journal article·2017-05Open access

Optimization of lightweight GGBFS and FA geopolymer mortars by response surface method

Kasım Mermerdaş, Zeynep Algın, Safie Mahdi Oleiwi, Dia Eddin Nassani

Abstract

Abstract In the first stage of the paper, the effect of binder content, curing temperature and curing time on the compressive strength of light-weight geopolymer mortar (LWGM) was investigated. The base materials used for LWGM are ground granulated blast furnace slag (GGBFS) and fly ash (FA). The main components of LWGM are lightweight pumice aggregate and alkali activated FA or GGBFS binder. Effectiveness of aforementioned parameters was examined in terms of variation of the compressive strengths of LWGMs. The experiments were performed on LWGM cubes under curing temperatures of 60, 80, 100 and 120 °C with curing period of 2, 6, 8, 24, 48 and 72 h. The alkaline activator is a mix of 12 M NaOH solution with sodium silicate in ratio of 1:2.5. The ratio of alkaline solution to binder was taken as 0.50. 7 binder contents were taken between 650 to 1250 kg/m 3 with 100 kg/m 3 increment. Full factorial experimental program was adopted to observe compressive strength development of LWGMs. Therefore, 336 data samples were obtained. The second stage of the paper is to optimize those experimental parameters through response surface method. Test results indicate that the increment in the binder content increases the compressive strength of LWGM. The strength increases with the increase of curing temperature and curing period of LWGM. The experimental verification indicated a good agreement with optimized results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Global warming impact on the cement and aggregate Industrie
2. Engineering properties of alkali-activated fly ash concrete
3. Effect of curing temperature and silicate concentration on fly-ash-based geopolymerization10.1021/ie051251p ↗
4. Davidovits · 1994 · vol. 144
5. Alkali activation of Australian slag cements10.1016/S0008-8846(98)00170-7 ↗
6. P. Nath, P. Sarker, Geopolymer concrete for ambient curing condition, in: Proceedings of the Australasian Structural Engineering Conference, Perth, Australia; 11–13 July, 2012.
7. Compressive strength, modulus of elasticity, and water permeability of inorganic polymer concrete10.1016/j.matdes.2010.05.012 ↗
8. Resistance of alkali-activated slag concrete to alkali–aggregate reaction10.1016/S0008-8846(00)00483-X ↗
9. Resistance of alkali-activated slag concrete to carbonation
10. Engineering properties and carbon footprint of ground granulated blast-furnace slag-palm oil fuel ash-based structural geopolymer concrete10.1016/j.conbuildmat.2015.10.026 ↗
11. On the development of fly ash based geopolymer concrete
12. Environmental, physical and structural characterisation of geopolymer matrixes synthesised from coal combustion fly ashes
13. Geopolymer as well cement and the variation of its mechanical behavior with curing temperature10.1002/ghg.39 ↗
14. NaOH activated ground fly ash geopolymer cured at ambient temperature10.1016/j.fuel.2011.01.018 ↗
15. The effect of composition and temperature on the properties of fly ash-and kaolinite-based geopolymers10.1016/S1385-8947(02)00025-6 ↗
16. Geopolymerisation: a review and prospects for the minerals industry10.1016/j.mineng.2007.07.011 ↗
17. Acceleration of strength gain of lime–pozzolan cements by thermal activation
18. Effect of elevated temperature curing on properties of alkali-activated slag concrete
19. Strength and setting times of low calcium fly ash-based geopolymer mortar10.5539/mas.v2n4p3 ↗
20. Compressive strength and microstructural analysis of fly ash/palm oil fuel ash based geopolymer mortar under elevated temperatures10.1016/j.conbuildmat.2014.04.064 ↗
21. Neville · 2004
22. Shi · 2006
23. Lightweight concretes of activated metakaolin-Fy ash binders, with blast furnace slag aggregates10.1016/j.conbuildmat.2009.12.024 ↗
24. RILEM commission for concrete, “Correlation factors between the strengths of different specimen types” RILEM bulletin, Paris, No. 39, 1957, pp. 81–105.
25. The effects of Na2O/SiO2 molar ratio, curing temperature and age on compressive strength, morphology and microstructure of alkali-activated fly ash-based geopolymers10.1016/j.cemconcomp.2011.03.006 ↗
26. The development of compressive strength of ground granulated blast furnace slag-palm oil fuel ash-fly ash based geopolymer mortar10.1016/j.matdes.2013.11.080 ↗
27. Kinetics of geopolymerization: role of Al2O3 and SiO210.1016/j.cemconres.2007.01.003 ↗
28. Influence of granulated blast furnace slag on the reaction, structure and properties of fly ash based geopolymer10.1007/s10853-009-3934-5 ↗
29. Early strength development and hydration of alkali-activated blast furnace slag/fly ash blends10.1680/adcr.1999.11.4.189 ↗
30. Mineralogical and microstructural characterization of alkali-activated fly ash/slag pastes10.1016/S0958-9465(02)00059-8 ↗
31. Mechanical properties and durability of volcanic ash based geopolymer mortars10.1016/j.conbuildmat.2016.07.141 ↗
32. Properties of lightweight high calcium fly ash geopolymer concretes containing recycled packaging foam10.1016/j.conbuildmat.2015.07.080 ↗
33. Whitcomb · 2004
34. Pradeep · 2008
35. Myers · 2009
36. Evaluating free time activities of university students: Kocaeli University study
37. Study on computer and Internet addiction among university students: an application of Kocaeli
38. Statistical analysis of the performance of the soft computing based prediction model for shrinkage of concrete including mineral admixtures
39. Influence of molarity and chemical composition on the development of compressive strength in POFA based geopolymer mortar10.1155/2015/647071 ↗