Using calcium carbide residue as an alkaline activator for glass powder–clay geopolymer
Source abstract
Abstract
Abstract This study investigated the viability of using calcium carbide residue (CCR) as an alkaline activator and recycled glass powder (RGP) as a precursor to improve properties of clay soils. The chemical composition of soil, RGP and CCR were determined by XRF. A compressive strength test was run on the specimens to investigate their mechanical behavior. The effect of different factors such as the CCR content, RGP content, initial synthesis temperature and curing time was investigated. SEM/EDX analysis confirmed the formation of a geopolymeric gel. The results show that both CCR and RGP materials can be used to stabilize clay soil.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Fundamental parameters of cement-admixed clay new approach10.1061/(ASCE)1090-0241(2004)130:10(1042) ↗
2. Waste glass powderbased alkali-activated mortar10.15623/ijret.2014.0325006 ↗
3. Geopolymers: inorganic polymeric new materials10.1007/BF01912193 ↗
4. Davidovits · 2008
5. He · 2012
6. Effect of the alkali metal activator on the properties of fly ash-based geopolymers10.1021/ie980804b ↗
7. Xu · 2002
8. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
9. Mechanism of geopolymerization and factors influencing its development: a review10.1007/s10853-006-0401-4 ↗
10. Sodium silicate-based, alkali-activated slag mortars Part I. Strength, hydration and microstructure10.1016/S0008-8846(02)00717-2 ↗
11. Binding mechanism and properties of alkaliactivated fly ash/slag mortars10.1016/j.conbuildmat.2012.11.003 ↗
12. Strenth development in silty clay stabilized with calcium carbide residue and fly ash10.1016/j.sandf.2013.06.001 ↗
13. Influence of wet-dry cycles on compressive strength of calcium carbide residue-fly ash stabilized clay10.1061/(ASCE)MT.1943-5533.0000853 ↗
14. Soil stabilization by calcium carbide residue10.1061/(ASCE)MT.1943-5533.0000370 ↗
15. Engineering properties of calcium carbide residue stabilized silty clay10.1061/(ASCE)MT.1943-5533.0000618 ↗
16. Calcium carbide residue: alkaline activator for clay–fly ash geopolymer10.1016/j.conbuildmat.2014.07.018 ↗
17. Marginal lateritic soil stabilized with calcium carbide residue and fly ash geopolymers as a sustainable pavement base material10.1061/(ASCE)MT.1943-5533.0001708 ↗
18. Stabilisation of marginal lateritic soil using high calcium fly ash-based geopolymer10.1080/14680629.2015.1132632 ↗
19. Waste glass powder-based alkali-activated mortar10.15623/ijret.2014.0325006 ↗
20. Waste glass in the geopolymer preparation. Mechanical and microstructural characterization10.1016/j.jclepro.2014.11.074 ↗
21. Preparacion de cementos alcalinos a partir de residuos vitreos. Solubilidad de residuos vítreos en medios fuertemente basicos
22. Use of glass waste as an activator in the preparation of alkali-activated slag.Mechanical strength and paste characterisation10.1016/j.cemconres.2013.12.005 ↗
23. Puertas Sodium silicate solutions from dissolution of glass wastes: statistical analysis10.3989/mc.2014.05213 ↗
24. High strength geopolymer binder based on waste-glass powder10.1016/j.apt.2016.09.034 ↗
25. Alkali activated slag cements using waste glass as alternative activators. Rheological behaviour10.1016/j.bsecv.2015.03.004 ↗
26. ASTM D4318-00 · 2010
27. ASTM D422 · 2007
28. ASTM D2487 · 2011
29. Experimental feasibility study of geopolymer as the next-generation soil stabilizer10.1016/j.conbuildmat.2013.06.017 ↗
30. ASTM D698 · 2007
31. Analysis of strength development in cement-stabilized silty clay from microstructural considerations10.1016/j.conbuildmat.2010.03.011 ↗
32. A laboratory study on the strength improve of expansive soil treated with calcium carbide residue and fly ash
33. ASTM D2216-05, Standard Test Methods for Laboratory Determination of Water (Moisture) Content of Soil and Rock by Mass, Annual Book of ASTM Standards, West Conshohocken, PA, 2005.
34. ASTM D2166, Standard Test Method for Unconfined Compressive Strength of Cohesive Soil, Annual Book of ASTM Standards, West Conshohocken, 2016.
35. Alkali activated fly ashes: a cement for the future10.1016/S0008-8846(98)00243-9 ↗
36. Effect of curing temperature and silicate concentration on fly-ashbased geopolymerization
37. Alkaline activation of metakaolin and calcium hydroxide mixtures: influence of temperature, activator concentration and solids ratio10.1016/S0167-577X(00)00212-3 ↗
38. Improving the compressive strength of mortar from a binder of fly ash-calcium carbide residue10.1016/j.conbuildmat.2017.04.167 ↗
39. Characterization of the pore structure of metakaolin-derived geopolymers by neutron scattering and electron microscopy10.1107/S0021889811021078 ↗
40. Strength development of Recycled Asphalt Pavement - Fly ash geopolymer as a road construction material10.1016/j.conbuildmat.2016.04.136 ↗
41. Recycled asphalt pavement - fly ash geopolymers as a sustainable pavement base material: strength and toxic leaching investigations10.1016/j.scitotenv.2016.08.078 ↗
42. Effect of wetting-drying cycles on compressive strength and microstructure of recycled asphalt pavement - Fly ash geopolymer10.1016/j.conbuildmat.2017.03.243 ↗
43. Understanding the relationship between geopolymer composition, microstructure and mechanical properties10.1016/j.colsurfa.2005.06.060 ↗