52. Alkali activation of fly ashes. Part 1: effect of curing conditions on the carbonation of the reaction products10.1016/j.fuel.2005.03.030 ↗
53. Workability loss and compressive strength development of cementless mortars activated by combination of sodium silicate and sodium hydroxide10.1061/(ASCE)0899-1561(2009)21:3(119) ↗
54. Alkali activated fly ash binders. A comparative study between sodium and potassium activators10.3989/mc.2006.v56.i281.92 ↗
55. The effect of alkali metals on the formation of geopolymeric gels from alkali-feldspars10.1016/S0927-7757(02)00499-5 ↗
56. On the glass in coal fly ashes: recent advances10.1557/PROC-113-3 ↗
57. Characterization of some glasses in the system SiO2, Na2O·RO by infrared spectroscopy10.1016/S0254-0584(02)00215-8 ↗
58. Preparación y caracterización de vidrios del sistema CaO-SiO2 por el procedimiento sol-gel
59. FTIR study of the sol-gel synthesis of cementitious gels: C-S-H and N-A-S-H10.1007/s10971-007-1643-6 ↗
60. The structure of alkaline earth aluminosilicate glasses as determined by vibrational spectroscopy10.1016/0022-3093(91)90152-V ↗
61. Alkali activation of fly ash: effect of the SiO2/Na2O ratio10.1016/j.micromeso.2007.02.055 ↗
62. Effect of the SiO2/Na2O ratio on the alkali activation of fly ash. Part II: 29Si MAS-NMR Survey10.1016/j.micromeso.2007.05.062 ↗
63. Do Geopolymers actually contain nanocrystalline zeolites? A reexamination of existing results10.1021/cm050230i ↗
64. Breck · 1973
65. Understanding the relationship between geopolymer composition, microstructure and mechanical properties10.1016/j.colsurfa.2005.06.060 ↗
66. The effect of alkali and Si/Al ratio on the development of mechanical properties of metakaolin based geopolymers10.1016/j.colsurfa.2006.05.044 ↗
67. Alkali-activated fly ashes A cement for the future10.1016/S0008-8846(98)00243-9 ↗
68. Pore solution in alkali-activated slag cement pastes. relation to the composition and structure of calcium silicate hydrate10.1016/S0008-8846(03)00254-0 ↗
69. Alkali activation of a slag at ambient and elevated temperatures10.1016/j.cemconcomp.2011.08.003 ↗
70. Influence of different curing temperatures and alkali activators on properties of GBFS geopolymer mortars containing fly ash and palm-oil fuel ash10.1016/j.conbuildmat.2016.08.153 ↗
71. Fracture properties of GGBFS-blended fly ash geopolymer concrete cured in ambient temperature10.1617/s11527-016-0893-6 ↗
72. Effect of cement addition, solution resting time and curing characteristics on fly ash based geopolymer concrete performance10.1016/j.conbuildmat.2016.07.043 ↗
73. Influence of curing schedule on the integrity of geopolymers10.1007/s10853-006-0533-6 ↗
74. K-Based Geopolymer from metakaolin: roles of K / Al ratio and water or steam curing at different temperatures10.3989/mc.2016.03115 ↗
75. Fernández-Navarro · 2003