Study on the resistance to seawater corrosion of the cementitious systems containing ordinary Portland cement or/and calcium aluminate cement
Source abstract
Abstract
Abstract The resistance to seawater corrosion was investigated for OPC, CAC, OPC-CAC-gypsum, OPC-SG-FA, and OPC-CAC-gypsum-SG. The specimens were cured in tap water for 28 days and then immersed in artificial seawater for 30, 90, and 180 days. Compressive strength, weight change, apparent porosity, free and total chloride content were measured. The results demonstrated that the compressive strength of all specimens immersed in seawater increased up to 90 days and then decreased up to 180 days. Additional, the compressive strength of CAC immersed in seawater is higher than that in tap water. The OPC-CAC-gypsum-SG system had the highest resistance to seawater corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete and Cement Materials Research · Concrete Corrosion and Durability · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Changes in the phase assemblage of concrete exposed to sea water10.1016/j.cemconcomp.2013.09.015 ↗
2. Effect of temperature on the durability of class C fly ash belite cement in simulated radioactive liquid waste: synergy of chloride and sulphate ions10.1016/j.jhazmat.2008.10.073 ↗
3. Chloride binding of cement-based materials subjected to external chloride environment-a review10.1016/j.conbuildmat.2008.02.004 ↗
4. Attack on plain and blended cements exposed to aggressive sulfate environments10.1016/S0958-9465(01)00082-8 ↗
5. Evaluation of sulfate resistance of Portland and high alumina cement mortars using hardness test10.1016/j.conbuildmat.2009.11.016 ↗
6. A study of the hydration and setting behavior of OPC - HAC pastes10.1016/0008-8846(94)90192-9 ↗
7. The hydration of SECAR 71 aluminous cement at different temperatures10.1016/0008-8846(89)90093-8 ↗
8. Behavior of calcium aluminate cement (CAC) in the presence of hexavalent chromium10.1016/j.cemconcomp.2016.07.006 ↗
9. Hydration of calcium aluminates and calcium sulfoaluminate studied by Raman spectros copy10.1016/j.cemconres.2013.01.015 ↗
10. Moscow Civil Engineering. USSR Patent 487702. 1977.
11. Electrochemical K.K. Japanese Patent 010633. 1976.
12. Coal Industry Patent Ltd. British Patent 043504. 1978.
13. Seki Sui Chemical Industry. Japanese Patent 093874. 1979.
14. Effects of mortar ratio on the properties of super early strength grouting materials by ternary complex system10.1016/j.conbuildmat.2017.07.043 ↗
15. Study on a high strength ternary binder cured under different conditions10.1016/j.conbuildmat.2016.01.022 ↗
16. Hydration and durability of sulphate-resisting and slag cement blends in Caron’s Lake water10.1016/j.cemconres.2004.06.038 ↗
17. Modelling of chloride binding related to hydration products in slag-blended cements10.1016/j.conbuildmat.2014.04.038 ↗
18. The influence of silica fume on the compressive strength of cement paste and mortar10.1016/0008-8846(95)00152-3 ↗
19. Effect of mix proportions, seawater curing medium and applied voltages on corrosion resistance of concrete incorporating mineral admixtures10.1016/j.aej.2011.01.013 ↗
20. Developing chloride resisting concrete using PFA10.1016/S0008-8846(97)00146-4 ↗
21. Influence of Ca(OH)2 and CaSO4.2H20 on Hydration Reaction of Amorphous Calcium Aluminate10.1016/0008-8846(90)90016-Q ↗
22. Hydration and durability of sulphate-resisting and slag cement blends in Caron's Lake water10.1016/j.cemconres.2004.06.038 ↗
23. Investigation of relation between porosity, pore structure and chloride diffusion of fly ash and blended cement pastes10.1016/0008-8846(86)90049-9 ↗