Abstract

Abstract With the widely use of high-performance concrete, the lower and lower water-to-cement (w/c) ratio is applied in practice. This low w/c ratio can offer high strength and low permeability, however, coming with other drawbacks, such as high self-desiccation and high temperature rise, both of which can increase the early-age cracking potential of concrete. Creep is important to evaluate the early-age cracking resistance of concrete. Although studies on the influence of w/c ratio on the creep of mature concrete have been conducted, investigations on the influence of w/c ratio on the early-age tensile creep remain lacking. Therefore, investigations on the influence of w/c ratio on the tensile creep and cracking resistance of early-age concrete must be conducted. Experimental studies on the influence of w/c ratio (0.33, 0.40, and 0.50) on the temperature change, autogenous shrinkage, restrained stress, tensile creep, and cracking resistance of early-age concrete under adiabatic condition and at full restraint degree were conducted using Temperature Stress Test Machine. The test results indicate that (1) the temperature rise under adiabatic condition increased by 32.6%, and 74.2% when w/c ratio decreased from 0.50 to 0.40, and 0.33, respectively; (2) the restrained tensile stress rate under adiabatic condition and at full restraint degree increased by 16.7%, and 33.3% when w/c ratio decreased from 0.50 to 0.40, and 0.33, respectively; (3) the early-age specific basic tensile creep and basic tensile creep/shrinkage under adiabatic condition and at full restraint degree increased with the decrease of w/c ratio; (4) the early-age cracking potential under adiabatic condition and at full restraint degree increased with the decrease of w/c ratio according to the integrated criterion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Properties and Behavior · Concrete and Cement Materials Research · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Tensile creep behavior of high strength concretes at early ages10.1007/BF02479631 ↗
2. Using accelerated pavement testing to examine traffic opening criteria for concrete pavements10.1016/j.conbuildmat.2015.07.177 ↗
3. Relationship between tensile Young’s modulus and strength of fly ash high strength concrete at early age10.1016/j.conbuildmat.2016.06.145 ↗
4. Experimental study of early-age bond behavior between high strength concrete and steel bars using a pull-out test10.1016/j.conbuildmat.2016.03.094 ↗
5. Freeze–thaw durability of high strength concrete under deicer salt exposure10.1016/j.conbuildmat.2015.10.194 ↗
6. Real-time measurements of temperature, pressure and moisture profiles in high-performance concrete exposed to high temperatures during neutron radiography imaging10.1016/j.cemconres.2014.11.003 ↗
7. The effect of hybrid fibers and expansive agent on the shrinkage and permeability of high-performance concrete10.1016/S0008-8846(00)00479-8 ↗
8. Protected paste volume in concrete: extension to internal curing using saturated lightweight fine aggregate10.1016/S0008-8846(99)00178-7 ↗
9. An experimental approach for the analysis of early-age behavior of high-performance concrete structures under restrained shrinkage10.1016/j.cemconres.2006.11.005 ↗
10. Reducing cracking in concrete structures by using internal curing with high volumes of fly ash
11. Early-age properties of cement-based materials: II. Influence of water-to-cement ratio10.1061/(ASCE)0899-1561(2009)21:9(512) ↗
12. Self-desiccation and its importance in concrete technology10.1007/BF02486354 ↗
13. Early age creep
14. Tensile creep due to restraining stresses in high-strength concrete at early ages10.1016/j.cemconres.2005.11.017 ↗
15. Early age creep and stress relaxation tests
16. Tensile creep of concrete: study of its sensitivity to basic parameters
17. Tensile basic creep: measurements and behavior at early age
18. Tensile basic creep versus compressive basic creep at early ages: comparison between normal strength concrete and a very high strength fibre reinforced concrete10.1617/s11527-013-0150-1 ↗
19. Tensile creep at early ages of ordinary, silica fume and fiber reinforced concretes10.1016/0008-8846(95)00102-I ↗
20. Predicting the tensile creep of concrete10.1016/j.cemconcomp.2014.07.010 ↗
21. Creep, shrinkage, and cracking of restrained concrete at early age
22. Autogenous shrinkage and induced restraining stresses in high-strength concretes10.1016/S0008-8846(00)00399-9 ↗
23. Temperature and relative humidity analysis in early-age concrete decks of composite bridges
24. Effects of construction time and coarse aggregate on bridge deck cracking
25. ACI Committee 207 · 1995
26. Parametric assessment of stress development and cracking in internally cured restrained mortars experiencing autogenous deformations and thermal loading
27. Effect of internal curing with super absorbent polymers on the relative humidity of early-age concrete10.1016/j.conbuildmat.2015.08.042 ↗
28. Prediction model for relative humidity of early-age internally cured concrete with pre-wetted lightweight aggregates10.1016/j.conbuildmat.2017.03.088 ↗
29. Testing system for determining the mechanical behavior of early age concrete under restrained and free uniaxial shrinkage10.1007/BF02473424 ↗
30. Effect of internal curing with super absorbent polymers on residual stress development and stress relaxation in restrained concrete ring specimens10.1016/j.conbuildmat.2016.05.048 ↗
31. Tensile creep behavior of concrete subject to constant restraint at very early ages10.1061/(ASCE)MT.1943-5533.0000671 ↗
32. Internal curing of high-performance concrete with pre-soaked fine lightweight aggregate for prevention of autogenous shrinkage cracking10.1016/j.cemconres.2008.02.001 ↗
33. Influence of curing temperature on autogenous shrinkage and cracking resistance of high-performance concrete at an early age10.1016/j.conbuildmat.2015.11.039 ↗
34. Influence of constituents, mix proportions and temperature on cracking sensitivity of concrete
35. R. Springenschmid, E. Gierlinger, W. Kiernozicky, Thermal stresses in mass concrete: A new testing method and he influence of different cements, in: Proceedings of the 15th International Conference On Large Dams (ICOLD), Lausanne, 1985, pp. 57–72.
36. Test Device for Studying the Early-Age Stresses and Strains in Concrete
37. Quantifying stress development and remaining stress capacity in restrained, internally cured mortars
38. R. Springenschmmid, R. Breitenbücher, Practical experience with concrete technology measures to avoid cracking, in: RILEM Int. Symposium on Avoidance of Thermal Cracking in Concrete, Munich, 1994.
39. Influence of prewetted lightweight aggregates on the behavior and cracking potential of internally cured concrete at an early age10.1016/j.conbuildmat.2015.08.093 ↗
40. Influence of cement fineness and water-to-cement ratio on mortar early-age heat of hydration and set times10.1016/j.conbuildmat.2013.10.011 ↗
41. Specific heat and thermal diffusivity of hardening concrete10.1680/macr.1995.47.172.203 ↗
42. Van Breugel · 1991
43. de Larrard · 1999 · 77
44. Effects of cement and water contents on adiabatic temperature rise of concrete
45. On the origin of eigenstresses in lightweight aggregate concrete10.1016/S0958-9465(03)00072-6 ↗
46. Effect of internal curing with super absorbent polymers on autogenous shrinkage of concrete at early age10.1016/j.conbuildmat.2015.12.115 ↗
47. Lura · 2003
48. Thermo-mechanical assessment of concrete microcracking damage due to early-age temperature rise10.1016/j.conbuildmat.2014.12.126 ↗
49. Autogenous shrinkage measurement
50. Internal curing efficiency of prewetted LWFAs on concrete humidity and autogenous shrinkage development10.1061/(ASCE)MT.1943-5533.0000883 ↗
51. Autogenous shrinkage of concrete containing granulated blast-furnace slag10.1016/j.cemconres.2006.01.005 ↗
52. Effect of curing temperature and type of cement on early-age shrinkage of high-performance concrete10.1016/S0008-8846(01)00601-9 ↗
53. Early-age tensile creep and cracking potential of concrete internally cured with pre-wetted lightweight aggregate10.1016/j.conbuildmat.2016.12.187 ↗
54. Effect of water-to-cementitious materials ratio and silica fume on the autogenous shrinkage of concrete10.1016/S0008-8846(03)00149-2 ↗
55. Coefficient of thermal expansion of cement paste and concrete: mechanisms of moisture interaction10.1617/s11527-006-9086-z ↗
56. Lokhorst · 1998
57. Estimation of temperature effects on autogenous shrinkage of concrete by a new prediction model10.1016/j.conbuildmat.2012.03.005 ↗
58. ACI Committee 231 · 2010
59. Emborg · 1989
60. Influence of ring size on the restrained shrinkage behavior of ultra high performance fiber reinforced concrete10.1617/s11527-013-0119-0 ↗
61. Influence of exposure conditions on the efficacy of internal curing
62. A laboratory test to analyze creep under tension of young concrete. Creep and shrinkage of concrete
63. ASTM · 2013
64. Cracking sensitivity of normal- and high-strength concretes
65. Effect of concrete and binder composition on cracking sensitivity. Concrete Repair, Rehabilitation and Retrofitting III